Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.0015 - 0.0035 cm/cm | 0.0015 - 0.0035 in/in | Polymerization Shrinkage |
Premix Premi-Glas® 1100-15 Fiberglass Reinforced Thermoset BMC Premi-Glas® 1100-15 is a fiberglass reinforced thermoset bulk molding compound for general purpose applications requiring thermal stability and stiffness.Key features and benefits are:Excellent sti.. |
|||
Linear Mold Shrinkage | 0.0015 - 0.0035 cm/cm | 0.0015 - 0.0035 in/in | Polymerization Shrinkage |
Premix Premi-Glas® 1100V-20 Fiberglass Reinforced Thermoset BMC Premi-Glas® 1100V-20 is a fiberglass reinforced thermoset bulk molding compound for electrical and flame retardant applications.Key features and benefits are:Non-Halogen FR technology for regulator.. |
|||
Linear Mold Shrinkage | 0.0020 - 0.0035 cm/cm | 0.0020 - 0.0035 in/in | Polymerization Shrinkage |
Premix Premi-Glas® 1200-10 Fiberglass Reinforced Thermoset SMC Premi-Glas® 1200-10 is a fiberglass reinforced thermoset sheet molding compound for general purpose applications requiring thermal stability and stiffness.Key features and benefits are:Excellent st.. |
|||
Linear Mold Shrinkage | 0.0015 - 0.0035 cm/cm | 0.0015 - 0.0035 in/in | Polymerization Shrinkage |
Premix Premi-Glas® 2103-25 CRSX Polyester BMC Premi-Glas® 2103-25 CR-SX is a 25% glass reinforced thermoset Sheet Molding Compound designed for electrical switchgear and industrial circuit breaker applications. Key features and benefits are:U.. |
|||
Linear Mold Shrinkage | 0.0015 - 0.0035 cm/cm | 0.0015 - 0.0035 in/in | Polymerization Shrinkage |
Premix Premi-Glas® 2200-15 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2200-15 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Linear Mold Shrinkage | 0.0015 - 0.0035 cm/cm | 0.0015 - 0.0035 in/in | Polymerization Shrinkage |
Premix Premi-Glas® 2200-22 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2200-22 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Linear Mold Shrinkage | 0.0015 - 0.0035 cm/cm | 0.0015 - 0.0035 in/in | Polymerization Shrinkage |
Premix Premi-Glas® 2203-22 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2203-22 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Linear Mold Shrinkage | 0.0015 - 0.0035 cm/cm | 0.0015 - 0.0035 in/in | Polymerization Shrinkage |
Premix Premi-Glas® 2203-25 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2203-25 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Linear Mold Shrinkage | 0.0015 - 0.0035 cm/cm | 0.0015 - 0.0035 in/in | Polymerization Shrinkage |
Premix Premi-Glas® 2203-30 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2203-30 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Linear Mold Shrinkage | 0.0015 - 0.0035 cm/cm | 0.0015 - 0.0035 in/in | Polymerization Shrinkage |
Premix Premi-Glas® 2205-15 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2205-15 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Linear Mold Shrinkage | 0.0015 - 0.0035 cm/cm | 0.0015 - 0.0035 in/in | Polymerization Shrinkage |
Premix Premi-Glas® 3200-22 Fiberglass Reinforced SMC Description: Premi-Glas® 3200-22 is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal and di.. |
|||
Linear Mold Shrinkage | 0.0015 - 0.0035 cm/cm | 0.0015 - 0.0035 in/in | Polymerization Shrinkage |
Premix Premi-Glas® 3200-25 Fiberglass Reinforced SMC Description: Premi-Glas® 3200-25 is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal and di.. |
|||
Linear Mold Shrinkage | 0.0025 - 0.0035 cm/cm | 0.0025 - 0.0035 in/in | With Flow; ISO 2577 |
Polykemi AB POLYfill PPH GF5030 PB Polypropylene Homopolymer, Glass Fibre-Reinforced, Chemically Coupled Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.0025 - 0.0035 cm/cm | 0.0025 - 0.0035 in/in | With Flow; ISO 2577 |
Polykemi AB POLYfill PPH GF8030 PD2 Polypropylene Homopolymer, Glass Fibre-Reinforced, Chemically Coupled Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.0015 - 0.0035 cm/cm | 0.0015 - 0.0035 in/in | ISO 2577 |
NOVA Chemicals Dylark® 378P30 Glass Reinforced Engineering Resin Features: Ultra high modulus, High heat resistance, excellent adhesion to urethaneApplications: Instrument panel substrates, Brackets, Structural components |
|||
Linear Mold Shrinkage | 0.0030 - 0.0035 cm/cm @Thickness 3.17 mm |
0.0030 - 0.0035 in/in @Thickness 0.125 in |
ASTM D955 |
PolyOne Edgetek® ES-20GF-15GM/000 Polyethersulfone - 20% Glass Fiber - 15% Milled Glass
(discontinued **) Data provided by PolyOne. |
|||
Linear Mold Shrinkage | 0.0030 - 0.0035 cm/cm | 0.0030 - 0.0035 in/in | ASTM D955 |
PolyOne Edgetek® AT-30GF/000 FDA Acetal-Copolymer, Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedFDA CapablePolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Linear Mold Shrinkage | 0.0020 - 0.0035 cm/cm | 0.0020 - 0.0035 in/in | IS 13411-1992 |
Amity Thermosets ATS 134 Phenolic Molding Inorganic, graphite Filler, Compression Molded Characteristics: Low coefficient of frictionSelf lubricating ( graphite modified )Good thermal conductivityGood glide propertiesNot suitable for electrical applicationColor- black gray Soft/medium f.. |
|||
Linear Mold Shrinkage | 0.0025 - 0.0035 cm/cm | 0.0025 - 0.0035 in/in | |
Bulk Molding Compounds BMC 620 Mineral Filled, Glass Fiber Reinforced Polyester Compound BMC 620 molding compound is a mineral filled, glass fiber-reinforced polyester compound suitable for compression, and stuffer injection molding It is characterized by good moldability high impact st.. |
|||
Linear Mold Shrinkage | 0.0015 - 0.0035 cm/cm | 0.0015 - 0.0035 in/in | |
Bulk Molding Compounds BMC 851 Corrosion Resistant, Flame Retardant Molding Compound BMC 851is a high strength, corrosion resistant and flame retardant molding compound. As with all other BMCI compounds, this Series can be supplied in logs, slugs or bulk form.Typical applications ar.. |
|||
Linear Mold Shrinkage | 0.0025 - 0.0035 cm/cm | 0.0025 - 0.0035 in/in | Across Flow; ISO 2577 |
Polykemi AB POLYfill PPH GF5035 PD2 VT Polypropylene Homopolymer, Glass Fibre-Reinforced, Chemically Coupled/Heat Resistant Information provided by Polykemi AB |