Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.65 g/cc | 1.65 g/cc | ASTM D297 |
Process Technologies Inc Sanifluor® 1000 Formulated Aflas® Elastomer O-Rings, Gaskets and Seals produced from Sanifluor® 1000 have excellent chemical, heat and steam resistance. They provide superior performance in hot water, steam and virtually all caustics; makin.. |
|||
Specific Gravity | 1.65 g/cc | 1.65 g/cc | ASTM D792 |
Polymer Resources NY66-FRG25 Flame Retardant Nylon 66, 25% Glass Reinforced Nylon 66, 25% Glass Reinforced, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are.. |
|||
Specific Gravity | 1.65 - 1.75 g/cc | 1.65 - 1.75 g/cc | ISO 1183 |
Raschig Group AMPLA® 7250 melamine-modified polyester Cellulose reinforced melamine-modified Polyester molding compound. Very good electrical values, excellent heat resistance, excellent surface quality, low post shrinkage. This product meets the allow.. |
|||
Specific Gravity | 1.65 - 1.85 g/cc | 1.65 - 1.85 g/cc | ISO 1183 |
Raschig Group RALUPOL® 2100 UP Polyester Organically and inorganically filled polyester molding compound. Low post-shrinkage, very good electrical values, good mechanical strength. This product meets the allowed upper limits for heavy meta.. |
|||
Specific Gravity | 1.65 g/cc | 1.65 g/cc | ASTM D792 |
PolyOne Edgetek® XP9242701 Polyphenylene Sulfide (PPS) Injection Speed: 50 to 80% Holding Time: 3 to 9 sec Injection Time: 1 to 3 sec Cycle Time: 18 to 70 secInformation provided by PolyOne |
|||
Specific Gravity | 1.65 g/cc | 1.65 g/cc | ASTM D792 |
Polymer Resources NY66-G55 Nylon 66, 55% Glass Reinforced Nylon 66, 55% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are test.. |
|||
Specific Gravity | 1.65 g/cc | 1.65 g/cc | ISO 1183 |
Lehmann & Voss LUVOCOM® 1105-7938/GY PEEK, with glass fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension.. |
|||
Specific Gravity | 1.65 g/cc | 1.65 g/cc | ISO 1183 |
Lehmann & Voss LUVOCOM® 1850/GF/30/TF/15/BK PBT, with glass fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec.. |
|||
Specific Gravity | 1.65 g/cc | 1.65 g/cc | ISO 1183 |
GEHR Plastics PPS-40GF Polyphenylene Sulfide, 40% Glass Fiber The linear polyphenylensulfide belongs to the semi-crystalline materials and offers a very high mechanical capacity, thermal and chemical resistance distinguished at the same time, high dimensional .. |
|||
Specific Gravity | 1.65 g/cc | 1.65 g/cc | |
Momentive Performance Materials TSE3941 Flame Retardant Adhesive Sealant, White TSE3940 and TSE3941 flame retardant adhesive/sealants are non-flowable, one-component RTVs that cure quickly by reacting with atmospheric moisture forming a soft elastic silicone rubber. These mater.. |
|||
Specific Gravity | 1.65 g/cc | 1.65 g/cc | ASTM D792 |
SABIC Innovative Plastics Valox® 865 PBT (Europe-Africa-Middle East) VALOX 865 is a 30% glass fibre reinforced, non blooming flame retardant PBT+PET blend with an excellent surface appearance. Applications: External housings, steam irons, appliance housings and light.. |
|||
Specific Gravity | 1.65 g/cc | 1.65 g/cc | ASTM D792 |
SABIC Innovative Plastics Valox® IQ4860HR PBT Valox iQ* Resin iQ4860HR: Environmentally responsible iQ* PBT resin with 30% Glass reinforcement + UL94 V-0. Hydrolytically stable and impact modified. |
|||
Specific Gravity | 1.65 g/cc | 1.65 g/cc | |
Silberline EternaBrite® Premier 251 EternaBrite® Premier 251 is a fine, very bright, leafing aluminum pigment with excellent opacity and distinctness of image (D.O.I) for solvent based general industrial coatings. This grade is not.. |
|||
Specific Gravity | 1.65 g/cc | 1.65 g/cc | |
Silberline Sparkle Silver® Premier 331AR Sparkle Silver® Premier flakes provide more uniform surfaces than Sparkle Silver® products, and also sharper edges and controlled particle size distribution. "Sparkle Silver® Premier or Sil.. |
|||
Specific Gravity | 1.65 g/cc | 1.65 g/cc | ASTM D792 |
Saint-Gobain Meldin® 3140 Thermoplastic Bearing Material Meldin 3140 is an ideal thrust washer material and is well suited for thrust washer applications. Its high strength and stiffness, combined with its excellent heat dissipation properties, make it a.. |
|||
Specific Gravity | 1.65 g/cc | 1.65 g/cc | |
Aremco Ceramacoat™ 845-GRY High Temperature Ceramic-Inorganic Coating Single part, waterborne, silicon-filled, phosphate-bonded, gray coating for glass and quartz to 2000 ºF (1093 ºC). Primarily used for marking ceramic parts and coating automotive headlamps, stadiu.. |
|||
Specific Gravity | 1.65 - 1.95 g/cc | 1.65 - 1.95 g/cc | |
Parker Chomerics CHO-SHIELD® 598 A/B Silver-Epoxy Coating Silver-Epoxy Coating. This coating is a two-component, silver bearing, highly conductive epoxy paint designed to provide EMI shielding when applied to a plastic, non-conductive substrate. Used as a .. |