Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.05 g/cc | 1.05 g/cc | 23/23°C; ASTM D792 |
RheTech Products T20P105-00FA 20% Talc Reinforced Polypropylene, FDA Compliant Components, Natural Applications: Food traysFood service implementsContainersConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Specific Gravity | 1.05 g/cc | 1.05 g/cc | ASTM D792 |
Polymax® Maxelast® D6840 TPE, Extruded Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsSporting GoodsSealsWire & Cable ElectronicsMedical DevicesInformation from.. |
|||
Specific Gravity | 1.05 g/cc | 1.05 g/cc | Liquid State |
Palm Labs Adhesives TURBO FUSE SERIES 110 MEDICAL DEVICES APPROVED (5 Viscosity) Rapid Bonding Adhesive Palm Lab's cyanoacrylate is a one component rapid bonding adhesive. TURBO FUSE SERIES 110 MEDICAL DEVICES APPROVED advanced formula is designed to polymerize instantly by absorbing surface moisture... |
|||
Specific Gravity | 1.05 g/cc | 1.05 g/cc | Liquid State |
Palm Labs Adhesives Turbo Fuse Series 130 (100 Viscosity) Rapid Bonding Adhesive Palm Lab's Cyanoacrylate is a one component rapid bonding adhesive. TURBO FUSE SERIES 130 advanced formula is designed to polymerize instantly by absorbing surface moisture. The product's performanc.. |
|||
Specific Gravity | 1.05 g/cc | 1.05 g/cc | ASTM D792 |
Polymer Resources PPX-GP3-[color]-EN Modified-PPO, Extrusion Grade Modified-Polyphenylene Oxide, Extrusion Grade, 235F HDTFeatures: • Hydrolytically Stable • Low to No Water AbsorptionProcess: ExtrusionNotes: All physical, mechanical and thermal testing conduct.. |
|||
Specific Gravity | 1.05 g/cc | 1.05 g/cc | ASTM D792 |
PolyOne Dynaflex™ G7630-1 (Natural) Thermoplastic Elastomer (TPE) Dynaflex™ G7630-1 (Natural) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Non-Slip Grip - Overmold Adhe.. |
|||
Specific Gravity | 1.05 g/cc | 1.05 g/cc | |
Alcoa KAMA 2700 OPS Lamination, Film
(discontinued **) CapabilitiesGauge: .001” to .004” (28 to 101µm)Width: .2” to 80” (50.8 to 2032mm)Core size: 3” and 6” standard cores, 8” availableRoll O.D.: various confiations availableCustom colors and ti.. |
|||
Specific Gravity | 1.05 g/cc | 1.05 g/cc | |
Resinlab® CYNERGY CA6204 Adhesive Description: The CYNERGY 6200 SERIES products are for use in demanding applications where very fast cure speeds are required. Also used when difficult to bond and acidic surfaces are used such as EP.. |
|||
Specific Gravity | 1.05 g/cc | 1.05 g/cc | |
Resinlab® CYNERGY CA6802 Adhesive Description: The CYNERGY 6800 SERIES are clear, high strength products ideal for bonding dissimilar materials with excellent performance on a wide range of surfaces. This series of products has USP .. |
|||
Specific Gravity | 1.05 g/cc | 1.05 g/cc | 23/23°C; ASTM D792 |
M. Holland Company AB308LG ABS Acrylonitrile Butadiene Styrene High flowGood impact resistanceHigh stiffnessApplications: Household goodsPackagingInformation provided by M. Holland |
|||
Specific Gravity | 1.05 g/cc | 1.05 g/cc | ASTM D792 |
LG Chemical HT700 ABS, High Stiffness Feature: Injection Molding, High StiffnessApplication: Electric & Electronic Products, Miscellaneous GoodsCAS No. 9003-56-9Information provided by LG Chemical |
|||
Specific Gravity | 1.05 - 1.07 g/cc | 1.05 - 1.07 g/cc | |
Michelman® DigiGuard® Gloss 100 Water based overprint varnish Description: Water based overprint varnishUsage: DigiGuard® Gloss 100 is a heat resistant, glossy overprint varnishFood Contact Information when manufactured in the USA:FDA: 175.105: Components o.. |
|||
Specific Gravity | 1.05 g/cc | 1.05 g/cc | ISO 1183 |
Gromax BTE45-DN00N1 Nylon 6 (Conditioned) Information provided by Gromax Enterprises Corp. |
|||
Specific Gravity | 1.05 g/cc | 1.05 g/cc | ASTM D 792 |
MRC Polymers SATRANâ„¢ 805 ABS Terpolymer, Impact Modified Information provided by MRC Polymers Inc. |
|||
Specific Gravity | 1.05 - 1.09 g/cc | 1.05 - 1.09 g/cc | A component |
Taiwan PU Corporation CPU-69-A/B Polyurethane Casting Elastomer CPU-69-A consists of polyether polyols and other additives. CPU-69-b is an isocyanate prepolymer. Together they create compounds that cure under room temperature and have short working times, shor.. |
|||
Specific Gravity | 1.05 g/cc | 1.05 g/cc | ASTM D792 |
Spartech SP-9080 High Heat ABS Sheet Description: ABS SheetInformation provided by Spartech. |
|||
Specific Gravity | 1.05 g/cc | 1.05 g/cc | ASTM D792 |
Samsung Cheil Industries Starex® BC-0130 X ABS, Unreinforced General Purpose Stiff ABS material that is used for battery casesInformation provided by Samsung Cheil Industries. |
|||
Specific Gravity | 1.05 g/cc | 1.05 g/cc | ASTM D792 |
SABIC Innovative Plastics NORYL HH180 PPE+PS (Europe-Africa-Middle East) Noryl* HH180 is a high heat, unfilled modified polyphenylene ether resin with a Vicat B/120 temperature of 185 deg C. Noryl HH180 is only available in color 80365. |
|||
Specific Gravity | 1.05 g/cc | 1.05 g/cc | ASTM D 792 |
SABIC Innovative Plastics Noryl MX5569 PPE+PS PPE+PS blend. High Heat. Good balance of flow and impact. Offers good aging performance under heat. Typical applications include Automotive Interiors and Lighting.This data was supplied by SABIC-.. |
|||
Specific Gravity | 1.05 g/cc | 1.05 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ Green 3015 Concentrate Based In Polyethylene DescriptionPOLYBATCH® 3015 is a green color concentrate based in polyethylene. This concentrate was designed to provide opacity and color in polyolefin film and molding applications. POLYBATCH® .. |
|||
Specific Gravity | 1.05 g/cc | 1.05 g/cc | ASTM D792 |
A. Schulman POLYFORT™ FPP 1285U Glass Filled, UV Stable Impact Copolymer Polypropylene DescriptionPolyfort® FPP 1285U is a 20% glass filled UV stable impact copolymer polypropylene product. Information provided by A. Schulman. |
|||
Specific Gravity | 1.05 g/cc | 1.05 g/cc | ASTM D792 |
A. Schulman POLYFLAM™ RPP 1133 Flame Retardant, Copolymer Polypropylene DescriptionPolyflam® RPP 1133 is a 30% glass filled, flame retardant copolymer polypropylene compound. Information provided by A. Schulman. |
|||
Specific Gravity | 1.05 g/cc | 1.05 g/cc | |
Zylog Hipolyene® 8021 M Thermoplastic Polyolefin & PP Compound Information provided by Zylog Plastalloys Pvt. Ltd. |
|||
Specific Gravity | 1.05 g/cc | 1.05 g/cc | ASTM D792 |
ELASTO UK Dryflex® 662550S SEBS Based Material, Semi-Filled Qualities, 55A Hardness, Black The 660-series is recommended when the properties of the produced detail requires the advantages of the 500-series in combination with the 600-series. A semi-filled material can therefore combine t.. |
|||
Specific Gravity | 1.05 g/cc | 1.05 g/cc | ASTM D792 |
ELASTO UK Dryflex® 662650S SEBS Based Material, Semi-Filled Qualities, 65A Hardness, Black The 660-series is recommended when the properties of the produced detail requires the advantages of the 500-series in combination with the 600-series. A semi-filled material can therefore combine t.. |
|||
Specific Gravity | 1.05 g/cc | 1.05 g/cc | ISO 2781 |
ELASTO UK Dryflex® 8006-101 Flame Retardant TPE for Extrusion, Black, Halogen Free Vitaprene® thermoplastic elastomers combine the performance of most vulcanized rubber with the process properties of thermoplastics. Vitaprene® compounds permit sophisticated component design and.. |
|||
Specific Gravity | 1.05 g/cc | 1.05 g/cc | ASTM D792 |
Calsak CS-72 General Purpose ABS Resin Product Characteristics:High Impact, High GlossInjection molding grade |
|||
Specific Gravity | 1.05 g/cc | 1.05 g/cc | |
Alcoa KAMA 3200 Prime High Impact Polystyrene
(discontinued **) CapabilitiesGauge: .007” to .060” (178 to 1524µm)Width: 12” to 62” (304 to 1575mm)Core Size: 6” standard cores, 3” and 8” availableRoll O.D.: 29” standard, up to 40” availableSilicone trea.. |
|||
Specific Gravity | 1.05 g/cc | 1.05 g/cc | ASTM D792 |
LTL Color Compounds ColorFast® GPA100 ABS High impact, high gloss injection molding ABS, HB-rated, FDAAll information provided by LTL Color Compounders, Inc. |
|||
Specific Gravity | 1.05 g/cc | 1.05 g/cc | ASTM D792 |
Supreme Petrochem SP 731 9920 High Impact Polystyrene Characteristics Speciality grade containing silicon oil to provide wear resistance and high opacity jet black color Easy flowing grade Processing Injection moldingApplications Camera parts Photogr.. |