Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.22 - 1.28 g/cc | 1.22 - 1.28 g/cc | ASTM D792 |
S&E Specialty Polymers TufFlex™ GTPE-2272SG-K8 TPE Compound Application: A flame retardant, matte finish, 90°C oil resistant, flexible TPE jacketing material.Information provided by S&E Specialty Polymers |
|||
Specific Gravity | 1.22 - 1.28 g/cc | 1.22 - 1.28 g/cc | ASTM D792 |
Parker Chomerics Tecknit SC-Consil® FR861 Carbon-Filled Silicone Elastomer Description: SC-CONSIL is a silicone elastomer filled with carbon particles. It provides superior shielding and a reliable environmental seal. The combination of carbon particles and silicone allows.. |
|||
Specific Gravity | 1.22 - 1.28 g/cc | 1.22 - 1.28 g/cc | ASTM D792 |
Parker Chomerics Tecknit SC-Consil® FR862 Carbon-Filled Silicone Elastomer Description: SC-CONSIL is a silicone elastomer filled with carbon particles. It provides superior shielding and a reliable environmental seal. The combination of carbon particles and silicone allows.. |
|||
Specific Gravity | 1.22 - 1.28 g/cc | 1.22 - 1.28 g/cc | ASTM D 792 |
Karina E 90/212-DA-IS-SI-AT Compound PVC Crystal PVC Compound used for films. Non-toxic. Approved by food packaging safety, Pira International, United Kingdom.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.22 - 1.28 g/cc | 1.22 - 1.28 g/cc | ASTM D 792 |
Karina FADA 45-YAT White PVC Compound Non-toxic PVC compound recommended for injection of inseminator for veterinary applicationsInformation provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.22 - 1.28 g/cc | 1.22 - 1.28 g/cc | ASTM D 792 |
Karina KAPU 6535/1-Y Ivory PVC Compound Foamed PVC compound to be used like an alternative to PU for injection of extra-light shoes soles.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.22 - 1.28 g/cc | 1.22 - 1.28 g/cc | ASTM D 792 |
Karina 75/204-D-AT-IS-H Clear PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.22 - 1.28 g/cc | 1.22 - 1.28 g/cc | ASTM D 792 |
Karina 750D10/120-IS-PO White PVC Compound PVC powder compound, recommended for covering metallic parts in fluidized bed.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.22 - 1.28 g/cc | 1.22 - 1.28 g/cc | ASTM D 792 |
Karina 80/213-D-IS-SI Clear PVC Compound (DAY Brazil) Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.22 - 1.28 g/cc | 1.22 - 1.28 g/cc | ASTM D 792 |
Karina 804D40/146-AT Green PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.22 - 1.28 g/cc | 1.22 - 1.28 g/cc | ASTM D 792 |
Karina 813D11/4-IS-AS Bronze PVC Compound Heavy metal free and UV resistant compound, recommended for extrusion of refrigeration chamber curtain.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.22 - 1.28 g/cc | 1.22 - 1.28 g/cc | ASTM D 792 |
Karina 920-10/156-Y-IS-BZ White PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.22 - 1.28 g/cc | 1.22 - 1.28 g/cc | NBR NM-IEC 60811-1-3 |
Karina E 06/815-FC-LMP MB Concentration de Pigment Blue for PVC Heavy metal free pigment concentration for PVC usage. Usage 2% MinimumFlexible and rigidExtrusion and injection generalExcellent for cables and wiresOrganicInformation provided by Karina Indústr.. |
|||
Specific Gravity | 1.22 - 1.28 g/cc | 1.22 - 1.28 g/cc | ASTM D 792 |
Karina E 34/20-RG-PO Lilac Color Concentrate for PVC Color concentrate in powder form recommended for application in PVC compounds for general purposes extrusion and injection. Recommended to use 2%.Information provided by Karina Indústria e ComÃ.. |
|||
Specific Gravity | 1.22 - 1.28 g/cc | 1.22 - 1.28 g/cc | ASTM D 792 |
Karina E 40/43-RG-PO Green Color Concentrate for PVC Color concentrate in powder form recommended for application in PVC compounds for general purposes extrusion and injection. Recommended to use 2%.Information provided by Karina Indústria e ComÃ.. |
|||
Specific Gravity | 1.22 - 1.28 g/cc | 1.22 - 1.28 g/cc | ASTM D 792 |
Karina E 42/129-RG-PO Red Color Concentrate for PVC Color concentrate in powder form recommended for application in PVC compounds for general purposes extrusion and injection. Recommended to use 2%.Information provided by Karina Indústria e ComÃ.. |
|||
Specific Gravity | 1.22 - 1.28 g/cc | 1.22 - 1.28 g/cc | ASTM D 792 |
Karina E 52/10-FC-LMP Purple Color Concentrate for PVC Heavy metal free color concentrate recommended for application in electrical wire and cable PVC compounds. Also suitable for pigmentation of flexible and rigid PVC compounds for general purposes. .. |
|||
Specific Gravity | 1.22 - 1.28 g/cc | 1.22 - 1.28 g/cc | ASTM D 792 |
Karina E 85/201-DA-IS-SI-AT Clear Crystal PVC Compound Non toxic PVC compound, free of phthalate plasticizers, recommended for stretch films for food contact use.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.21 - 1.28 g/cc | 1.21 - 1.28 g/cc | ASTM D792 |
Spartech Royalite R570 FR-ABS Fire Rated Sheet Description: Fire Rated SheetInformation provided by Spartech. |
|||
Specific Gravity | 1.22 - 1.28 g/cc | 1.22 - 1.28 g/cc | ASTM D792 |
Buckeye Polymers BP RPP 4010 T NAT Polypropylene, Talc Filled Product Information: Our Talc filled product lines exhibit excellent properties such as high stiffness, surface aesthetics, low coefficient of thermal expansion, low shrinkage, improved scratch and .. |
|||
Specific Gravity | 1.22 - 1.28 g/cc | 1.22 - 1.28 g/cc | ASTM D792 |
Buckeye Polymers BP RPP 4012 T BLK Polypropylene, Talc Filled Product Information: Our Talc filled product lines exhibit excellent properties such as high stiffness, surface aesthetics, low coefficient of thermal expansion, low shrinkage, improved scratch and .. |
|||
Specific Gravity | 1.24 - 1.28 g/cc | 1.24 - 1.28 g/cc | ASTM D-792 |
Axiall 10850 Wire & Cable Flexible PVC Non-metallic conduit. 3/4" and smaller.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.24 - 1.28 g/cc | 1.24 - 1.28 g/cc | ASTM D-792 |
Axiall 7900 Moldings & Extrusions Flexible PVC Clear, injection molding compound with good UV resistance.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.24 - 1.28 g/cc | 1.24 - 1.28 g/cc | ASTM D-792 |
Axiall 801-90B Moldings & Extrusions Flexible PVC Automotive harness tape.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.24 - 1.28 g/cc | 1.24 - 1.28 g/cc | ASTM D-792 |
Axiall 8651 Moldings & Extrusions Flexible PVC A quality, low gravity extrusion compound with excellent low temperature properties. Designed for use in weatherstrips, flexible gaskets and extruded shapes.Information provided by Georgia GulfGeor.. |
|||
Specific Gravity | 1.24 - 1.28 g/cc | 1.24 - 1.28 g/cc | ASTM D-792 |
Axiall 8810 Moldings & Extrusions Flexible PVC Low gravity extrusion compound especially formulated for extruded T-moldings and other shapes where uniform flow through the die is required. Exhibits good flex whitening resistance.Information pro.. |
|||
Specific Gravity | 1.24 - 1.28 g/cc | 1.24 - 1.28 g/cc | ASTM D-792 |
Axiall 8881 Moldings & Extrusions Flexible PVC Profile extrusion compound especially formulated to impart a matte surface appearance to the finished article.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.24 - 1.28 g/cc | 1.24 - 1.28 g/cc | ASTM D-792 |
Axiall 8941 Moldings & Extrusions Flexible PVC A clear extrusion and molding grade compound with good toughness.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.22 - 1.28 g/cc | 1.22 - 1.28 g/cc | ASTM D 792 |
Karina E 85/201-DA-IS-SI Clear PVC Compound Non toxic PVC compound, free of phthalate plasticizers, recommended for stretch films for food contact use.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.22 - 1.28 g/cc | 1.22 - 1.28 g/cc | ASTM D792 |
Buckeye Polymers BP RPP 4008 TR BLK Polypropylene, Talc Filled Product Information: Our Talc filled product lines exhibit excellent properties such as high stiffness, surface aesthetics, low coefficient of thermal expansion, low shrinkage, improved scratch and .. |