Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.000100 - 0.0200 cm/cm | 0.000100 - 0.0200 in/in | ASTM D955 |
Niche Polymer PPHM15BK Homopolymer PP Information provided by Niche Polymer |
|||
Linear Mold Shrinkage | 0.000100 - 0.0200 cm/cm | 0.000100 - 0.0200 in/in | ASTM D955 |
Niche Polymer PPHM6BK Homopolymer PP Information provided by Niche Polymer |
|||
Linear Mold Shrinkage | 0.000100 - 0.00600 cm/cm | 0.000100 - 0.00600 in/in | Average value: 0.00250 cm/cm Grade Count:54 |
Overview of materials for Polyphthalamide (PPA), 50% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 50% Glass Fiber Reinforced". Each property range of values reported is minimum and maxi.. |
|||
Linear Mold Shrinkage | 0.000100 - 0.00260 cm/cm | 0.000100 - 0.00260 in/in | Average value: 0.00117 cm/cm Grade Count:3 |
Overview of materials for Polystyrene, Wood Filled This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Wood Filled". Each property range of values reported is minimum and maximum values of appro.. |
|||
Linear Mold Shrinkage | 0.000100 - 0.00300 cm/cm | 0.000100 - 0.00300 in/in | Average value: 0.00150 cm/cm Grade Count:18 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), NCG Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), NCG Fiber Filled". Each property range of values reported is mini.. |
|||
Linear Mold Shrinkage | 0.000100 - 0.00200 cm/cm | 0.000100 - 0.00200 in/in | Average value: 0.000593 cm/cm Grade Count:15 |
Overview of materials for Liquid Crystal Polymer (LCP), Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), Carbon Fiber Filled". Each property range of values reported is minimum an.. |
|||
Linear Mold Shrinkage | 0.000100 - 0.0140 cm/cm | 0.000100 - 0.0140 in/in | Average value: 0.00727 cm/cm Grade Count:51 |
Overview of materials for Polyimide This property data is a summary of similar materials in the MatWeb database for the category "Polyimide". Each property range of values reported is minimum and maximum values of appropriate MatWeb e.. |
|||
Linear Mold Shrinkage | 0.000100 - 0.00400 cm/cm | 0.000100 - 0.00400 in/in | Average value: 0.00183 cm/cm Grade Count:6 |
Overview of materials for Thermoplastic Polyimide, Carbon Fiber This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyimide, Carbon Fiber". Each property range of values reported is minimum and maximum va.. |
|||
Linear Mold Shrinkage | 0.000100 - 0.00400 cm/cm | 0.000100 - 0.00400 in/in | Average value: 0.00150 cm/cm Grade Count:17 |
Overview of materials for Polyphenylene Sulfide (PPS) with Carbon Fiber + PTFE Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with Carbon Fiber + PTFE Filler". Each property range of values reported is .. |
|||
Linear Mold Shrinkage | 0.000100 - 0.00200 cm/cm | 0.000100 - 0.00200 in/in | Average value: 0.000875 cm/cm Grade Count:4 |
Overview of materials for Acrylic/Polycarbonate Alloy, Carbon Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Acrylic/Polycarbonate Alloy, Carbon Fiber Filler". Each property range of values reported is minimum and.. |
|||
Linear Mold Shrinkage | 0.000100 - 0.00600 cm/cm | 0.000100 - 0.00600 in/in | Average value: 0.00178 cm/cm Grade Count:10 |
Overview of materials for Polyetherimide (PEI), Nickel Coated Graphite Filled This property data is a summary of similar materials in the MatWeb database for the category "PEI, NCG Filled". Each property range of values reported is minimum and maximum values of appropriate Ma.. |
|||
Linear Mold Shrinkage | 0.000100 - 0.0100 cm/cm | 0.000100 - 0.0100 in/in | Average value: 0.00414 cm/cm Grade Count:227 |
Overview of materials for Polyethersulfone (PES) This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Linear Mold Shrinkage | 0.000100 - 0.0500 cm/cm | 0.000100 - 0.0500 in/in | Average value: 0.0144 cm/cm Grade Count:176 |
Overview of materials for Polypropylene, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Flame Retardant". Each property range of values reported is minimum and maximum values of.. |
|||
Linear Mold Shrinkage | 0.000100 - 0.0350 cm/cm | 0.000100 - 0.0350 in/in | Average value: 0.0127 cm/cm Grade Count:220 |
Overview of materials for Nylon 6, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Impact Grade". Each property range of values reported is minimum and maximum values of appropri.. |