Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

S&E Specialty Polymers TufFlex™ GTPE-2272SG-K8 TPE Compound

Category Polymer , Thermoplastic , Elastomer, TPE
Manufacturer S&E Specialty Polymers
Trade Name TufFlex™
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF S&E Specialty Polymers TufFlex™ GTPE-2272SG-K8 TPE Compound.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Application: A flame retardant, matte finish, 90°C oil resistant, flexible TPE jacketing material.Information provided by S&E Specialty Polymers
Physical Properties Metric English Comments
Specific Gravity 1.22 - 1.28 g/cc
1.22 - 1.28 g/cc
ASTM D792
Deformation 29.0 %
<br>@Load 2.00 kg,<br> Temperature 150 °C
29.0 %
<br>@Load 4.41 lb,<br> Temperature 302 °F
UL 1581
Mechanical Properties Metric English Comments
Hardness, Shore A 65.0 - 71.0
<br>@Time 15.0 sec
65.0 - 71.0
<br>@Time 0.00417 hour
ASTM D2240
Tensile Strength 13.8 MPa
2000 psi
ASTM D412
13.248 MPa
<br>@Temperature 100 °C,<br> Time 346000 sec
1921.5 psi
<br>@Temperature 212 °F,<br> Time 96.0 hour
Oil Aged
Elongation at Break 450 %
450 %
ASTM D412
324 %
<br>@Treatment Temp. 100 °C,<br> Time 346000 sec
324 %
<br>@Treatment Temp. 212 °F,<br> Time 96.0 hour
Oil Aged
Thermal Properties Metric English Comments
Brittleness Temperature -55.0 °C
-67.0 °F
ASTM D746
Oxygen Index 27.0 %
27.0 %
ASTM D2863
Copyright © lookpolymers.com All Rights Reserved