| Category | Polymer , Thermoplastic , Polypropylene (PP) |
| Manufacturer | Niche Polymer |
| Trade Name | |
| Port | Shanghai port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Niche Polymer PPHM15BK Homopolymer PP.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Linear Mold Shrinkage | 0.000100 - 0.0200 cm/cm | 0.000100 - 0.0200 in/in | ASTM D955 |
| Melt Flow | 15.0 g/10 min | 15.0 g/10 min | ASTM D123 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | >= 31.0 MPa | >= 4500 psi | ASTM D638 |
| Elongation at Break | 150 % | 150 % | ASTM D638 |
| Flexural Strength | 48.3 MPa | 7000 psi | ASTM D790 |
| Flexural Modulus | >= 1.24 GPa | >= 180 ksi | ASTM D790 |
| Izod Impact, Unnotched | 0.427 J/cm @Thickness 3.17 mm |
0.800 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 1.8 MPa (264 psi) | 119 °C | 246 °F | ASTM D648 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 160 - 165 °C | 320 - 329 °F | ASTM D789 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Color | Black |