Polymer Property : Linear Mold Shrinkage, Flow = 0.0085 in/in Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Flow 0.0085 - 0.0125 cm/cm
0.0085 - 0.0125 in/in
LATI Larpeek 50 PEEK
Polyetheretherketone (PEEK). Unfilled. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; Asia Pacific; Europe;..
Linear Mold Shrinkage, Flow 0.0085 - 0.011 cm/cm
0.0085 - 0.011 in/in
LATI Latamid 68 H2-V0 PA6/PA66 copolymer, Heat Stabilized, Flame Retardant
PA6/PA66 copolymer (PA6/PA66) based compound. Heat stabilized. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Good surface appearance.Availability: Africa & Middle Ea..
Linear Mold Shrinkage, Flow 0.0085 cm/cm
0.0085 in/in
Solvay TECHNYL® A 230 V13 PA66, 13% glass fiber, DRY
Description: Modified polyamide 66, reinforced with 13% of glass fiber, with improved impact resistance, for injection molding.Available in: Europe and North AmericaProduct Applications: In addition..
Linear Mold Shrinkage, Flow 0.0085 cm/cm
0.0085 in/in
Solvay TECHNYL® A 238 V13 PA66, 13% glass fiber, DRY
Description: Polyamide 66, reinforced with 13% of glass fiber, heat stabilized, with improved impact resistance, for injection molding.Available in: Europe, Latin America and North AmericaProduct Ap..
Linear Mold Shrinkage, Flow 0.0085 cm/cm

@Time 86400 sec
0.0085 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP STAT-KON DX12411C PC
LNP* STAT-KON* DX12411C is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this material include: Electrically Conductive, Clean Compounding System.
Linear Mold Shrinkage, Flow 0.0085 - 0.0095 cm/cm
0.0085 - 0.0095 in/in
ISO DIS 294-4
Wellman Wellamid® GF10-66/6-LI6-NBK4 10% Glass Reinforced, Toughened Nylon 66/6
Description: Glass Reinforced, Toughened Nylon 66/6Information provided by Wellman.
Linear Mold Shrinkage, Flow 0.0085 cm/cm
0.0085 in/in
BASF Procom® D 1118 Polypropylene
Data was collected by ISO methods and provided by BASF.
Linear Mold Shrinkage, Flow 0.0085 cm/cm
0.0085 in/in
BASF Procom® D 1173 Polypropylene
Data was collected by ISO methods and provided by BASF.
Linear Mold Shrinkage, Flow 0.0085 cm/cm
0.0085 in/in
ISO 2577, 294-4
BASF Ultrason® E 3010 MR UN PESU
Description: Unreinforced, higher viscosity injection molding and extrusion grade with improved toughness and chemical resistance (stress crack resistance); demolding optimized. Abbreviated designat..
Linear Mold Shrinkage, Flow 0.0085 cm/cm
0.0085 in/in
BASF Procom® X10S 773 Polypropylene
Car bumpers and spoilers where good paintability is required.Data was collected by ISO methods and provided by BASF.
Linear Mold Shrinkage, Flow 0.0085 cm/cm
0.0085 in/in
ISO Data
BASF Ultrason E 3010 PES
Ultrason E 3010 is an unfilled, higher viscosity injection molding and extrusion PES grade, tougher and with improved chemical resistance.