Inhance Fluoro-Seal INHANCE® Si-8500 Polymer Alloy

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer Inhance Fluoro-Seal
Trade Name INHANCE®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Inhance Fluoro-Seal INHANCE® Si-8500 Polymer Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Product Description: INHANCE S i-8000 series polymer alloy consists of black, medium density, silicon carbide chemically modified for greater adhesion. This product was designed for alloying with various polymer materials such as epoxy, polyurea, polyurethane etc. When incorporated in polymers, unique grades of high-performance polymeric composites are formed that have exceptional abrasion-resistance and wear performance. Frequently these composites have abrasion resistance greater than metal. They are also are light weight, non-corroding, and electrically non-conductive.Applications: Ideal applications include wear resistant parts that can be molded for severe service in mechanical or chemical environments, where repair/replacement of worn parts is very costly because of down time, and where optimal performance is needed. Examples include belt wipers, mining components, impact resistant products, screens, dumping pads, chute liners, valve seats, piston rings, gears, wear-plates, guide-rails, cable (protective jacketing), steel replacement parts, and high performance coatings.Information provided by Inhance/Fluoro-Seal, Ltd.
Physical Properties Metric English Comments
Specific Gravity 3.20 g/cc
3.20 g/cc
Bulk Density 1.28 g/cc
0.0462 lb/in³
Particle Size 25 µm
25 µm
average
Mechanical Properties Metric English Comments
Hardness, Knoop 2450
2450