Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.025 - 0.035 cm/cm | 0.025 - 0.035 in/in | ISO 294-4 |
Premix Thermoplastics PRE-ELEC® PE 1200 Conductive Thermoplastic Compound PRE-ELEC® PE 1200 is a conductive thermoplastic masterbatch/compound based on PE-HD. Conductivity is achieved by using special conductive carbon black. PRE-ELEC® PE 1200 has a high concentration o.. |
|||
Linear Mold Shrinkage | 0.025 - 0.035 cm/cm | 0.025 - 0.035 in/in | ISO 294-4 |
Premix Thermoplastics PRE-ELEC® PE 1296 Conductive Thermoplastic Compound PRE-ELEC® PE 1296 is a conductive thermoplastic masterbatch/compound based on PE-HD. Conductivity is achieved by using special conductive carbon black. PRE-ELEC® PE 1296 has a high concentration o.. |
|||
Linear Mold Shrinkage | 0.025 - 0.035 cm/cm | 0.025 - 0.035 in/in | ISO 294-4 |
Premix Thermoplastics PRE-ELEC® PE 1297 Conductive Thermoplastic Compound PRE-ELEC® PE 1297 is a conductive thermoplastic compound based on PE-HD. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC® PE.. |
|||
Linear Mold Shrinkage | 0.025 - 0.035 cm/cm | 0.025 - 0.035 in/in | ISO 294-4 |
Premix Thermoplastics PRE-ELEC® PE 1299 Conductive Thermoplastic Compound PRE-ELEC® PE 1299 is a conductive thermoplastic masterbatch/compound based on PE-HD. Conductivity is achieved by using special conductive carbon black. PRE-ELEC® PE 1299 has a high concentration o.. |
|||
Linear Mold Shrinkage | 0.025 - 0.030 cm/cm | 0.025 - 0.030 in/in | |
Solvay Specialty Polymers Hylar® 460 PVDF Polyvinylidene Fluoride
(discontinued **) Data provided by the manufacturer.Hylar® polymers have the characteristic stability of fluoropolymers combined with a unique polarity that influences its solubility and electrical properties. In a.. |
|||
Linear Mold Shrinkage | 0.025 - 0.030 cm/cm | 0.025 - 0.030 in/in | |
Solvay Specialty Polymers Hylar® MP10 PVDF Polyvinylidene Fluoride
(discontinued **) Data provided by the manufacturer.Hylar® polymers have the characteristic stability of fluoropolymers combined with a unique polarity that influences its solubility and electrical properties. In a.. |
|||
Linear Mold Shrinkage | 0.025 cm/cm | 0.025 in/in | ASTM D995 |
Huntsman IROGRAN® A 70 E 4675 Polyester-Based TPU-High Performance Grade Introduction: IROGRAN A 70 E 4675 is a softener free thermoplastic special-polyester-polyurethane for injection molding applications. Additional characteristics of the product are very short cycle t.. |
|||
Linear Mold Shrinkage | <= 0.025 cm/cm | <= 0.025 in/in | |
Lucite International XL Sanitary Ware Acrylic Sheet Lucite® XL continuous-cast cross-linked acrylic sheet is specially formulated for deep-draw thermoforming. It is used primarily for production of spas.Benefits: Smooth surface; Infinite colors an.. |
|||
Linear Mold Shrinkage | 0.025 cm/cm | 0.025 in/in | ASTM D955 |
Teknor Apex Monprene® MP-1531 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Linear Mold Shrinkage | 0.025 cm/cm | 0.025 in/in | |
Teknor Apex TEKBOND® 6000-35 Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Linear Mold Shrinkage | 0.025 - 0.030 cm/cm | 0.025 - 0.030 in/in | |
Solvay Specialty Polymers Hylar® MP20 PVDF Polyvinylidene Fluoride
(discontinued **) Data provided by the manufacturer.Hylar® polymers have the characteristic stability of fluoropolymers combined with a unique polarity that influences its solubility and electrical properties. In a.. |
|||
Linear Mold Shrinkage | 0.025 cm/cm | 0.025 in/in | ASTM D955 |
Lubrizol Estane® S175A Thermoplastic Polyurethane Type: Estane® S175A is a Shore 77A, polyester type thermoplastic polyurethane (TPU). FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding, Extrusion.Availability: Americas, Europe, Mid.. |
|||
Linear Mold Shrinkage | 0.025 cm/cm | 0.025 in/in | ASTM D955 |
PlastxWorld Veroplas PA2002HI Nylon 6 general purpose, unfilled, high impact modified injection molding gradeInformation provided by PlastxWorld Inc. |
|||
Linear Mold Shrinkage | 0.025 cm/cm | 0.025 in/in | ASTM D955 |
PlastxWorld Veroplas PA2002MI Nylon 6 general purpose, unfilled, medium impact modified injection molding gradeInformation provided by PlastxWorld Inc. |
|||
Linear Mold Shrinkage | 0.025 cm/cm | 0.025 in/in | ASTM D955 |
Teknor Apex Monprene® MP 1037 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |