Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.32 g/cc | 1.32 g/cc | ASTM D792 |
Polymer Resources NY6/12-G33 Nylon 612, 33% Glass Reinforced Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide.. |
|||
Specific Gravity | 1.32 g/cc | 1.32 g/cc | ASTM D792 |
PolyOne Geon™ Vinyl Flexible 1351 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Specific Gravity | 1.32 g/cc | 1.32 g/cc | Part A; TM R050-16 |
Resinlab® EP1340 Medium Viscosity, Flame Retardant Epoxy Casting Resin System Resinlab™ EP1340 is a medium viscosity, flame retardant epoxy casting resin system. It is recognized under the Component Recognition Program of Underwriters Laboratories Inc., (File# E186034) for U.. |
|||
Specific Gravity | 1.32 g/cc | 1.32 g/cc | ASTM D792 |
2085A Polyurethane-based Biomedical Elastomer |
|||
Specific Gravity | 1.32 g/cc | 1.32 g/cc | |
Industrial Laminates/Norplex NP190 Synthetic Fabric
(discontinued **) Description: Aramid fabric material with a high performance phenolic resin matrix. Excellent electrical and mechanical properties at elevated temperatures, and in adverse environments. Applications .. |
|||
Specific Gravity | 1.32 g/cc | 1.32 g/cc | ISO 1183 |
Lehmann & Voss LUVOCOM® 20-8244 Polyphthalamide, with carbon fiber and glass fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Electrically conductive.. |
|||
Specific Gravity | 1.32 - 1.38 g/cc @Thickness 1.57 mm |
1.32 - 1.38 g/cc @Thickness 0.0620 in |
ASTM D792 |
Industrial Laminates/Norplex NP611 Paper Base Laminate Description: Hot punching general-purpose phenolic grade. Mechanical properties approach those of NP610 with improved electrical properties and moisture resistance.Thickness Tested: 0.062", 0 125" a.. |
|||
Specific Gravity | 1.32 g/cc | 1.32 g/cc | DIN 53479 |
Isoflon PEEK Polyetheretherketone Materials with strong mechanical and electrical performances under high temperatures.Information provided by Isoflon. |
|||
Specific Gravity | 1.32 g/cc | 1.32 g/cc | ASTM D792 |
SABIC Innovative Plastics LNP LUBRICOMP IBP34 PA6.12 LNP* LUBRICOMP* IBP34 is a compound based on Nylon 6/12 containing 20% Glass Bead, 15% PTFE/Silicone. Added features include: Wear Resistant. |
|||
Specific Gravity | 1.32 g/cc | 1.32 g/cc | ASTM D792 |
SABIC Innovative Plastics ULTEM AR9100 PEI (Asia Pacific) 10% Glass fiber filled, standard flow Polyetherimide (Tg 217C). Meets FAR 25.853 and OSU 65/65 with low toxicity, smoke, and flame evolution. ECO Conforming. |
|||
Specific Gravity | 1.32 g/cc | 1.32 g/cc | ASTM D792 |
SPS Guang Zhou PONYLâ„¢ EP4003G20 Non-halogen flame retardance/GF20%-PA66 Characteristic: Good flame retardance, high mechanical properties, superior heat resistance, good dimensional stabilityApplications: E/E partsInformation Provided by SPS (Guang Zhou) Ltd. |
|||
Specific Gravity | 1.32 g/cc | 1.32 g/cc | ASTM D792 |
SABIC Innovative Plastics LNP STAT-KON Ultem_UC1200 PEI (Europe-Africa-Middle East) LNP* Stat-kon* Ultem_UC1200 compound is a 12% carbon fiber reinforced PEI. High modulus with ESD characteristics for high-heat applications. |
|||
Specific Gravity | 1.32 g/cc | 1.32 g/cc | |
Shinil Chemical SHINNANO PA-6 Polymer Nanocomposite Air Intake Module SHINNANO is the product line of polymer nanocomposite made by dispersing nano fillers, mainly, NANOCLAY. Recently, Shinil has developed varios nanocomposite grades for automotive applications using.. |
|||
Specific Gravity | 1.32 g/cc | 1.32 g/cc | ASTM D792 |
Samsung Cheil Industries Infino® GP-3200G PBT/ABS, 20% Glass Filled PBT/ABS with 20% GF reinforcement that can be used in air-conditioner bladesInformation provided by Samsung Cheil Industries. |
|||
Specific Gravity | 1.32 g/cc | 1.32 g/cc | ASTM D792 |
Teknor Apex APEX® RE 8114 UV Polyvinyl Chloride, Rigid Forms: Pellets Additional Information: HDT, Unannealed; 264 psi, 0.125 in bars: 66.4°CInformation Provided by Teknor Apex |
|||
Specific Gravity | 1.32 g/cc | 1.32 g/cc | ASTM D792 |
SABIC Innovative Plastics LNP STAT-KON RE008 PA 66 LNP* STAT-KON* RE008 is a compound based on Nylon 66 containing 40% Carbon Fiber. Characteristics of this grade include: Electrically Conductive. |
|||
Specific Gravity | 1.32 g/cc | 1.32 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ Green 3011E Concentrate Based In Polyethylene DescriptionPOLYBATCH® 3011E is a green color concentrate based in polyethylene. This concentrate was designed to provide color in polyolefin film and molding applications. POLYBATCH® 3011E is he.. |
|||
Specific Gravity | 1.32 g/cc | 1.32 g/cc | |
Trelleborg E666 EPDM Rubber EPM -- EPDM or Ethylene -- Propylene Rubber. EPM can only be vulcanized by peroxides or radiation; whereas EPDM can be vulcanized conventionally using sulphur.Properties:Excellent inherent high and .. |
|||
Specific Gravity | 1.32 g/cc | 1.32 g/cc | ASTM D792 |
Colorite Polymers 2007NAT Rigid PVC Description: Colorite Polymers offers a wide range of rigid vinyl compounds for extrusion and injection molding applications for the medical industry. These compounds can be formulated for the produ.. |
|||
Specific Gravity | 1.32 g/cc @Temperature 25.0 °C |
1.32 g/cc @Temperature 77.0 °F |
|
Dow Corning 233 FLAKE RESIN Used as a powder coating binder or co-binder to improve heat stability and weatherability; colored baking enamels, decorative finishes; to increase hardness of other liquid silicone resins.Informati.. |
|||
Specific Gravity | 1.32 g/cc | 1.32 g/cc | ASTM D792 |
Colorite Polymers 8533 General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |
|||
Specific Gravity | 1.32 g/cc | 1.32 g/cc | ASTM D792 |
Colorite Polymers 9813 General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |
|||
Specific Gravity | 1.32 g/cc | 1.32 g/cc | ASTM D-792 |
Axiall 7803 Rigid PVC, Extrusion High Impact Profile Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.32 g/cc | 1.32 g/cc | ASTM D792 |
Samsung Cheil Industries Infino® GP-3200G PBT/ABS, 20% Glass Filled PBT/ABS with 20% GF reinforcement that can be used in air-conditioner bladesInformation provided by Samsung Cheil Industries. |