Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.34 g/cc | 1.34 g/cc | ASTM D792 |
NatureWorks® Ingeo™ AW 300D Injection Grade Biopolymer Specifically designed for use in injection molded food serviceware applications. This opaque, off-white molding grade creates parts that are rigid and heat resistant for tableware used with hot food.. |
|||
Specific Gravity | 1.34 g/cc | 1.34 g/cc | ASTM D792 |
SABIC Innovative Plastics Lexan® LUX2619 PC (Europe-Africa-Middle East) Lexan* LUX2619 Polycarbonate resin is an extrusion grade. It is UL94 V-2 rated at 1.5 mm. It was designed for high light reflectance. |
|||
Specific Gravity | 1.34 g/cc | 1.34 g/cc | ASTM D792 |
PolyOne Geon™ Vinyl Wire & Cable WR3792CL Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Specific Gravity | 1.34 g/cc | 1.34 g/cc | ASTM D792 |
S&E Specialty Polymers TufTech™ GA-1180JFR PVC Compound Application: A 90°C PVC based flame retardant material designed for flat ribbon cable jacketing applications.Information provided by S&E Specialty Polymers |
|||
Specific Gravity | 1.34 - 1.38 g/cc | 1.34 - 1.38 g/cc | ASTM D 792 |
Karina E800-18/258-CR-AS Gray PVC Compound UV resistant PVC compoundInformation provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.34 g/cc | 1.34 g/cc | ISO 1183 |
Lehmann & Voss LUVOCOM® 19-7810 Polyamide 46, with aramid reinforcement and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Good friction and wear behaviour especially at increased temperatures.Emergency running propert.. |
|||
Specific Gravity | 1.34 g/cc | 1.34 g/cc | ISO 1183 |
Lehmann & Voss LUVOCOM® 19-8094 Polyamide 46, with carbon fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Electrically conductive.. |
|||
Specific Gravity | 1.34 g/cc | 1.34 g/cc | ASTM D792 |
Kostat ICP-STAT ICD-1004 PVC Sheet KOSTATs ICP-STAT is a thermoplastic sheet coated with an inherently conductive polymer (ICP). ICP-STAT has distinctive advantages in ESD and cleanliness performances compared to other materials bas.. |
|||
Specific Gravity | 1.34 g/cc | 1.34 g/cc | |
Sylvin Technologies 9960-60 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Specific Gravity | 1.34 g/cc | 1.34 g/cc | 23°C; ASTM D792 |
Teknor Apex APEX® 3211-65 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMUses-Automotive Applications, Non-specific Food Applications, General Purpose, Medical Applications, Modeling.. |
|||
Specific Gravity | 1.34 g/cc | 1.34 g/cc | ASTM D792 |
A. Schulman ComAlloy® E-14756 Flame Retardant Easy Flow Polycarbonate Alloy Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Specific Gravity | 1.34 g/cc | 1.34 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ Opaque Blue 40356 Concentrate Based In LLDPE DescriptionPOLYBATCH® 40356 is a blue color concentrate based in LLDPE. This concentrate was designed to provide color and opacity in blow molding applications. POLYBATCH® 40356/4 is typically .. |
|||
Specific Gravity | 1.34 g/cc | 1.34 g/cc | ASTM D792 |
A. Schulman ComAlloy® E-14756 Flame Retardant Easy Flow Polycarbonate Alloy Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Specific Gravity | 1.34 g/cc | 1.34 g/cc | DIN 53479 |
Lubrizol ESTANE® 58565 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Specific Gravity | 1.34 g/cc | 1.34 g/cc | ASTM D-792 |
Axiall HF-6597 Rigid PVC, Molding Georgia Gulf HF-6597 is a high flow PVC compound designed for thin wall parts and multi-cavity molds. It is ideally suited for a variety of electrical and appliance applications.Information provide.. |
|||
Specific Gravity | 1.34 g/cc | 1.34 g/cc | ISO 1183 |
Azoty Tarnow™ Tarnamid® T-27 GB30 Polyamide 6 - Glass Beads Reinforced 30% Glass beads reinforced, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following main properties:High.. |
|||
Specific Gravity | 1.34 g/cc | 1.34 g/cc | Base |
ACC QM 245 QSI Quantum Silicones 45 Durometer Addition Cure Moldmaking Material QM 245 is a two component, room temperature addition cure silicone material. The cured rubber has excellent mechanical properties and good shelf-life stability. This material is a good choice for th.. |
|||
Specific Gravity | 1.34 - 1.38 g/cc | 1.34 - 1.38 g/cc | ASTM D-792 |
Axiall 14771 Wire & Cable Flexible PVC General purpose jacketing compound with good low temperature properties. Recommended for a maximum service temperature of 75°C.Information provided by Georgia GulfGeorgia Gulf became Axiall Corpor.. |
|||
Specific Gravity | 1.34 - 1.38 g/cc | 1.34 - 1.38 g/cc | ASTM D-792 |
Axiall 35061 Coax & Telecom Flexible PVC CMR jacket over PVC or flame retardant PE insulation with excellent low temperature properties.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.34 - 1.38 g/cc | 1.34 - 1.38 g/cc | ASTM D-792 |
Axiall 8808 Moldings & Extrusions Flexible PVC 105°C rated flexible polyvinyl chloride compound formulated for UL94 V-2 in all colors. The compound is formulated for sunlight resistance.Information provided by Georgia GulfGeorgia Gulf became A.. |
|||
Specific Gravity | 1.34 g/cc | 1.34 g/cc | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 60 PHR Iceberg Clay Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Specific Gravity | 1.34 g/cc | 1.34 g/cc | ASTM D792 |
Teknor Apex Sinvicomp SBF 3778 Polyvinyl Chloride, Rigid Notes: RoHS Compliant Availability: Asia Pacific Features: Food Contact AcceptableUses: Shrink Wrap Forms: Pellets Processing Method: Blown FilmInformation Provided by Teknor Apex |
|||
Specific Gravity | 1.34 - 1.38 g/cc | 1.34 - 1.38 g/cc | ASTM D-792 |
Axiall 22941 Coax & Telecom Flexible PVC Non-lead stabilized, 80C riser jacket.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.34 g/cc | 1.34 g/cc | |
Sylvin Technologies 6147-83 PVC Wire/Cable Compound Information provided by Sylvin Technologies Inc. |
|||
Specific Gravity | 1.34 g/cc | 1.34 g/cc | ASTM D792 |
Gharda Chemicals Gafone™ B2300 Polysupersulfone (PSS)
(discontinued **) Characteristics: Excellent Dimensional properties Transparent Improved Impact Strength and Toughness as compared to PES Excellent Hydorlytic Stability High Stress Cracking Resistance Good Chemical.. |
|||
Specific Gravity | 1.34 g/cc | 1.34 g/cc | ASTM D792 |
SABIC Innovative Plastics ULTEM 2110 PEI 10% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. |