Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | -0.000500 cm/cm | -0.000500 in/in | ISO 2577 |
Menzolit Menzolit® BMC 0400 Unsaturated Polyester UP BMC 0400 is a low profile DMC/BMC for automotive applications. It fulfills the requirements of the automotive industry regarding painted body panels including reduced C-emissions. For highest surfac.. |
|||
Linear Mold Shrinkage | -0.000500 cm/cm | -0.000500 in/in | ISO 2577 |
Menzolit Menzolit® BMC 0410 Unsaturated Polyester UP BMC 0410 is a low profile BMC with zero shrinkage and low coefficient of thermal expansion. It is especially suited for precision mouldings in office and communication equipment. The combination of .. |
|||
Linear Mold Shrinkage | -0.000500 cm/cm | -0.000500 in/in | ISO 2577 |
Menzolit Menzolit® SMC 0400 Unsaturated Polyester UP SMC 0400 is a Class-A SMC for exterior body applications on cars, LCV´s and trucks. These compounds mould to parts with good up to excellent surface quality for medium bake in-line and off-line p.. |
|||
Linear Mold Shrinkage | -0.000500 cm/cm | -0.000500 in/in | ISO 2577 |
Menzolit Menzolit® SMC 0410 Unsaturated Polyester UP SMC 0410 is a Premium Class-A SMC for on-line painted exterior body applications on cars developed with CCC technology. These compounds mould to parts with excellent surface quality for on-line pain.. |
|||
Linear Mold Shrinkage | -0.000500 cm/cm | -0.000500 in/in | ISO 2577 |
Menzolit Menzolit® SMC 0430 Unsaturated Polyester UP SMC 0430 is a low emission Class-A SMC for on-line painted exterior body applications on passenger cars. These compounds mould to parts with excellent surface quality for on-line painted body panel.. |
|||
Linear Mold Shrinkage | -0.000500 cm/cm | -0.000500 in/in | ISO 2577 |
Menzolit Menzolit® SMC 0412 Unsaturated Polyester UP SMC 0412 is a premium Class-A SMC for on-line painted conductive exterior body applications on cars. These compounds mould to parts with excellent surface quality and low surface conductivity for e.. |
|||
Linear Mold Shrinkage | -0.000500 cm/cm | -0.000500 in/in | ISO 2577 |
Menzolit Menzolit® SMC 0420 Unsaturated Polyester UP SMC 0420 is a low density Premium Class-A SMC for exterior body applications on cars, LCV´s and trucks. These compounds mould to light weight parts with good up to excellent surface quality for .. |
|||
Linear Mold Shrinkage | -0.000500 cm/cm | -0.000500 in/in | ISO 2577 |
Menzolit Menzolit® SMC 0421 Unsaturated Polyester UP SMC 0421 is a low density premium Class-A SMC for on-line painted exterior body applications on cars. These compounds mould to light weight parts with excellent surface quality for on-line painted .. |
|||
Linear Mold Shrinkage | -0.000500 - 0.0130 cm/cm | -0.000500 - 0.0130 in/in | Average value: 0.00732 cm/cm Grade Count:22 |
Overview of materials for Melamine-Phenolic Copolymer This property data is a summary of similar materials in the MatWeb database for the category "Melamine-Phenolic Copolymer". Each property range of values reported is minimum and maximum values of ap.. |