Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.0080 - 0.021 cm/cm | 0.0080 - 0.021 in/in | FRISETTA Test Method |
Nilit FRIANYL A63 CV-CM 0830 9005/Z Powder-coatable nylon 6.6 for injection molding, 8% carbon fiber reinforced, 30% ceramic filled Powder-coatable nylon 6.6 for injection moldingInformation provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Linear Mold Shrinkage | 0.014 - 0.021 cm/cm | 0.014 - 0.021 in/in | FRISETTA Test Method |
Nilit FRIANYL A63 S10 Nylon 6.6 for injection molding Nylon 6.6 for injection molding, impact modified.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Linear Mold Shrinkage | 0.014 - 0.021 cm/cm | 0.014 - 0.021 in/in | FRISETTA Test Method |
Nilit FRIANYL A63 S20 Nylon 6.6 for injection molding Nylon 6.6 for injection molding, impact modified.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Linear Mold Shrinkage | 0.018 - 0.021 cm/cm | 0.018 - 0.021 in/in | ASTM D955 |
Polymer Resources AH-GP1 Acetal Homopolymer, Low Flow, High Melt Strength, Heat Stabilized Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation. |
|||
Linear Mold Shrinkage | 0.018 - 0.021 cm/cm | 0.018 - 0.021 in/in | ASTM D955 |
Polymer Resources AH-GP2 Acetal Homopolymer, Medium Flow, Heat Stabilized Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation. |
|||
Linear Mold Shrinkage | 0.018 - 0.021 cm/cm | 0.018 - 0.021 in/in | ASTM D955 |
Polymer Resources AH-GP2-[color]-H Acetal Homopolymer, Medium Flow, General Purpose Molding, Heat Stabilized Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Linear Mold Shrinkage | 0.018 - 0.021 cm/cm | 0.018 - 0.021 in/in | ASTM D955 |
Polymer Resources AH-GP3-[color]-H Acetal Homopolymer, High Flow Resin, Heat Stabilized Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Linear Mold Shrinkage | 0.015 - 0.021 cm/cm | 0.015 - 0.021 in/in | Across Flow; ASTM D955 |
Polymer Resources NY66-GP2 General Purpose Nylon 66, Nucleated General Purpose Nylon 66, Nucleated Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry.. |
|||
Linear Mold Shrinkage | 0.018 - 0.021 cm/cm | 0.018 - 0.021 in/in | ASTM D955 |
Polymer Resources AH-GP3 Acetal Homopolymer, High Flow Resin
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Linear Mold Shrinkage | 0.015 - 0.021 cm/cm | 0.015 - 0.021 in/in | |
Lehmann & Voss LUVOCOM® 80-7580/BK Polyacetal-copolymer, with aramid reinforcement and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec.. |
|||
Linear Mold Shrinkage | 0.015 - 0.021 cm/cm | 0.015 - 0.021 in/in | |
Lehmann & Voss LUVOCOM® 80-7655/RD Polyacetal-copolymer, with aramid reinforcement and PTFE, toughness-modified, high viscosity Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec.. |
|||
Linear Mold Shrinkage | 0.018 - 0.021 cm/cm | 0.018 - 0.021 in/in | ASTM D955 |
LG Chemical LUCEL EC-605B Electrically Conductive POM, 5% Carbon Black Filled LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Linear Mold Shrinkage | 0.018 - 0.021 cm/cm | 0.018 - 0.021 in/in | ASTM D955 |
LG Chemical LUCEL N109-02 General Purpose POM, Unreinforced, Externally Lubricated, Standard Viscosity LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Linear Mold Shrinkage | 0.018 - 0.021 cm/cm | 0.018 - 0.021 in/in | ASTM D955 |
LG Chemical LUCEL N109-HR Heat Resistant POM, Unreinforced, Standard Viscosity LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Linear Mold Shrinkage | 0.018 - 0.021 cm/cm | 0.018 - 0.021 in/in | ASTM D955 |
LG Chemical LUCEL N115 POM, Unreinforced, High Viscosity LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Linear Mold Shrinkage | 0.018 - 0.021 cm/cm | 0.018 - 0.021 in/in | ASTM D955 |
LG Chemical LUCEL N115-LD Anti Mold Deposit POM, Unreinforced, Internally Lubricated, Standard Viscosity LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Linear Mold Shrinkage | 0.018 - 0.021 cm/cm | 0.018 - 0.021 in/in | ASTM D955 |
LG Chemical LUCEL N127-AS Antistatic POM, Unreinforced, High Flow LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Linear Mold Shrinkage | 0.018 - 0.021 cm/cm | 0.018 - 0.021 in/in | ASTM D955 |
LG Chemical LUCEL N127-WR Weather Resistant POM, Unreinforced, High Flow LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Linear Mold Shrinkage | 0.018 - 0.021 cm/cm | 0.018 - 0.021 in/in | ASTM D955 |
LG Chemical LUCEL N145-02 General Purpose POM, Unreinforced, Externally Lubricated, Ultra High Flow LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Linear Mold Shrinkage | 0.018 - 0.021 cm/cm | 0.018 - 0.021 in/in | ASTM D955 |
LG Chemical LUCEL N145-AS Antistatic POM, Unreinforced, Internally Lubricated, Ultra High Flow LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Linear Mold Shrinkage | 0.018 - 0.021 cm/cm | 0.018 - 0.021 in/in | ASTM D955 |
LG Chemical LUCEL WK-320 Wear Resistant POM, 20% Mineral Filled, High Modulus LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Linear Mold Shrinkage | 0.018 - 0.021 cm/cm | 0.018 - 0.021 in/in | ASTM D955 |
LG Chemical Lucet® N127 Acetal Copolymer Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Linear Mold Shrinkage | 0.012 - 0.021 cm/cm | 0.012 - 0.021 in/in | ASTM D955 |
LG Chemical Lupox® PBT-GP-1000 High Flow PBT Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Linear Mold Shrinkage | 0.017 - 0.021 cm/cm | 0.017 - 0.021 in/in | ISO 294-4 |
Wellman Wellamid® 220-N Unfilled Nylon 66, Not Lubricated, Nucleated, or Heat Stabilized Typical Applications: Automotive components, gears, switches, bearings, pulleys, fasteners, electrical coil forms, chain-saw hand guards, cable ties, furniture hardware, small appliance housings, ae.. |
|||
Linear Mold Shrinkage | 0.017 - 0.021 cm/cm | 0.017 - 0.021 in/in | ISO 294-4 |
Wellman Wellamid® 22L-N Unfilled Nylon 66, Lubricated Typical Applications: Automotive components, gears, switches, bearings, pulleys, fasteners, electrical coil forms, chain-saw hand guards, cable ties, furniture hardware, small appliance housings, ae.. |
|||
Linear Mold Shrinkage | 0.017 - 0.021 cm/cm | 0.017 - 0.021 in/in | Asahi Kasei Method |
Asahi Kasei Tenac® 7054 Homopolymer Acetal Resin High-flow grade with high crystallization rate for higher productivity.Information provided by Asahi Kasei Corporation. |