Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 3.20 g/cc | 3.20 g/cc | ASTM D792 |
P & P Technology EC-S Pure Silver Loaded Silicone P & P Technology material reference EC-S is a silicone elastomer with Silver conductive filler. It is tan in color. The material is specially compounded to offer excellent physical and electrical p.. |
|||
Specific Gravity | 3.20 - 3.50 g/cc | 3.20 - 3.50 g/cc | |
Parker Chomerics CHO-SEAL 1260 Conductive Elastomer Conductive Elastomer. CHO-SEAL 1260 elastomer is a silver-filled-silicone intended for mounting silicon wafers during processes such as ion milling. It provides high levels of electrical and thermal.. |
|||
Specific Gravity | 3.20 - 3.38 g/cc | 3.20 - 3.38 g/cc | |
Reade Advanced Materials Diopside Powder (CaMg(CO3)2 and CaMg(SiO3)2) Description: A naturally mined mineral that is relatively difficult to source. Low-iron grades have use in glass manufacture, whiteware bodies, glazes, and welding rod coatings.Forms Available: Lum.. |
|||
Specific Gravity | 3.20 g/cc | 3.20 g/cc | 60°C for 1,000 hrs with 90% RH; JIS-K-6220 |
Fujipoly Industries Sarcon® GR-Hm Gap Filler Pad Sarcon GR-m is a highly formable, thermally conductive gel material (no electicity conductive) in a versatile sheet form that easily fits and adheres to most all shapes and sizes of components, and .. |
|||
Specific Gravity | 3.20 g/cc | 3.20 g/cc | JIS-K-6220; ASTM D-792 |
Fujipoly Industries Sarcon® GR-Hm Gap Filler Pad Sarcon GR-m is a highly formable, thermally conductive gel material (no electicity conductive) in a versatile sheet form that easily fits and adheres to most all shapes and sizes of components, and .. |
|||
Specific Gravity | 3.20 g/cc | 3.20 g/cc | 150°C for 1,000 hrs; JIS-K-6220 |
Fujipoly Industries Sarcon® GR-Hm Gap Filler Pad Sarcon GR-m is a highly formable, thermally conductive gel material (no electicity conductive) in a versatile sheet form that easily fits and adheres to most all shapes and sizes of components, and .. |
|||
Specific Gravity | 3.20 g/cc | 3.20 g/cc | 60°C for 1,000 hrs with 90% RH; JIS-K-6220 |
Fujipoly Industries Sarcon® GR-Hn Gap Filler Pad Sarcon GR-n is a highly formable, thermally conductive gel material (no electicity conductive) in a versatile sheet form that easily fits and adheres to most all shapes and sizes of components, and .. |
|||
Specific Gravity | 3.20 g/cc | 3.20 g/cc | 70°C for 1,000 hrs; JIS-K-6220 |
Fujipoly Industries Sarcon® GR-Hn Gap Filler Pad Sarcon GR-n is a highly formable, thermally conductive gel material (no electicity conductive) in a versatile sheet form that easily fits and adheres to most all shapes and sizes of components, and .. |
|||
Specific Gravity | 3.20 g/cc | 3.20 g/cc | 120°C for 1,000 hrs; JIS-K-6220 |
Fujipoly Industries Sarcon® GR-Hn Gap Filler Pad Sarcon GR-n is a highly formable, thermally conductive gel material (no electicity conductive) in a versatile sheet form that easily fits and adheres to most all shapes and sizes of components, and .. |
|||
Specific Gravity | 3.20 g/cc | 3.20 g/cc | JIS-K-6220; ASTM D-792 |
Fujipoly Industries Sarcon® GR-Hn Gap Filler Pad Sarcon GR-n is a highly formable, thermally conductive gel material (no electicity conductive) in a versatile sheet form that easily fits and adheres to most all shapes and sizes of components, and .. |
|||
Specific Gravity | 3.20 g/cc | 3.20 g/cc | 150°C for 1,000 hrs with 90% RH; JIS-K-6220 |
Fujipoly Industries Sarcon® GR-Hn Gap Filler Pad Sarcon GR-n is a highly formable, thermally conductive gel material (no electicity conductive) in a versatile sheet form that easily fits and adheres to most all shapes and sizes of components, and .. |
|||
Specific Gravity | 3.20 g/cc | 3.20 g/cc | 60°C for 1,000 hrs with 90% RH; JIS-K-6220 |
Fujipoly Industries Sarcon® GR-m Gap Filler Pad Sarcon GR-m is a highly formable, thermally conductive gel material (no electicity conductive) in a versatile sheet form that easily fits and adheres to most all shapes and sizes of components, and .. |
|||
Specific Gravity | 3.20 g/cc | 3.20 g/cc | 120°C for 1,000 hrs; JIS-K-6220 |
Fujipoly Industries Sarcon® GR-m Gap Filler Pad Sarcon GR-m is a highly formable, thermally conductive gel material (no electicity conductive) in a versatile sheet form that easily fits and adheres to most all shapes and sizes of components, and .. |
|||
Specific Gravity | 3.20 g/cc | 3.20 g/cc | JIS-K-6220; ASTM D-792 |
Fujipoly Industries Sarcon® GR-m Gap Filler Pad Sarcon GR-m is a highly formable, thermally conductive gel material (no electicity conductive) in a versatile sheet form that easily fits and adheres to most all shapes and sizes of components, and .. |
|||
Specific Gravity | 3.20 g/cc | 3.20 g/cc | 150°C for 1,000 hrs; JIS-K-6220 |
Fujipoly Industries Sarcon® GR-m Gap Filler Pad Sarcon GR-m is a highly formable, thermally conductive gel material (no electicity conductive) in a versatile sheet form that easily fits and adheres to most all shapes and sizes of components, and .. |
|||
Specific Gravity | 3.20 g/cc | 3.20 g/cc | 60°C for 1,000 hrs with 90% RH; JIS-K-6220 |
Fujipoly Industries Sarcon® GR-n Gap Filler Pad Sarcon GR-n is a highly formable, thermally conductive gel material (no electicity conductive) in a versatile sheet form that easily fits and adheres to most all shapes and sizes of components, and .. |
|||
Specific Gravity | 3.20 g/cc | 3.20 g/cc | 70°C for 1,000 hrs; JIS-K-6220 |
Fujipoly Industries Sarcon® GR-n Gap Filler Pad Sarcon GR-n is a highly formable, thermally conductive gel material (no electicity conductive) in a versatile sheet form that easily fits and adheres to most all shapes and sizes of components, and .. |
|||
Specific Gravity | 3.20 g/cc | 3.20 g/cc | 120°C for 1,000 hrs; JIS-K-6220 |
Fujipoly Industries Sarcon® GR-n Gap Filler Pad Sarcon GR-n is a highly formable, thermally conductive gel material (no electicity conductive) in a versatile sheet form that easily fits and adheres to most all shapes and sizes of components, and .. |
|||
Specific Gravity | 3.20 g/cc | 3.20 g/cc | JIS-K-6220; ASTM D-792 |
Fujipoly Industries Sarcon® GR-n Gap Filler Pad Sarcon GR-n is a highly formable, thermally conductive gel material (no electicity conductive) in a versatile sheet form that easily fits and adheres to most all shapes and sizes of components, and .. |
|||
Specific Gravity | 3.20 g/cc | 3.20 g/cc | 150°C for 1,000 hrs with 90% RH; JIS-K-6220 |
Fujipoly Industries Sarcon® GR-n Gap Filler Pad Sarcon GR-n is a highly formable, thermally conductive gel material (no electicity conductive) in a versatile sheet form that easily fits and adheres to most all shapes and sizes of components, and .. |
|||
Specific Gravity | 3.20 g/cc | 3.20 g/cc | JIS-K-6220; ASTM D-792 |
Fujipoly Industries Sarcon® XR-j Gap Filler Pad Sarcon XR-e and XR-j are highly conformable/thermally conductive gel material (no electicity conductive) in a versatile sheet form that easily fits and adheres to most all shapes and sizes of compon.. |
|||
Specific Gravity | 3.20 g/cc | 3.20 g/cc | |
Inhance Fluoro-Seal INHANCE® Si-8220 Polymer Alloy Product Description: INHANCE S i-8000 series polymer alloy consists of black, medium density, silicon carbide chemically modified for greater adhesion. This product was designed for alloying with v.. |
|||
Specific Gravity | 3.20 g/cc | 3.20 g/cc | |
Inhance Fluoro-Seal INHANCE® Si-8900 Polymer Alloy Product Description: INHANCE S i-8000 series polymer alloy consists of black, medium density, silicon carbide chemically modified for greater adhesion. This product was designed for alloying with v.. |
|||
Specific Gravity | 3.20 g/cc | 3.20 g/cc | |
Inhance Fluoro-Seal INHANCE® Si-8500 Polymer Alloy Product Description: INHANCE S i-8000 series polymer alloy consists of black, medium density, silicon carbide chemically modified for greater adhesion. This product was designed for alloying with v.. |
|||
Specific Gravity | 3.20 g/cc | 3.20 g/cc | Mixed |
Tra-Con Tra-Duct 2705 Room Temperature Conductive Nickel Epoxy Adhesive TRA-DUCT 2705 is an electrically conductive nickel filled epoxy adhesive recommended for electronic bonding, sealing, and EMI-RFI shielding applications. This two-part smooth paste formulation is fr.. |
|||
Specific Gravity | 3.20 g/cc | 3.20 g/cc | Mixed |
Tra-Con Tra-Duct 2902 Room Temperature Conductive Silver Epoxy Adhesive TRA-DUCT 2902 is an electrically conducting silver-filled epoxy compound recommended for electronic bonding and sealing applications that require a combination of good mechanical and electrical prop.. |
|||
Specific Gravity | 3.20 - 3.90 g/cc | 3.20 - 3.90 g/cc | |
Parker Chomerics CHO-BOND 1038 Conductive Silicone RTV Adhesive Electrically conductive, one component silicone adhesive/sealant that may be used for bonding EMI gaskets or for providing EMI and environmental protection as a caulk. This material cures on exposur.. |
|||
Specific Gravity | 3.20 g/cc | 3.20 g/cc | ASTM D792 |
Parker Chomerics CHO-FORM 5531 EMI Shielding Material One component, moisture cure, form-in-place EMI gasketing material. This electrically conductive formulation contains silver-plated copper particles dispersed in a silicone elastomer. It is designed.. |
|||
Specific Gravity | 3.20 g/cc | 3.20 g/cc | |
Reade Advanced Materials Sillimanite Powder & Crystal (Al2SiO5) Description: Sillimanite is mineral composed of Aluminum and silicon pentoxide. It was named after the chemist B. Silliman (1779-1824). Sillimanite occurs throughout the world in metamorphosed peri-.. |