Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 0.960 g/cc | 0.960 g/cc | 23/23°C; ASTM D792 |
RheTech Products FT4650-01UV Thermoplastic Polyolefin, Non-UV Stabilized, Black Applications: Scuff platesExterior grillesBodyside moldingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Specific Gravity | 0.960 g/cc | 0.960 g/cc | 23/23°C; ASTM D792 |
RheTech Products GC10P200-00 10% Glass Fiber Reinforced Polypropylene Copolymer, Non-UV Stabilized, Chemically Coupled, Natural Applications: Component housingsStorage binsRecreational vehicle trim and bumpersInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Specific Gravity | 0.960 g/cc | 0.960 g/cc | ASTM D792 |
Quadrant EPP TIVAR® CERAM P UHMW-PE, Premium Microsphere Filled (ASTM Product Data Sheet) |
|||
Specific Gravity | 0.960 g/cc | 0.960 g/cc | ASTM D792 |
Quadrant EPP TIVAR® Extended Wear UHMW-PE, Premium Glass-filled, Partially Cross-linked (ASTM Product Data Sheet) |
|||
Specific Gravity | 0.960 g/cc | 0.960 g/cc | 23°C; ASTM D792 |
ExxonMobil Santoprene® 8123-45S100 Thermoplastic Elastomer
(discontinued **) A hard, black thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material has low friction and is especially designed for use as a co-extruded slip-coat layer on weath.. |
|||
Specific Gravity | 0.960 g/cc | 0.960 g/cc | ISO 1183 |
Polimeri Europa Eraclene® MP 90 High Density Polyethylene - Injection Molding Eraclene MP 90 is a high density polyethylene homopolymer resin (HDPE) with antioxidants, suitable for injection molding application.Eraclene MP 90 has a narrow molecular weight distribution and a h.. |
|||
Specific Gravity | 0.960 g/cc | 0.960 g/cc | ASTM D297 |
LG Chemical KEYFLEX TO-1075A Thermoplastic Olefin for Injection Molding, 75A Hardness KEYFLEX resins, thermoplastic elastomers divided by polyester and polyolefin type, have been developed by LG`s own polymerization and compounding technology. They display the flexibility of rubber .. |
|||
Specific Gravity | 0.960 - 0.980 g/cc | 0.960 - 0.980 g/cc | |
Michelman® FiberMax® 5000 Water based medium treatment to replace paraffin wax Description: Water based medium treatment to replace paraffin waxUsage: FibreMax® 5000 is a new alternative to paraffin wax for treating medium. It is a repulpable, machine ready fiber treatment .. |
|||
Specific Gravity | 0.960 - 0.980 g/cc | 0.960 - 0.980 g/cc | |
Michelman® Michem® Emulsion 48040M2 Nonionic microcrystalline wax emulsion Description: Nonionic microcrystalline wax emulsionUsage: Michem® Emulsion 47950 is a wax emulsion which is effective as an anti-graffiti and sacrificial coating and can also contribute water res.. |
|||
Specific Gravity | 0.960 g/cc | 0.960 g/cc | |
Lord Adhesives Flocklok® P13 Adhesive Flocklok® P13 is a moisture curing, flexible polyurethane adhesive used for automotive weatherstrip sealing profiles to flock. This adhesive will adhere polyester or polyamide flock to a variety .. |
|||
Specific Gravity | 0.960 g/cc | 0.960 g/cc | ISO 1183/1 |
A. Schulman FORMION™ FI 555-31 Recycled Ionomer Information provided by A. Schulman. |
|||
Specific Gravity | 0.960 g/cc | 0.960 g/cc | ASTM D792 |
Teknor Apex UNIPRENE® 7010-73 Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Specific Gravity | 0.960 g/cc | 0.960 g/cc | ASTM D792 |
Teknor Apex UNIPRENE® 7010-87 Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Specific Gravity | 0.960 g/cc | 0.960 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ Teal 30316 Concentrate Based In LLDPE DescriptionPOLYBATCH® 30316 is a teal color concentrate based in LLDPE. This concentrate was designed to provide color and opacity in blow molding applications. POLYBATCH® 30316 is typically re.. |
|||
Specific Gravity | 0.960 g/cc | 0.960 g/cc | 15°C; ASTM D1298 |
ExxonMobil 68 Mobil EAL Arctic Series Mobil EAL Arctic Series are high performance Environmental Awareness Lubricants (EAL) that are fully synthetic products designed specifically for the lubrication of refrigeration compressors and sys.. |
|||
Specific Gravity | 0.960 g/cc | 0.960 g/cc | ISO 1183/1 |
A. Schulman FORMION™ FI 555-31 Recycled Ionomer Information provided by A. Schulman. |
|||
Specific Gravity | 0.960 g/cc | 0.960 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ 10178Z Amber Concentrate Based in LDPE Description POLYBATCH® Amber 10178Z is an amber color concentrate based in LDPE. ApplicationPOLYBATCH® 10178Z is designed for use between 3 and 5% in HDPE molded bottles (approx. 50 mil) to achiev.. |
|||
Specific Gravity | 0.960 g/cc | 0.960 g/cc | ASTM D 792 |
Zylog Neoplast® 173 FT EB Thermoplastic Vulcanizate Neoplast 173 FT EB is a soft, dynamically vulcanized thermoplastic vulcanizate (TPV), based on polyolefin chemistry, and is intended for Injection Molding, Blow Molding and Extrusion applications.Ro.. |
|||
Specific Gravity | 0.960 g/cc | 0.960 g/cc | ISO 1183 |
Total HDPE HD 6081 High Density Polyethylene - Injection Molding HD 6081 is a high density polyethylene with very good organoleptic properties, rigidity and processability.It is especially suited for the production of caps & closures for non-carbonated drinks by .. |
|||
Specific Gravity | 0.960 g/cc | 0.960 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ Teal 30316 Concentrate Based In LLDPE DescriptionPOLYBATCH® 30316 is a teal color concentrate based in LLDPE. This concentrate was designed to provide color and opacity in blow molding applications. POLYBATCH® 30316 is typically re.. |
|||
Specific Gravity | 0.960 g/cc @Temperature 25.0 °C |
0.960 g/cc @Temperature 77.0 °F |
|
Dow Corning 9045 Silicone Elastomer Blend A mixture of high molecular weight silicone elastomers (dimethicone crosspolymer) in cyclopentasiloxane for use in skincare, suncare, shower gel, hair care, and color cosmetic applications.Informati.. |
|||
Specific Gravity | 0.960 g/cc | 0.960 g/cc | |
Dow Corning 9-6346 SILANE 72% solids quaternary ammonium functional alkoxysilane, provides anti-static properties.Information provided by Dow Corning |
|||
Specific Gravity | 0.960 g/cc | 0.960 g/cc | |
Dow Corning SYL-OFF® SL 3000 CATALYST 1,000 ppm platinum in vinyl polymerInformation provided by Dow Corning |
|||
Specific Gravity | 0.960 g/cc | 0.960 g/cc | 23°C; ASTM D792 |
ExxonMobil Santoprene® 8271-55 Thermoplastic Elastomer A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated .. |
|||
Specific Gravity | 0.960 g/cc | 0.960 g/cc | Part B |
Epoxy Technology EPO-TEK® OE121 Black Epoxy Adhesive Material Description: A two component, low temperature curing epoxy adhesive designed for semiconductor flip chip underfill. It is color coded black for visual ID during the underfilling process. .. |
|||
Specific Gravity | 0.960 g/cc | 0.960 g/cc | ASTM D 1298 |
ConocoPhillips Gear Shield NC Open Gear Lubricant Description: Conoco Gear Shield NC is a black, viscous fluid designed to lubricate open gears. Gear Shield NC contains neither chlorinated solvents nor lead compounds. Gear Shield NC is designed to .. |
|||
Specific Gravity | 0.960 g/cc | 0.960 g/cc | 23°C; ASTM D792 |
ExxonMobil Santoprene® 121-68W228 Thermoplastic Elastomer
(discontinued **) A soft, black thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material is specially formulated for low density foamed profile extrusion applications and has long te.. |
|||
Specific Gravity | 0.960 g/cc | 0.960 g/cc | Mixed |
Resinlab® UR3005 Clear Two Part Urethane Elastomer Resinlab™ UR 3005 Clear is a two component, room temperature curing polybutadiene polyurethane casting and potting system. It is designed to cure completely at room temperature. UR 3005 Clear provi.. |
|||
Specific Gravity | 0.960 - 1.00 g/cc | 0.960 - 1.00 g/cc | ASTM D792 |
S&E Specialty Polymers GPP1001V0M-HCO PP Application: A polypropylene compound designed for injection molded industrial battery, electrical housing or appliance applications. It affords medium impact resistance with a high level of flam.. |
|||
Specific Gravity | 0.960 g/cc | 0.960 g/cc | ASTM D792 |
PolyOne Synprene® ST-6240 Thermoplastic Elastomer - SBC
(discontinued **) Description/Features:Over-Molding GradeUV StabilizedApplications:Multi-PurposeProcessing Method:Injection MoldingPolyOne First ChoiceInformation provided by PolyOne Corporation. |