Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 3.40 - 3.60 g/cc | 3.40 - 3.60 g/cc | ASTM D792 |
P & P Technology EC-H Silver Copper Loaded Silicone P & P Technology material reference EC-H is a printing grade silicone elastomer with a Silver/Copper conductive filler and is Tan in color. The material is specially compounded to offer excellent p.. |
|||
Specific Gravity | 3.40 g/cc | 3.40 g/cc | ASTM D395 |
Parker Chomerics CHOFORM® 5513 Conductive Form-in-Place Gasket Description: A range of conductive particle technologies combined with thermoset and RTV silicone systems provide a material selection for most opportunities. Multiple filler grades balance material.. |
|||
Specific Gravity | 3.40 g/cc | 3.40 g/cc | |
Parker Chomerics CHO-MUTE 9000 Microwave Absorber Microwave Absorber Material. Elastomer microwave absorber is designed to offer wide band attenuation within operating frequencies of 500 MHz to 18 GHz. CHO-MUTE 9000 incorporates a high tech silicon.. |
|||
Specific Gravity | 3.40 g/cc | 3.40 g/cc | |
Parker Chomerics CHO-MUTE 9020 RF Absorber Microwave Absorber Material. Elastomer microwave absorber is designed to offer wide band attenuation within operating frequencies of 30 MHz to 12 GHz. CHO-MUTE 9020 incorporates a high tech silicone.. |
|||
Specific Gravity | 3.40 g/cc | 3.40 g/cc | Fiber |
Zircar Zirconia BusterF Alumina Bulk Fiber Insulation Alumina Bulk Fibers Type BusterF are Hi-Alpha alumina fibers available in two different forms, both having useful properties up to 1700°C. These polycrystalline fibers can be vacuum formed into rig.. |
|||
Specific Gravity | 3.40 g/cc | 3.40 g/cc | Fiber |
Zircar Zirconia BusterF-10 Alumina Bulk Fiber Insulation Alumina Bulk Fibers Type BusterF are Hi-Alpha alumina fibers available in two different forms, both having useful properties up to 1700°C. These polycrystalline fibers can be vacuum formed into rig.. |
|||
Specific Gravity | 3.40 g/cc | 3.40 g/cc | ASTM D4745 |
3M Dyneon™ CC155 Custom Fluoropolymer Compound
(discontinued **) This compound consists of a mixture of 50% stainless steel blended with PTFE.Information provided by Dyneon, A 3M Company |
|||
Specific Gravity | 3.40 g/cc | 3.40 g/cc | Fiber |
Zircar Zirconia BusterF Alumina Bulk Fiber Insulation Alumina Bulk Fibers Type BusterF are Hi-Alpha alumina fibers available in two different forms, both having useful properties up to 1700°C. These polycrystalline fibers can be vacuum formed into rig.. |
|||
Specific Gravity | 3.40 g/cc | 3.40 g/cc | Fiber |
Zircar Zirconia BusterF-10 Alumina Bulk Fiber Insulation Alumina Bulk Fibers Type BusterF are Hi-Alpha alumina fibers available in two different forms, both having useful properties up to 1700°C. These polycrystalline fibers can be vacuum formed into rig.. |
|||
Specific Gravity | 3.40 g/cc | 3.40 g/cc | ASTM D792 |
Ecomass® 4703ZC76 Stainless Steel Filled Polyurethane Nontoxic alternative to Lead (Pb), weighting and balancing applicationsModerate Specific GravityStainless Steel Filled Polyurethane (TPU)FlexibleInformation provided by Technical Polymers |
|||
Specific Gravity | 3.40 g/cc | 3.40 g/cc | ASTM D792 |
Parker Chomerics CHO-FORM 5528 Conductive Form-In-Place Gaskets Description: A range of conductive particle technologies combined with thermoset and RTV silicone systems provide a material selection for most opportunities. Multiple filler grades balance material.. |
|||
Specific Gravity | 3.40 g/cc | 3.40 g/cc | ASTM D792 |
Parker Chomerics CHO-MUTE 9005 Microwave Absorber Microwave Absorber Material. Elastomer microwave absorber is designed to offer wide band attenuation within operating frequencies of 500 MHz to 18 GHz. CHO-MUTE 9005 incorporates a high tech silicon.. |
|||
Specific Gravity | 3.40 g/cc | 3.40 g/cc | ASTM D792 |
Parker Chomerics CHO-MUTE 9025 Conductive Elastomer Microwave Absorber Material. Elastomer microwave absorber is designed to offer wide band attenuation within operating frequencies of 500 MHz to 18 GHz. CHO-MUTE 9005 incorporates a high tech silicon.. |