Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.77 g/cc | 1.77 g/cc | ASTM D792 |
Noble Polymers Ecobarrier™ 2618 Thermoplastic Olefin (TPO) Ecobarrier is a TPO (thermoplastic olefin) produced by Noble Polymers based on olefin/elastomer compounding. Ecobarrier is primarily used as a sound barrier material in low heat applications.Informa.. |
|||
Specific Gravity | 1.77 - 1.83 g/cc | 1.77 - 1.83 g/cc | ASTM D 792 |
Karina E 42/268-FC-HSF MBU Red (OP) Color Concentrate Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.77 g/cc | 1.77 g/cc | ASTM D792 |
SABIC Innovative Plastics Valox® 780 PBT 40% gl/min, UL94 V-0 rated. Nonblooming flame retardant. Circuit breaker handles/housings, motor coil housings. |
|||
Specific Gravity | 1.77 g/cc | 1.77 g/cc | ASTM D792 |
SABIC Innovative Plastics Valox® 780 PBT (Asia Pacific) 40% gl/min, UL94 V-0 rated. Nonblooming flame retardant. Circuit breaker handles/housings, motor coil housings. |
|||
Specific Gravity | 1.77 - 1.78 g/cc | 1.77 - 1.78 g/cc | ISO R1183D |
Shanghai Ofluorine 9201F PVDF Powder for cables Description: Excellent mechanical properties, heat resistance and flame resistance, PVDF for cable can bear high temperature, corrosive chemicals etc harsh working environment, which has low smoke, .. |
|||
Specific Gravity | 1.77 - 1.78 g/cc | 1.77 - 1.78 g/cc | ISO R1183D |
Shanghai Ofluorine 9202F PVDF Powder for cables Description: Excellent mechanical properties, heat resistance and flame resistance, PVDF for cable can bear high temperature, corrosive chemicals etc harsh working environment, which has low smoke, .. |
|||
Specific Gravity | 1.77 - 1.79 g/cc | 1.77 - 1.79 g/cc | ASTM D792 |
Shanghai Ofluorine J-2 PVDF Extrusion Grade Description: J-2 PVDF is a kind of granules homopolymer, which has middle melt viscosity, J-2 is more suitable for extrusion process. J-2 PVDF pellets as raw materials, the finished products has exc.. |
|||
Specific Gravity | 1.77 - 1.79 g/cc | 1.77 - 1.79 g/cc | ASTM D792 |
Shanghai Ofluorine M-1 PVDF Molding Grade Description: M-1 PVDF is a kind of granules homopolymer, which has high melt viscosity, M-1 is more suitable for compression molding process. M-1 PVDF pellets as raw materials, the finished products.. |
|||
Specific Gravity | 1.77 - 1.79 g/cc | 1.77 - 1.79 g/cc | ASTM D792 |
Shanghai Ofluorine T-2 PVDF for Powder Coatings Description: T-2 PVDF belong to thermoplastic fluorocarbon resin, which has high melt flow rate, low melt viscosity. T-2 PVDF has characteristic of chemical resistance, heat resistance, high mechani.. |
|||
Specific Gravity | 1.77 - 1.79 g/cc | 1.77 - 1.79 g/cc | ASTM D792 |
Shanghai Ofluorine Z-1 PVDF Injection Grade Description: Z-1 PVDF is a kind of granular homopolymer, which has low melt viscosity, Z-1 is more suitable for injection molding. Z-1 PVDF pellets as raw materials, the finished products has excell.. |
|||
Specific Gravity | 1.77 g/cc | 1.77 g/cc | |
BYK Cloisite® 20A Nanoclay Cloisite® 20A is an additive for plastics to improve various plastic physical properties, such as reinforcement, HDT, CLTE and barrier.Information provided by Southern Clay ProductsSouthern Clay Pr.. |
|||
Specific Gravity | 1.77 - 1.80 g/cc | 1.77 - 1.80 g/cc | ASTM D792 |
Arkema Group KYNAR FLEX® 2850-02 Polyvinylidene Fluoride Copolymer - Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani.. |
|||
Specific Gravity | 1.77 - 1.80 g/cc | 1.77 - 1.80 g/cc | ASTM D792 |
Arkema Group KYNAR FLEX® 2850-04 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani.. |
|||
Specific Gravity | 1.77 - 1.79 g/cc | 1.77 - 1.79 g/cc | ASTM D792 |
Arkema Group KYNAR® 710, 710 HDP Polyvinylidene Fluoride Homopolymer- Injection Molding Characteristics: Natural resin - translucent, off-white hemispheres. HDP indicates higher color stability. High stability in harsh thermal, chemical and ultraviolet environments. High toughness .. |
|||
Specific Gravity | 1.77 - 1.79 g/cc | 1.77 - 1.79 g/cc | ASTM D792 |
Arkema Group KYNAR® 740 Black/Red Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion Characteristics: Pigmented. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeability, abrasion resistance; high purityAppli.. |
|||
Specific Gravity | 1.77 - 1.79 g/cc | 1.77 - 1.79 g/cc | ASTM D792 |
Arkema Group KYNAR® 740 Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili.. |
|||
Specific Gravity | 1.77 - 1.79 g/cc | 1.77 - 1.79 g/cc | ASTM D792 |
Arkema Group KYNAR® 740-02 Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. Flame and smoke suppressant. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mecha.. |
|||
Specific Gravity | 1.77 - 1.79 g/cc | 1.77 - 1.79 g/cc | ASTM D792 |
Arkema Group KYNAR® 760 Polyvinylidene Fluoride Homopolymer - Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili.. |
|||
Specific Gravity | 1.77 g/cc | 1.77 g/cc | |
Bulk Molding Compounds BMC 501E Mineral Filled, Glass Reinforced Polyester BMC 501E molding compound is a mineral filled, glass-fiber-reinforced polyester compound suitable for compression and transfer molding. It is a product with good overall electrical properties, flame.. |
|||
Specific Gravity | 1.77 g/cc | 1.77 g/cc | |
Bulk Molding Compounds BMC 620 Mineral Filled, Glass Fiber Reinforced Polyester Compound BMC 620 molding compound is a mineral filled, glass fiber-reinforced polyester compound suitable for compression, and stuffer injection molding It is characterized by good moldability high impact st.. |
|||
Specific Gravity | 1.77 g/cc | 1.77 g/cc | ASTM D792 |
Premix Premi-Glas® 1282-32 VE Glass Reinforced Vinyl Ester SMC
(discontinued **) Description: Premi-Glas® 1282-32 VE SMC is an enhanced high strength glass reinforced vinyl ester molding compound formulated for under-the-hood automotive applications.
Key features and benefi.. |
|||
Specific Gravity | 1.77 - 1.79 g/cc | 1.77 - 1.79 g/cc | ASTM D792 |
Shanghai Ofluorine 904 PVDF for water UF (ultrafiltration) Membranes Description: Ofluorine 904 PVDF Powder for water UF membranes has good solubility in some special solvent, which is a good raw material for PVDF UF membranes. Ofluorine 904 PVDF as raw materials, th.. |
|||
Specific Gravity | 1.77 - 1.80 g/cc | 1.77 - 1.80 g/cc | ASTM D792 |
Arkema Group KYNAR FLEX® 2850-00 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani.. |
|||
Specific Gravity | 1.77 - 1.80 g/cc | 1.77 - 1.80 g/cc | ASTM D792 |
Arkema Group KYNAR FLEX® 2850-07 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani.. |