Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.49 g/cc | 1.49 g/cc | ASTM D792 |
PolyOne LubriOne™ NN-30GF/15T Black Polyamide 66 (Nylon 66) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Specific Gravity | 1.49 g/cc | 1.49 g/cc | ASTM D792 |
PolyOne Nymax™ GMF 600 A 40 Storm Grey Polyamide 6 (Nylon 6) The Nymax® GMF 600 Series of compounds are based upon nylon 6 resins and select combinations of glass fiber and mineral reinforcements offering a unique balance of physical property and part perfor.. |
|||
Specific Gravity | 1.49 g/cc | 1.49 g/cc | ASTM D792 |
Ovation Polymers Nemcon™ H ES DP110/X3 Polycarbonate Alloy Polycarbonate alloy-Thermally conducting, electrically insulating grade with high HDT and improved processability.Information provided by Ovation Polymers |
|||
Specific Gravity | 1.49 g/cc | 1.49 g/cc | ASTM D792 |
PolyOne Geon™ Vinyl Flexible D6500 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Specific Gravity | 1.49 g/cc | 1.49 g/cc | ASTM D792 |
Polymer Resources NY6-M40 Nylon 6, 40% Mineral Filled Nylon 6, 40% Mineral Filled, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested .. |
|||
Specific Gravity | 1.49 g/cc | 1.49 g/cc | ISO 1183 |
Lehmann & Voss LUVOCOM® 50-7164/BL02 Polycarbonate, with glass fiber and PTFE Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Reduced moment of inertia compared with metal parts.Low warpag.. |
|||
Specific Gravity | 1.49 g/cc | 1.49 g/cc | ASTM D792 |
LG Chemical LUMID GP2430A(W) PA6+GF43%, General Purpose Feature: Injection Molding, PA6+GF43%, General PurposeApplication: Automotive (Air Intake Manifold, Cooling Fan)CAS No. 25038-54-4 and 65997-17-3Information provided by LG Chemical |
|||
Specific Gravity | 1.49 - 1.55 g/cc | 1.49 - 1.55 g/cc | NBR NM-IEC 60811-1-3 |
Karina E 02/5-FC-LMP Yellow Color Concentrate for PVC Color concentrate recommended for application in PVC compounds for electrical wires and cables. Also suitable for pigmentation of flexible and rigid PVC compounds for general purposes.Important con.. |
|||
Specific Gravity | 1.49 - 1.55 g/cc | 1.49 - 1.55 g/cc | ASTM D 792 |
Karina E 835-10/156-C-ERYB White PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.49 - 1.55 g/cc | 1.49 - 1.55 g/cc | ASTM D 792 |
Karina E 835-10/91-C-ERYB White PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.49 g/cc | 1.49 g/cc | ISO 1183 |
Lehmann & Voss LUVOCOM® 1105/GF/30/NAT-2 PEEK, with glass fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension.. |
|||
Specific Gravity | 1.49 g/cc | 1.49 g/cc | |
Sylvin Technologies 8980-80 Natural PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Specific Gravity | 1.49 - 1.55 g/cc | 1.49 - 1.55 g/cc | ASTM D792 |
Spartech Royalite R722 PVC Alloy Aircraft Grade Sheet Description: Aircraft Grade SheetInformation provided by Spartech. |
|||
Specific Gravity | 1.49 g/cc | 1.49 g/cc | |
Shin-Etsu Silicones FE-381U Fluorosilicone Elastomer ShinEtsu FE381 U is one of a series of high tensile, high tear fluorosilicone compounds. It is designed to process well in molding applications. It can be blended with other members of the series fo.. |
|||
Specific Gravity | 1.49 g/cc | 1.49 g/cc | ASTM D792 |
SPS Guang Zhou POBUXâ„¢ 3001G10 Flame-retarded/GF10%-PBT Characteristic: Good flame retardance, high mechanical properties, high rigidity, superior heat resistance, good dimensional stabilityApplications: E/E partsInformation Provided by SPS (Guang Zhou) .. |
|||
Specific Gravity | 1.49 g/cc | 1.49 g/cc | |
Silberline Aquasil® "BP" SN Silberline has specifically created Aquasil® BP grades for aqueous architectural and industrial maintenance coatings. This family offers a cost-effective alternative for achieving stability and .. |
|||
Specific Gravity | 1.49 g/cc | 1.49 g/cc | ASTM D 792 |
SABIC Innovative Plastics LNP Thermocomp OC008A PPS - Branched LNP* Thermocomp* OC008A is a compound based on Branched Polyphenylene Sulfide containing Carbon Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Specific Gravity | 1.49 g/cc | 1.49 g/cc | ASTM D792 |
SABIC Innovative Plastics LNP STAT-KON RE0069S PA 66 LNP* STAT-KON* RE0069S is a compound based on Nylon 66 resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive, Flame Retardant, Heat Stabilized. |
|||
Specific Gravity | 1.49 g/cc | 1.49 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ Blue 4012 Concentrate Based in Polyethylene DescriptionPOLYBATCH® 4012 is a blur color concentrate based in polyethylene. This concentrate was designed to provide opacity and color in polyolefin film and molding applications. POLYBATCH® 4.. |
|||
Specific Gravity | 1.49 g/cc | 1.49 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ Gardenia P80515PF Concentrate Based In Polypropylene DescriptionPOLYBATCH® P80515PF is a color matched white color concentrate based in polypropylene. This concentrate was designed to provide opacity and color in polypropylene film, extrusion, and m.. |
|||
Specific Gravity | 1.49 g/cc | 1.49 g/cc | ASTM D792 |
E-Polymers SEPAZ® V335HS 35% Glass Fiber Reinforced Heat Stabilized PPA Polyphthal Amide Resin (High Temperature Nylon): SEPAZ PPA is a unique semi-crystalline engineering plastic that bridges the cost-performance gap between traditional engineering thermoplastics and s.. |
|||
Specific Gravity | 1.49 g/cc | 1.49 g/cc | ASTM D792 |
3D Systems DuraForm® GF Glass Filled Nylon For use with all selective laser sintering (SLS®) systems.ApplicationsHousings and enclosuresConsumer sporting goodsAppropriate for low- to mid-volume rapid manufacturingParts requiring machining o.. |
|||
Specific Gravity | 1.49 g/cc | 1.49 g/cc | Method A; ASTM D792 |
LNP Lubricomp® OCL-4536 Polyphenylene Sulfide, Carbon Fiber Reinforced, PTFE + Silicone Lubricant
(discontinu Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac.. |