Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.00 g/cc | 1.00 g/cc | 23/23°C; ASTM D792 |
RheTech Products HP514-434 14% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 9648 Medium Dark Neutral Applications: Interior trimCenter consolesFuse panelsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Specific Gravity | 1.00 g/cc | 1.00 g/cc | 23/23°C; ASTM D792 |
RheTech Products HP521-00UV 15% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, Natural Applications: Interior trimIP structural componentsCenter consolesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Specific Gravity | 1.00 g/cc | 1.00 g/cc | 23/23°C; ASTM D792 |
RheTech Products HP521-229 15% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 195A Medium Neutral Applications: Interior trimIP structural componentsScuff/kick platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Specific Gravity | 1.00 g/cc | 1.00 g/cc | ASTM D792 |
Polymax® Maxelast® P3896 TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Specific Gravity | >= 1.00 g/cc | >= 1.00 g/cc | |
Parker Chomerics CHO-BOND 1067, Part A Silicone Resin Mixture Information provided by Chomerics |
|||
Specific Gravity | >= 1.00 g/cc | >= 1.00 g/cc | |
Parker Chomerics CHO-FORM 5525, Part A Silicone Information provided by Chomerics |
|||
Specific Gravity | 1.00 g/cc | 1.00 g/cc | |
Parker Chomerics CHO-BOND 2166 Part A Silicone Information provided by Chomerics |
|||
Specific Gravity | 1.00 g/cc | 1.00 g/cc | Uncured |
Permabond F201 Anaerobic Retainer Permabond® F201 is an anaerobic adhesive which has been developed to give excellent resistance to peel and impact forces. This toughening, combined with good adhesion to aluminum and copper alloys,.. |
|||
Specific Gravity | 1.00 g/cc | 1.00 g/cc | |
LG Chemical DCPD Structure & Characteristics: Dimer of cyclopentadiene. Purified after Isolating from pyrolysis oil evolved during NCC pyrolysis processUses: Used during manufacturing of unsaturated polyester resin .. |
|||
Specific Gravity | 1.00 g/cc | 1.00 g/cc | ASTM D792 |
LG Chemical LUPOL GP-1000FA General Purpose Polypropylene, High Impact, Flame Retardant, Non-Bleed LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive: Bumper cover, instrument panel, glove box, air cleaner.. |
|||
Specific Gravity | 1.00 - 1.05 g/cc | 1.00 - 1.05 g/cc | LSY-QB-ID002 |
LG Chemical Lutex 704 SBR Latex Description: Binding Force, Print gloss, High Shear Rheology, Coater RunnabilityApplication: Art Paper-Single, Pre-Film, Blade Coater, Adhesive coated paper and Carpet back-coating adhesiveCSA No. 7.. |
|||
Specific Gravity | 1.00 - 1.02 g/cc | 1.00 - 1.02 g/cc | |
Michelman® Licomer® W 483 Nonionic montan emulsion Description: Nonionic montan emulsionUsage: Licomer® W 483 is a high gloss concentrated emulsion, used for dry-bright polishes.Information provided by Michelman® |
|||
Specific Gravity | 1.00 - 1.10 g/cc | 1.00 - 1.10 g/cc | ASTM D792 |
Loxim 820 12 HB Polypropylene Compound, Flame Retardant Information provided by Loxim Industries |
|||
Specific Gravity | 1.00 g/cc | 1.00 g/cc | |
Shin-Etsu Silicones KE-3472T Silicone, RTV Conformal Coating Information Provided by Shin-Etsu Silicones of America, Inc. |
|||
Specific Gravity | 1.00 g/cc | 1.00 g/cc | ASTM D792 |
Teknor Apex TEKBOND® 6000-60 Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Specific Gravity | 1.00 g/cc | 1.00 g/cc | ASTM D792 |
Teknor Apex TEKBOND® MP 1728 UVF Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Specific Gravity | 1.00 g/cc | 1.00 g/cc | ASTM D792 |
Teknor Apex Telcar® TL-1050-75 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Specific Gravity | 1.00 g/cc | 1.00 g/cc | ASTM D792 |
A. Schulman POLYFORT™ FPP 2067HU UV Stabilized, High Heat Resistant Impact Polypropylene DescriptionPolyfort® FPP 2067HU is a unique high flow, UV stabilized high heat resistant impact polypropylene available in matched automotive colors. It molds to a fine appearance with good scrat.. |
|||
Specific Gravity | 1.00 g/cc | 1.00 g/cc | ASTM D792 |
A. Schulman POLYFORT™ FPP 3716 Talc Filled Copolymer Polypropylene DescriptionPolyfort® FPP 3716 is a 12% talc filled copolymer polypropylene product. Information provided by A. Schulman. |
|||
Specific Gravity | 1.00 g/cc | 1.00 g/cc | |
Dow Corning SYL-OFF® 1171A CATALYST Syl-Off® 1171A Catalyst Emulsion is a 50% solids emulsion of an organotin catalyst in water. Suitable for use with Syl-Off® 1181 Emulsion Coating.Information provided by Dow Corning |
|||
Specific Gravity | 1.00 g/cc | 1.00 g/cc | |
Dow Corning SYL-OFF® SL 7688 CROSSLINKER Minimizes mist at speeds up to 1600 m/min, good anchorage to and stability with many paper substrates, suitable for lamination with a variety of adhesives.Information provided by Dow Corning |
|||
Specific Gravity | 1.00 g/cc @Temperature 15.6 - 25.0 °C |
1.00 g/cc @Temperature 60.1 - 77.0 °F |
|
Dow Corning 1250 SURFACTANT 50% silicone resin in Xylene solvent. Silicone Profoamer for mechanically frothing PVC dispersions. Good foam control for PVC foam coatings. Better water resistance and less odor than alkali metal s.. |
|||
Specific Gravity | 1.00 g/cc | 1.00 g/cc | Uncatalyzed, QM CAT PURPLE |
ACC QM128 QSI Quantum Silicones 28 Durometer Condensation Cured Moldmaking Material QM 128 is a two-component, room temperature condensation cure silicone material. The cured rubber has excellent mechanical properties and shelf-life stability. This material is an excellent choice f.. |
|||
Specific Gravity | 1.00 g/cc | 1.00 g/cc | Uncatalyzed, Moldmaster Red |
ACC QM 2125 QSI Quantum Silicones 25 Durometer Condensation Cure Moldmaking Material QM 2125 is a two-component, room temperature condensation cure silicone material. The cured rubber has excellent mechanical properties and good shelf-life stability. This material is an excellent ch.. |
|||
Specific Gravity | 1.00 g/cc | 1.00 g/cc | ASTM D792 |
PolyOne Synprene® IT 37-035 Thermoplastic Elastomer - SBC, Mineral Filled
(discontinued **) Description/Features:Multi-Purpose Thermoplastic ElastomerMineral FilledUV StabilizedApplications:General PurposeMarket:Consumer GoodsIndustrialProcessing Method:Injection MoldingPolyOne First Choic.. |
|||
Specific Gravity | 1.00 g/cc | 1.00 g/cc | Uncatalyzed, QM CAT BLUE |
ACC QM 113 QSI Quantum Silicones 13 Durometer Condensation Cured Moldmaking Material QM 113 is a two component, room temperature condensation cure silicone material. The cured rubber is very soft, has excellent mechanical properties and good shelf-life stability. This material is an.. |
|||
Specific Gravity | 1.00 g/cc | 1.00 g/cc | Uncatalyzed, QM CAT PURPLE |
ACC QM 113 QSI Quantum Silicones 13 Durometer Condensation Cured Moldmaking Material QM 113 is a two component, room temperature condensation cure silicone material. The cured rubber is very soft, has excellent mechanical properties and good shelf-life stability. This material is an.. |
|||
Specific Gravity | 1.00 g/cc | 1.00 g/cc | 23/23°C; ASTM D792 |
RheTech Products HP522-357 15% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, JA6A Black Applications: Center consolesAir vents louversInterior trimInjection molding conditions reported in table.Information provided by RheTech Products. |