Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.93 g/cc | 1.93 g/cc | ASTM D297 |
Greene Tweed CHEMRAZ® 505 Perfluoroelastomer Chemraz® 505, a perfluoroelastomer, provides a broader range of chemical resistance than any other compound on the market. With a temperature range of -22°F to 446°F (-30°C to 230°C).. |
|||
Specific Gravity | 1.93 g/cc | 1.93 g/cc | ASTM D297 |
Greene Tweed CHEMRAZ® 565 Perfluoroelastomer Chemraz®, a proprietary Greene, Tweed compound, has the broadest chemical resistance of any elastomeric material. Chemraz combines the resilience and sealing force of an elastomer with chemical r.. |
|||
Specific Gravity | 1.93 g/cc | 1.93 g/cc | ASTM D297 |
Greene Tweed CHEMRAZ® 550 Perfluoroelastomer Chemraz ® 550 is recommended for use in wet systems where chemical compatibility is required and small amounts of contamination are acceptable. This seal material has a wide variety of uses in d.. |
|||
Specific Gravity | 1.93 g/cc | 1.93 g/cc | |
Silberline Silvet® 420-20-P Silvet® P grades are recommended for use with engineering resins or transparent polymers where compatibility, maintenance of polymer clarity and distinctiveness of image (D.O.I.) observed from th.. |
|||
Specific Gravity | 1.93 g/cc | 1.93 g/cc | |
Silberline Silvet® 620-20-E Silvet® E grades are economical aluminum pigments provided in pellet form for easy handling and incorporation. They are composed of 80% aluminum pigment and 20% polyolefin and are compatible with.. |
|||
Specific Gravity | 1.93 g/cc | 1.93 g/cc | |
Silberline Silvet® 730-20-P Silvet® P grades are recommended for use with engineering resins or transparent polymers where compatibility, maintenance of polymer clarity and distinctiveness of image (D.O.I.) observed from th.. |
|||
Specific Gravity | 1.93 g/cc | 1.93 g/cc | |
Silberline Silvet® 790-20-P Silvet® P grades are recommended for use with engineering resins or transparent polymers where compatibility, maintenance of polymer clarity and distinctiveness of image (D.O.I.) observed from th.. |
|||
Specific Gravity | 1.93 g/cc | 1.93 g/cc | |
Silberline Silvet® 960-20-P Silvet® P grades are recommended for use with engineering resins or transparent polymers where compatibility, maintenance of polymer clarity and distinctiveness of image (D.O.I.) observed from th.. |
|||
Specific Gravity | 1.93 g/cc | 1.93 g/cc | |
Silberline Silvex® 223-20-C Silvex® C grades are aluminum pigment flakes dampened with a plasticizer to help prevent the individual flakes from becoming airborne during handling and processing. They are well suited for use .. |
|||
Specific Gravity | 1.93 g/cc | 1.93 g/cc | |
Silberline Silvex® 333-20-C Silvex® C grades are aluminum pigment flakes dampened with a plasticizer to help prevent the individual flakes from becoming airborne during handling and processing. They are well suited for use .. |
|||
Specific Gravity | 1.93 g/cc | 1.93 g/cc | |
Silberline Silvet® 460-20-P Silvet® P grades are recommended for use with engineering resins or transparent polymers where compatibility, maintenance of polymer clarity and distinctiveness of image (D.O.I.) observed from th.. |
|||
Specific Gravity | 1.93 g/cc | 1.93 g/cc | |
Silberline Silvex® 543-20-C Silvex® C grades are aluminum pigment flakes dampened with a plasticizer to help prevent the individual flakes from becoming airborne during handling and processing. They are well suited for use .. |
|||
Specific Gravity | 1.93 g/cc | 1.93 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ White LL8425 AP Concentrate Based In LLDPE DescriptionPOLYBATCH® LL8425 AP is an advanced performance white color concentrate containing 45% TiO2 in LLDPE. This product has been specifically engineered to provide improved resistance to phe.. |
|||
Specific Gravity | 1.93 g/cc | 1.93 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ White LL8844 GP DescriptionPOLYBATCH® LL8844 GP is a general purpose white color concentrate containing 45% TiO2 based in LLDPE. This product has been designed to provide color and opacity with good dispersion an.. |
|||
Specific Gravity | 1.93 g/cc | 1.93 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ White LL8425 AP Concentrate Based In LLDPE DescriptionPOLYBATCH® LL8425 AP is an advanced performance white color concentrate containing 45% TiO2 in LLDPE. This product has been specifically engineered to provide improved resistance to phe.. |
|||
Specific Gravity | 1.93 g/cc | 1.93 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ White LL8425 MG Concentrate Based In LLDPE DescriptionPOLYBATCH® LL8425 MG is an advanced performance white color concentrate containing 45% TiO2 in LLDPE. This product has been specifically engineered to provide improved resistance to phe.. |
|||
Specific Gravity | 1.93 g/cc | 1.93 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ White LL8425 AP Concentrate Based In LLDPE DescriptionPOLYBATCH® LL8425 AP is an advanced performance white color concentrate containing 45% TiO2 in LLDPE. This product has been specifically engineered to provide improved resistance to phe.. |
|||
Specific Gravity | 1.93 g/cc | 1.93 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ White LL8425 MG Concentrate Based In LLDPE DescriptionPOLYBATCH® LL8425 MG is an advanced performance white color concentrate containing 45% TiO2 in LLDPE. This product has been specifically engineered to provide improved resistance to phe.. |
|||
Specific Gravity | 1.93 g/cc | 1.93 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ White LL8425 MG Concentrate Based In LLDPE DescriptionPOLYBATCH® LL8425 MG is an advanced performance white color concentrate containing 45% TiO2 in LLDPE. This product has been specifically engineered to provide improved resistance to phe.. |
|||
Specific Gravity | 1.93 - 1.96 g/cc | 1.93 - 1.96 g/cc | ASTM D792 |
Adamas Adalon® 406 PTFE, 15% PEEK Information provided by Adamas, HPM |
|||
Specific Gravity | 1.93 g/cc | 1.93 g/cc | |
Bulk Molding Compounds BMC 501 Mineral Filled, Glass Fiber Reinforced Compound BMC 501 molding compound is a mineral filled glass-fiber-reinforced compound suitable for compression, transfer and stuffer injection molding. It provides the user with good electrical properties An.. |
|||
Specific Gravity | 1.93 - 1.95 g/cc | 1.93 - 1.95 g/cc | ASTM D792 |
Adamas Adalon® 703 PTFE, 15% Carbon Fiber Information provided by Adamas, HPM |
|||
Specific Gravity | 1.93 g/cc | 1.93 g/cc | ASTM D792 |
3M Dyneon™ THV 221AZ Fluoroplastic Agglomerate 3M™ Dyneon™ Fluoroplastic Agglomerate THV 221AZ is a flexible, transparent fluoroplastic composed of tetrafluoroethylene, hexafluoropropylene, and vinylidene fluoride in the form of agglomerate or.. |
|||
Specific Gravity | 1.93 g/cc | 1.93 g/cc | |
Bulk Molding Compounds BMC 610 Mineral Filled, Glass Reinforced Polyester Compound BMC 610 molding compound is a mineral filled, glass fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is set a part form other medium impact el.. |
|||
Specific Gravity | 1.93 g/cc | 1.93 g/cc | |
Silberline Sparkle Silvet® 790-20-E Sparkle Silvet® E grades are economical aluminum pigments provided in pellet form for easy handling and incorporation. They are composed of 80% aluminum pigment and 20% polyolefin and are compatibl.. |
|||
Specific Gravity | 1.93 g/cc | 1.93 g/cc | |
Silberline Sparkle Silvet® 880-20-E Sparkle Silvet® E grades are economical aluminum pigments provided in pellet form for easy handling and incorporation. They are composed of 80% aluminum pigment and 20% polyolefin and are compatibl.. |
|||
Specific Gravity | 1.93 g/cc | 1.93 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ White LL8425 AP Concentrate Based In LLDPE DescriptionPOLYBATCH® LL8425 AP is an advanced performance white color concentrate containing 45% TiO2 in LLDPE. This product has been specifically engineered to provide improved resistance to phe.. |
|||
Specific Gravity | 1.93 g/cc | 1.93 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ White LL8425 MG Concentrate Based In LLDPE DescriptionPOLYBATCH® LL8425 MG is an advanced performance white color concentrate containing 45% TiO2 in LLDPE. This product has been specifically engineered to provide improved resistance to phe.. |
|||
Specific Gravity | 1.93 g/cc | 1.93 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ White LL8844 GP DescriptionPOLYBATCH® LL8844 GP is a general purpose white color concentrate containing 45% TiO2 based in LLDPE. This product has been designed to provide color and opacity with good dispersion an.. |