Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.00050 - 0.0015 cm/cm | 0.00050 - 0.0015 in/in | |
Lehmann & Voss LUVOCOM® 1105-8048 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at.. |
|||
Linear Mold Shrinkage | 0.00050 - 0.0015 cm/cm | 0.00050 - 0.0015 in/in | ASTM D955 |
IDI Composites 44-10 MW Thermoset Polyester, Molding Moderate strength material specifically formulated for microwave oven performance.Data provided by the manufacturer. |
|||
Linear Mold Shrinkage | 0.00010 - 0.0015 cm/cm @Thickness 4.00 mm |
0.00010 - 0.0015 in/in @Thickness 0.157 in |
|
Teijin Panlite® B-8130R Carbon Fiber Reinforced Polycarbonate Resin CF 30% reinforced grade, meeting UL 94 V-2. It has excellent strength, stiffness, heat resistance and electric conductivity. Other features are low molding shrinkage and dimensional accuracy.Applica.. |
|||
Linear Mold Shrinkage | 0.00050 - 0.0015 cm/cm @Thickness 3.20 mm |
0.00050 - 0.0015 in/in @Thickness 0.126 in |
72 hr; ISO 294 |
A. Schulman FORMION™ FI 226 40% Glass Fiber Reinforced Ionomer / Nylon Alloy DescriptionFormion® FI 226 is an injection molding grade, 40% glass fiber reinforced Ionomer / Nylon alloy, which has been formulated for high scratch resistance, heat resistance and high stiffness.. |
|||
Linear Mold Shrinkage | 0.00 - 0.0015 cm/cm | 0.00 - 0.0015 in/in | |
Bulk Molding Compounds BMC 501E Mineral Filled, Glass Reinforced Polyester BMC 501E molding compound is a mineral filled, glass-fiber-reinforced polyester compound suitable for compression and transfer molding. It is a product with good overall electrical properties, flame.. |
|||
Linear Mold Shrinkage | 0.00050 - 0.0015 cm/cm | 0.00050 - 0.0015 in/in | |
Bulk Molding Compounds BMC A20-(a) High Strength Grade Molding Compound BMC A20 is a high strength, low shrink general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC A20 is well suited for injection, transfer or compression molding o.. |
|||
Linear Mold Shrinkage | 0.0010 - 0.0015 cm/cm | 0.0010 - 0.0015 in/in | ISO 294-4 |
Premix Thermoplastics PRE-ELEC® 12-034
(discontinued **) PRE-ELEC 12-034 is a conductive thermoplastic compound based on a polyacetal copolymer with 40% carbon fiber. PRE-ELEC 12-034 exhibits excellent mechanical properties and electrical conductivity. Te.. |
|||
Linear Mold Shrinkage | 0.0010 - 0.0015 cm/cm | 0.0010 - 0.0015 in/in | ASTM D955 |
PolyOne Edgetek® AM-30CF/000 Polyphthalamide (PPA), Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |