Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.17 g/cc | 1.17 g/cc | ASTM D792 |
Polymax® Maxelast® A9740 TPE, ABS/PC Overmold Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesInform.. |
|||
Specific Gravity | 1.17 g/cc | 1.17 g/cc | ASTM D792 |
PolyOne Geon™ Vinyl Flexible R108BM Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Specific Gravity | 1.17 g/cc | 1.17 g/cc | ASTM D792 |
Kolon ELLAS K-585A Caprolactone Based Thermoplastic Polyurethane ApplicationsInjectionIndustry Parts Information provided by API-Kolon. |
|||
Specific Gravity | 1.17 g/cc | 1.17 g/cc | ISO 2781 |
Lubrizol Advanced Materials PEARLTHANE® 11T92E Thermoplastic Polyurethane Elastomer Type: Pearlthane® 11T92E is a polycaprolactone copolyester-based thermoplastic polyurethane.Main Application : Extrusion/MouldingSpecial Features : Combining hardness with excellent mechanical pr.. |
|||
Specific Gravity | 1.17 g/cc | 1.17 g/cc | |
Momentive Performance Materials Addisilâ„¢ 1070 E Industrial Extrusion Heat Cured Rubber Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta.. |
|||
Specific Gravity | 1.17 g/cc | 1.17 g/cc | ASTM D792 |
Lubrizol Advanced Materials PEARLTHANE® 16N95UV Thermoplastic Polyurethane Elastomer PEARLTHANE® 16N95UV is a polyether-based TPU, containing an anti-UV additive, supplied in form of translucent, colorless pellets, combining hardness with excellent mechanical properties and excel.. |
|||
Specific Gravity | 1.17 g/cc | 1.17 g/cc | |
Momentive Performance Materials Addisilâ„¢ 470 E Healthcare Extrusion Grade Heat Cured Rubber Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta.. |
|||
Specific Gravity | 1.17 - 1.21 g/cc | 1.17 - 1.21 g/cc | ASTM D 792 |
Karina 500D48/1-A-IS-BZ Black PVC Compound Heavy metal free PVC compound recommended for injection of automotive parts.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.17 - 1.23 g/cc | 1.17 - 1.23 g/cc | ASTM D 792 |
Karina E 550D48/1 Black PVC Compound Shoe IndustryInformation provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.17 g/cc | 1.17 g/cc | +.02 |
Spartech E65060 General Purpose PVC First choice for compounds meeting the stringent requirements of Spiral Hose, Automotive, Housewares, Farm Equipment, Coated Fencing and numerous other applications including Lawn & Garden Wheels. B.. |
|||
Specific Gravity | 1.17 g/cc | 1.17 g/cc | |
Shin-Etsu Silicones X-30-783U Silicone Elastomer ShinEtsu X30783 U is a phenyl (PVMQ) silicone product. This product is designed for good low temperature characteristics. Product Features: A broad range of service temperatures from 100 to +260°.. |
|||
Specific Gravity | 1.17 g/cc | 1.17 g/cc | ASTM D792 |
Samsung Cheil Industries Starex® VH-0800 ABS, Unreinforced FR Flame-retardant ABS with excellent weather resistance that is used in the exterior of OA devices such as monitors, printers, fax machines, duplicators etc.Information provided by Samsung Cheil Indus.. |
|||
Specific Gravity | 1.17 g/cc | 1.17 g/cc | 23°C; ASTM D792 |
Teknor Apex APEX® 3300-60 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Sterilizable, Radiation Uses-Automotive Applications, Food Service Applications, General Purpose, Me.. |
|||
Specific Gravity | 1.17 g/cc | 1.17 g/cc | ASTM D792 |
Teknor Apex APEX® 583 Polyvinyl Chloride, Flexible Notes: RoHS Compliant Features: General Purpose Uses: Tubing; Wire Jacketing Agency Ratings: UL 498; UL 62 Wire Types: SPT-1; SPT-2 Processing Method: Injection MoldingForms: PelletsInformation Prov.. |
|||
Specific Gravity | 1.17 g/cc | 1.17 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ Light Blue 40442 Concentrate Based In LLDPE DescriptionPOLYBATCH® 40442 is a light blue color concentrate based in LLDPE. This concentrate was designed to provide color and opacity in blow molding applications. POLYBATCH® 40442 is typical.. |
|||
Specific Gravity | 1.17 g/cc | 1.17 g/cc | ASTM D792 |
A. Schulman SCHULAMID® 66 MV3FR Flame Retardant Nylon 6/6 Information provided by A. Schulman. |
|||
Specific Gravity | 1.17 g/cc | 1.17 g/cc | ASTM D792 |
ELASTO UK Dryflex® 602300S SEBS Based Material, Filled Qualities, 30A Hardness, Black The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material .. |
|||
Specific Gravity | 1.17 g/cc | 1.17 g/cc | ASTM D792 |
C.O.I.M. LARIPUR® LPR6260 PTMG Polyether Polyurethane Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion.. |
|||
Specific Gravity | 1.17 g/cc | 1.17 g/cc | Silicone Property; Arlon SQA-TMS-024 |
Arlon 920-10R##-P-1 Cured Self-Fusing Silicone Rubber Tape 1 inch wide, 20 mil thick, Red, Rectangular cross-section self-fusing silicone tape. Meets U.S. Military Specification A-A-59163 (supercedes Mil-I-46852C) except for packaging and sampling. The foll.. |
|||
Specific Gravity | 1.17 g/cc | 1.17 g/cc | ASTM D471; ISO 2781; DIN 53479 |
Advanced Polymer Alloys DURACRYN 8070 NC Thermoplastic Rubber Information provided by Advanced Polymer Alloys |
|||
Specific Gravity | 1.17 g/cc | 1.17 g/cc | ASTM D792 |
Bhansali Engineering Abstron AN450N Flame Retardant ABS Flame Retardant- V0 at 2.0mmInformation provided by Bhansali |
|||
Specific Gravity | 1.17 g/cc | 1.17 g/cc | ASTM D792 |
Asahi Kasei Thermylene® P7-30FG-0890 30% Glass Fiber Reinforced, UV Stabilized Information provided by Asahi Thermofil |
|||
Specific Gravity | 1.17 g/cc | 1.17 g/cc | Cured |
Tra-Con Tra-Bond FS411 Fast Cure Epoxy Adhesive System TRA-BOND FS-411 is an exceptional epoxy formulation recommended for lower temperature or wet industrial bonding applications where FAST CURING is required. It was designed to have low outgassing in .. |
|||
Specific Gravity | 1.17 g/cc | 1.17 g/cc | ASTM D792 |
LG Chemical HI835H PMMA, Impact Resistant Grade Molding granule designed for greater impact strength combined with the outstanding properties of conventional acrylic materialsFeatures: Excellent transparency and eleganceWeather resistance and che.. |