Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.00100 - 0.00200 cm/cm | 0.00100 - 0.00200 in/in | ASTM D955 |
Niche Polymer PPHT20BK Homopolymer PP, 20% Talc Fiber Filled Information provided by Niche Polymer |
|||
Linear Mold Shrinkage | 0.000500 - 0.00200 cm/cm | 0.000500 - 0.00200 in/in | Average value: 0.00107 cm/cm Grade Count:4 |
Overview of materials for Polyetherketoneetherketoneketone (PEKEKK), Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetherketoneetherketoneketone (PEKEKK), Carbon Fiber Filled". Each property range of values reported .. |
|||
Linear Mold Shrinkage | 0.00100 - 0.00200 cm/cm | 0.00100 - 0.00200 in/in | Average value: 0.00144 cm/cm Grade Count:6 |
Overview of materials for PPE/PPO + Carbon Fiber This property data is a summary of similar materials in the MatWeb database for the category "PPE/PPO + Carbon Fiber". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Linear Mold Shrinkage | 0.000500 - 0.00200 cm/cm | 0.000500 - 0.00200 in/in | Average value: 0.00118 cm/cm Grade Count:7 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 40% Glass Fiber Filled". Specific grades with glass content betwe.. |
|||
Linear Mold Shrinkage | 0.000500 - 0.00200 cm/cm | 0.000500 - 0.00200 in/in | Average value: 0.00119 cm/cm Grade Count:8 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 30% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 30% Carbon Fiber Filled". Specific grades with carbon fiber conte.. |
|||
Linear Mold Shrinkage | 0.00100 - 0.00200 cm/cm | 0.00100 - 0.00200 in/in | Average value: 0.00150 cm/cm Grade Count:3 |
Overview of materials for Polycarbonate, Carbon + Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Carbon + Glass Fiber Reinforced". Each property range of values reported is minimum and m.. |
|||
Linear Mold Shrinkage | 0.000 - 0.00200 cm/cm | 0.000 - 0.00200 in/in | Average value: 0.000869 cm/cm Grade Count:12 |
Overview of materials for Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled". Specific grades with glass content between 45% an.. |
|||
Linear Mold Shrinkage | 0.000100 - 0.00200 cm/cm | 0.000100 - 0.00200 in/in | Average value: 0.000593 cm/cm Grade Count:15 |
Overview of materials for Liquid Crystal Polymer (LCP), Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), Carbon Fiber Filled". Each property range of values reported is minimum an.. |
|||
Linear Mold Shrinkage | 0.000 - 0.00200 cm/cm | 0.000 - 0.00200 in/in | Average value: 0.000760 cm/cm Grade Count:5 |
Overview of materials for Phenolic, Carbon Fiber Composite This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Carbon Fiber Composite". Each property range of values reported is minimum and maximum values .. |
|||
Linear Mold Shrinkage | 0.000200 - 0.00200 cm/cm | 0.000200 - 0.00200 in/in | Average value: 0.00110 cm/cm Grade Count:17 |
Overview of materials for Polyphenylene Sulfide (PPS) with 20% Carbon Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 20% Carbon Fiber Filler". Specific grades with carbon fiber content bet.. |
|||
Linear Mold Shrinkage | 0.000500 - 0.00200 cm/cm | 0.000500 - 0.00200 in/in | Average value: 0.000692 cm/cm Grade Count:11 |
Overview of materials for Polyphenylene Sulfide (PPS) with 40% Carbon Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 40% Carbon Fiber Filler". Specific grades with carbon fiber content bet.. |
|||
Linear Mold Shrinkage | 0.00200 - 0.00200 cm/cm @Temperature 80.0 - 80.0 °C |
0.00200 - 0.00200 in/in @Temperature 176 - 176 °F |
Average value: 0.00200 cm/cm Grade Count:6 |
Overview of materials for Nylon 6, 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. E.. |
|||
Linear Mold Shrinkage | 0.000100 - 0.00200 cm/cm | 0.000100 - 0.00200 in/in | Average value: 0.000875 cm/cm Grade Count:4 |
Overview of materials for Acrylic/Polycarbonate Alloy, Carbon Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Acrylic/Polycarbonate Alloy, Carbon Fiber Filler". Each property range of values reported is minimum and.. |
|||
Linear Mold Shrinkage | 0.00100 - 0.00200 cm/cm | 0.00100 - 0.00200 in/in | Average value: 0.00175 cm/cm Grade Count:3 |
Overview of materials for Polyethylene Terephthalate (PET), 60% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 60% Glass Reinforced". Specific grades with glass content between 55% .. |