Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.0052 cm/cm | 0.0052 in/in | ASTM D955 |
Multibase Multi-Flex® TPE A 7699 BLK Multi-Flex® A 7699 is an acoustic barrier compound for medium density applications . Multi-Flex® TPE compounds are based on Shell Kraton G polymers licensed to Multibase. Multi-Flex TPE contains.. |
|||
Linear Mold Shrinkage | 0.0052 cm/cm | 0.0052 in/in | ASTM D955 |
RheTech Products G10P100-00 10% Glass Fiber Reinforced Polypropylene, Natural Applications: BracketsIP structural componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Linear Mold Shrinkage | 0.0052 cm/cm | 0.0052 in/in | ASTM D955 |
RheTech Products G10P100-01 10% Glass Fiber Reinforced Polypropylene, Black Applications: BracketsIP structural componentsDome light housingInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Linear Mold Shrinkage | 0.0052 cm/cm | 0.0052 in/in | ASTM D955 |
RheTech Products G10P100-01UV 10% Glass Fiber Reinforced Polypropylene, UV Stabilized, Black Applications: BracketsIP structural componentsDome light housingInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Linear Mold Shrinkage | 0.0052 cm/cm | 0.0052 in/in | ASTM D955 |
RheTech Products GC10P100-00 10% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Natural Applications: Air ducts - distributionFuel filler pocketsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Linear Mold Shrinkage | 0.0052 cm/cm | 0.0052 in/in | ASTM D955 |
RheTech Products GC10P100-01 10% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Black Applications: Air ducts - distributionFuel filler pocketsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Linear Mold Shrinkage | 0.0052 cm/cm | 0.0052 in/in | |
Plastcom SLOVAMID 6 GF 25 FRC 3 PA6, 25% glass fibre, flame retardant FeaturesPA 6 for injection moulding, chemically strengthened with 25 % glass fibre. Application: impacted mouldings and mouldings with high strength applied in automotive, electrical, engineering an.. |
|||
Linear Mold Shrinkage | 0.0052 cm/cm | 0.0052 in/in | STN 64 0808 |
Plastcom SLOVAMID 66 GF 25 FRG 5 Polyamide 66, 25% Glass Fiber, Halogen Free Flame Retardant FeaturesPA 66 for injection moulding, chemical reinforced with 25% glass fiber and non-halogen flame retardant, with heat and flammability resistance, achieves V-0 in accordance with UL 94. Non-hal.. |
|||
Linear Mold Shrinkage | 0.0052 cm/cm | 0.0052 in/in | |
Plastcom SLOVAMID 66 GF 25 FRG 5 TS PA66, 25% glass fibre, flame retardant FeaturesPA 66 for injection moulding, chemically reinforced with 25% glass fibre and non-halogen flame retardant, with heat resistance and nonflammability, achieves V 0 in accordance with UL 94. Non.. |
|||
Linear Mold Shrinkage | 0.0052 cm/cm | 0.0052 in/in | STN 64 0808 |
Plastcom SLOVAMID 66 GF 25 FRI 3 Polyamide 66, 25% Glass Fiber, Halogen Free Flame Retardant FeaturesPA 66 for injection moulding, chemically reinforced with 25% glass fiber and non-halogen flame retardant, with heat and flammability resistance, achieves V-0 in accordance with UL 94. Non-h.. |
|||
Linear Mold Shrinkage | 0.0052 cm/cm | 0.0052 in/in | |
Plastcom SLOVAMID 66 GF 25 FRI 3 TS PA66, 25% glass fibre, flame retardant FeaturesPA 66 for injection moulding, chemically reinforced with 25% glass fibre and non-halogen flame retardant, with heat resistance and nonflammability, achieves V 0 in accordance with UL 94. Non.. |
|||
Linear Mold Shrinkage | 0.0052 cm/cm | 0.0052 in/in | |
Plastcom SLOVAMID 66 GF 30 FRG 5 PA66, 30% glass fibre, flame retarder FeaturesPA 66 for injection moulding, chemically reinforced with 30 % glass fibre and non-halogen flame retardant, with heat resistance and nonflammability, achieves V 0 /0,8 mm/ in accordance with .. |
|||
Linear Mold Shrinkage | 0.0052 cm/cm | 0.0052 in/in | STN 64 0808 |
Plastcom SLOVAMID 66 GF 35 FRG 5 Polyamide 66, 35% Glass Fiber, Halogen Free Flame Retardant FeaturesPA 66 for injection moulding, chemical reinforced with 35% glass fiber and non-halogen flame retardant, with heat and flammability resistance, achieves V-0 in accordance with UL 94. Non-hal.. |
|||
Linear Mold Shrinkage | 0.0052 cm/cm | 0.0052 in/in | |
Plastcom SLOVAMID 66 Y 35 FRY 7 PA66, 35% mineral filling FeaturesPA 66 for injection moulding, chemically reinforced with 35 % mineral filler and non-halogen flame retardant, with heat resistance and nonflammability, achieves V 0 /3.2 mm/ in accordance wi.. |
|||
Linear Mold Shrinkage | 0.0052 cm/cm | 0.0052 in/in | ASTM D955 |
Plenco 1508 Polyester, Briquette, Injection Molded PLENCO 01508 is a mineral filled pelletized polyester molding compound, which offers excellent heat resistance and electrical properties. UL recognized under component file E40654. 01508 is availabl.. |
|||
Linear Mold Shrinkage | 0.0052 cm/cm @Thickness 3.175 mm |
0.0052 in/in @Thickness 0.1250 in |
ASTM D955 |
A. Schulman ComAlloy® E-13819 Heat Dissipative PPS Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Linear Mold Shrinkage | 0.0052 cm/cm | 0.0052 in/in | ASTM D955 |
Plenco 4548 Phenolic, Granular, Transfer Molded PLENCO 04548 is a heat resistant mineral filled phenolic molding compound, offering fast cure rates and hot rigidity. Type ASTM 5948 CFG, and UL recognized under component file E40654. 04548 is avai.. |
|||
Linear Mold Shrinkage | 0.0052 cm/cm @Thickness 3.175 mm |
0.0052 in/in @Thickness 0.1250 in |
ASTM D955 |
A. Schulman ComAlloy® E-13819 Heat Dissipative PPS Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Linear Mold Shrinkage | 0.0052 cm/cm @Thickness 3.175 mm |
0.0052 in/in @Thickness 0.1250 in |
ASTM D955 |
A. Schulman ComAlloy® E-13819 Heat Dissipative PPS Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Linear Mold Shrinkage | 0.0052 cm/cm @Thickness 3.175 mm |
0.0052 in/in @Thickness 0.1250 in |
ASTM D955 |
A. Schulman ComAlloy® E-13819 Heat Dissipative PPS Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Linear Mold Shrinkage | 0.0052 cm/cm @Thickness 3.175 mm |
0.0052 in/in @Thickness 0.1250 in |
ASTM D955 |
A. Schulman ComAlloy® E-13819 Heat Dissipative PPS Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Linear Mold Shrinkage | 0.0052 cm/cm @Thickness 3.175 mm |
0.0052 in/in @Thickness 0.1250 in |
ASTM D955 |
A. Schulman ComAlloy® E-13819 Heat Dissipative PPS Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |