Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.0040 - 0.0065 cm/cm | 0.0040 - 0.0065 in/in | ASTM D955 |
Star Plastics PC/ABSFR9001 Molding Grade PC/ABSFR Information provided by Star Plastics, Inc. |
|||
Linear Mold Shrinkage | 0.0050 - 0.0065 cm/cm | 0.0050 - 0.0065 in/in | Compression specimen; IS 13411-1992 |
Amity Thermosets ATO 176 Phenolic Molding Organic and inorganic Filler, Compression Molded Characteristics:Heat resistant ( asbestos free )Good electric insulationLow shrinkageLow water absorptionMedium mechanical strengthNot suitable for high mechanical tensionColor-blackMedium flow App.. |
|||
Linear Mold Shrinkage | 0.0060 - 0.0065 cm/cm | 0.0060 - 0.0065 in/in | ASTM D955 |
PolyOne Edgetek® AM-30GM/15TF Polyphthalamide (PPA), Glass Filled, PTFE Lubricated
(discontinued **) Description/Features:Glass Fiber ReinforcedPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |