Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.60 g/cc | 1.60 g/cc | ASTM D792 |
Oxford Polymers 40GF 40% Glass Fiber Reinforced Polyphenylene Sulfide 40% Glass Fiber Reinforced Polyphenylene SulfideInformation provided by Oxford Polymers. |
|||
Specific Gravity | 1.60 g/cc | 1.60 g/cc | ASTM D792 |
PolyOne Nymax™ GF 1200 A 55 HS Black 13 Polyamide 66 (Nylon 66) The Nymax® GF 1200 Series of glass fiber-reinforced nylon 6/6 compounds have been specifically formulated for applications requiring high stiffness, tensile properties, heat resistance, and durabil.. |
|||
Specific Gravity | 1.60 g/cc | 1.60 g/cc | ASTM D792 |
LG Chemical Lupox® LW-5402 Low Warpage PBT, 40%Glass Filled, High Impact LUPOX semi-crystalline thermoplastic PBT resins exhibit properties including high strength, rigidity and good resistance to fatigue and creep at elevated temperatures. Furthermore, LUPOX resins sho.. |
|||
Specific Gravity | 1.60 g/cc | 1.60 g/cc | ISO 1183 |
Gromax BFG45-AS00N1 Nylon 6 46% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Specific Gravity | 1.60 g/cc | 1.60 g/cc | ISO 1183 |
Gromax BFG45-DN00N1 Nylon 6 46% Glass Filled (Conditioned) Information provided by Gromax Enterprises Corp. |
|||
Specific Gravity | 1.60 g/cc | 1.60 g/cc | ISO 1183 |
Gromax BFM40-DL04N1 Nylon 6 40% Mineral Filled (Conditioned) Information provided by Gromax Enterprises Corp. |
|||
Specific Gravity | 1.60 - 1.70 g/cc | 1.60 - 1.70 g/cc | ASTM D1475 |
Lotus Nano Paint NAX 01 Tow-Component Nano-paint Description: More durable and specific application methods. This paint is suitable for traffic signs on the road, cross-walks, warning vibrating lines and limited lot marking. Related machines could.. |
|||
Specific Gravity | 1.60 g/cc | 1.60 g/cc | ASTM D792 |
Haysite HTF Polyester, High Temp Flex HTF exhibits excellent flexibility and retention of electrical properties at elevated temperatures. For use in 220º C insulation systems in dry type transformers and where flexibility and high te.. |
|||
Specific Gravity | 1.60 g/cc | 1.60 g/cc | ISO 1183 |
Lehmann & Voss LUVOCOM® 1301-7869/BL PPS, linear, with glass fiber Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High-strength and stiff parts with low creep.High continuous use and heat distortion temperature. .. |
|||
Specific Gravity | 1.60 g/cc | 1.60 g/cc | ISO 1183 |
Gromax CFG45-PN11N1 Nylon 6 46% Glass Filled (Conditioned) Information provided by Gromax Enterprises Corp. |
|||
Specific Gravity | 1.60 g/cc | 1.60 g/cc | ASTM D 792 |
SABIC Innovative Plastics LNP Lubricomp KZL34 POM LNP* Lubricomp* KZL34 is a compound based on Acetal resin containing Milled Glass and PTFE. Characteristic of this grade is Internally Lubricated.This data was supplied by SABIC-IP for the Americas.. |
|||
Specific Gravity | 1.60 g/cc | 1.60 g/cc | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP PDXE98480 PEI LNP* Thermocomp* PDXE98480 is a compound based on Polyetherimide with Proprietary Fillers. Added feature of this grade: Reinforced. |
|||
Specific Gravity | 1.60 g/cc | 1.60 g/cc | ASTM D792 |
Teknor Apex Chemlon® 233 GVH Nylon 6, 33% Glass Fiber Reinforced Features: Flame Retardant; Good Stiffness; High Strength Processing Method: Injection Method Forms: Pellets Additive: Flame RetardantInformation Provided by Teknor Apex |
|||
Specific Gravity | 1.60 g/cc | 1.60 g/cc | ASTM D792 |
SABIC Innovative Plastics LNP VERTON EV008 PEI LNP* VERTON* EV008 is a compound based on Polyetherimide containing 40% Long Glass Fiber. Added feature of this grade is: Structural. |
|||
Specific Gravity | 1.60 g/cc | 1.60 g/cc | ASTM D-792 |
Saint-Gobain Norton® Fluorglas® Chemfilm® R128/R129 Premium Grade Extruded Full Density PTFE Film (0.004" thick) Description: Full Density Unsintered Tape is used as primary insulation for high-temperature wires, jackets and cables and wall for convoluted hose. It meets the requirements of component insulation.. |
|||
Specific Gravity | 1.60 g/cc | 1.60 g/cc | ASTM D792 |
A. Schulman POLYFLAM™ RCP 770C/CW DescriptionPolyflam® RCP 770C/CW is a flame-retardant concentrate based in low-density polyethylene that features excellent dispersion and processing stability up to 550°F.ApplicationRCP 770 C/CW.. |
|||
Specific Gravity | 1.60 g/cc | 1.60 g/cc | Mixed |
Tra-Con Tra-Cast 3143 Fire Retardant Epoxy Casting Compound TRA-CAST 3143 has a low viscosity and long pot life. It is certified to the requirements of UL 94 V-O, and is recommended for rigid potting, laminating, transformer encapsulating, filament winding a.. |
|||
Specific Gravity | 1.60 g/cc | 1.60 g/cc | ASTM D792 |
Daelim H&L Plavis MS Aromatic Polyimide, 15% MoS2 Filled, Machined Parts Available in vacuum or non-lubrication condition, very high abrasion resistance and low friction coefficient propertyInformation provided by Daelim H&L |
|||
Specific Gravity | 1.60 - 1.90 g/cc | 1.60 - 1.90 g/cc | IEC 1212-2 7.2 |
Hippe SI MP 21 Mica Paper Reinforced Silicone Resin - Round, Rolled Tube Used in mechanical, electrical and electronic applications. Good stability of electrical properties at elevated temperatures.Information provided by Hippe. |
|||
Specific Gravity | 1.60 g/cc | 1.60 g/cc | |
Radici Radiflam® S RV300AE (dry) Nylon 6 Radiflam® S is a range of flame retardant polyamides 6 (PA 6) used for injection molding and extrusion for all applications where high fire resistance is required.Information provided by Radici gro.. |
|||
Specific Gravity | 1.60 g/cc | 1.60 g/cc | Method A; ASTM D792 |
LNP Thermocomp® JF-1006 BK8-115 Polyethersulfone, Glass Fiber Reinforcement
(discontinued **) Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names.. |
|||
Specific Gravity | 1.60 g/cc | 1.60 g/cc | ASTM D792 |
Samsung Cheil Industries Infino® TK-2046H PCT, Glass Filled Information provided by Samsung Cheil Industries. |
|||
Specific Gravity | 1.60 g/cc | 1.60 g/cc | ASTM D792 |
PolyOne Edgetek® PS-20GF/000 FR Polybutylene Terephthalate (PBT), Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedIgnition ResistantUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation. |