Linear Mold Shrinkage 0.00100 - 0.0350 cm/cm
0.00100 - 0.0350 in/in
Average value: 0.0125 cm/cm Grade Count:219
Overview of materials for Thermoplastic Olefinic Elastomer (TPO)
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Olefinic Elastomer (TPO)". Each property range of values reported is minimum and maximum v..
Linear Mold Shrinkage 0.00400 - 0.0350 cm/cm
0.00400 - 0.0350 in/in
Average value: 0.0215 cm/cm Grade Count:15
Overview of materials for Acetal Copolymer, Silicone Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Silicone Filled". Each property range of values reported is minimum and maximum values..
Linear Mold Shrinkage 0.00100 - 0.0350 cm/cm
0.00100 - 0.0350 in/in
Average value: 0.00705 cm/cm Grade Count:50
Overview of materials for High Density Polyethylene (HDPE), Glass fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Glass fiber Filled". Each property range of values reported is minimum..
Linear Mold Shrinkage 0.0100 - 0.0350 cm/cm
0.0100 - 0.0350 in/in
Average value: 0.0255 cm/cm Grade Count:29
Overview of materials for Polyvinylidinefluoride (PVDF), Molded/Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Polyvinylidinefluoride (PVDF), Molded/Extruded". Each property range of values reported is minimum and m..
Linear Mold Shrinkage 0.00100 - 0.0350 cm/cm
0.00100 - 0.0350 in/in
Average value: 0.0300 cm/cm Grade Count:123
Overview of materials for Silicone Rubber
This property data is a summary of similar materials in the MatWeb database for the category "Silicone Rubber". Each property range of values reported is minimum and maximum values of appropriate Ma..
Linear Mold Shrinkage 0.000300 - 0.0350 cm/cm
0.000300 - 0.0350 in/in
Average value: 0.00391 cm/cm Grade Count:183
Overview of materials for Nylon 6, 40% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. E..
Linear Mold Shrinkage 0.000200 - 0.0350 cm/cm
0.000200 - 0.0350 in/in
Average value: 0.00317 cm/cm Grade Count:150
Overview of materials for Nylon 6, 50% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. E..
Linear Mold Shrinkage 0.000200 - 0.0350 cm/cm
0.000200 - 0.0350 in/in
Average value: 0.00376 cm/cm Grade Count:47
Overview of materials for Nylon 6, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of a..
Linear Mold Shrinkage 0.00150 - 0.0350 cm/cm
0.00150 - 0.0350 in/in
Average value: 0.0158 cm/cm Grade Count:263
Overview of materials for Nylon 66, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Impact Grade". Each property range of values reported is minimum and maximum values of appropr..
Linear Mold Shrinkage 0.00100 - 0.0350 cm/cm
0.00100 - 0.0350 in/in
Average value: 0.00738 cm/cm Grade Count:232
Overview of materials for Nylon 6, Heat Stabilized
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Heat Stabilized". Each property range of values reported is minimum and maximum values of appro..
Linear Mold Shrinkage 0.000300 - 0.0350 cm/cm
0.000300 - 0.0350 in/in
Average value: 0.00417 cm/cm Grade Count:497
Overview of materials for Nylon 6, 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. E..
Linear Mold Shrinkage 0.000100 - 0.0350 cm/cm
0.000100 - 0.0350 in/in
Average value: 0.0127 cm/cm Grade Count:220
Overview of materials for Nylon 6, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Impact Grade". Each property range of values reported is minimum and maximum values of appropri..
Linear Mold Shrinkage 0.00800 - 0.0350 cm/cm
0.00800 - 0.0350 in/in
Average value: 0.0193 cm/cm Grade Count:33
Overview of materials for Acetal Copolymer, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Impact Modified". Each property range of values reported is minimum and maximum values..
Linear Mold Shrinkage 0.000300 - 0.0350 cm/cm
0.000300 - 0.0350 in/in
Average value: 0.00325 cm/cm Grade Count:111
Overview of materials for Polypropylene with 40% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Glass Fiber Filler". Specific grades with glass content between 35% and 44% are i..
Linear Mold Shrinkage 0.000150 - 0.0350 cm/cm
0.000150 - 0.0350 in/in
Average value: 0.0123 cm/cm Grade Count:213