Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.021 cm/cm | 0.021 in/in | |
Plastcom SLOVALEN PC 16 FRD 1 PP, flame retardant Packaging, transport, stockingThe product is packed in hermetically closed thick-walled 25 kg PE bags, on a 1.000 kg palette coated in a stretch foil, in big bags with a thick PE foil fixed on a 1.0.. |
|||
Linear Mold Shrinkage | 0.021 cm/cm | 0.021 in/in | |
Plastcom SLOVALEN PC 81 T 30 PP, 30% mineral filling FeaturesModified copolymer PP for injection moulding with the content of 30% microground, floated, chemically modified talc. General application - packing material, garden flower-pots, toys, furnitu.. |
|||
Linear Mold Shrinkage | 0.021 cm/cm | 0.021 in/in | |
Plastcom SLOVALEN PC 82 T 30 PP, 30% mineral filling FeaturesModified copolymer PP for injection moulding with the content of 30% micronized, floated, chemically modified talc. General application - packing material, garden flower-pots, toys, furnitur.. |
|||
Linear Mold Shrinkage | 0.021 cm/cm | 0.021 in/in | STN 64 0808 |
Plastcom SLOVALEN PH 56 FRD 1 Polypropylene Homopolymer, Halogen Flame Retardant FeaturesModified homopolymer PP for injection moulding with increased flammability resistance. Contains flame retardant on the halogen basis. Used in the electrical industry - terminals, coil form.. |
|||
Linear Mold Shrinkage | 0.021 cm/cm | 0.021 in/in | Flow; ISO 294-4 |
PolyOne Versalloy™ HC 9220-90 Thermoplastic Elastomer (TPE) Versalloy™ HC 9220-90 is a TPV alloy targeted for extrusion and injection molding healthcare applications such as medical tubing, disposable medical items and soft-touch overmolding for surgical gr.. |
|||
Linear Mold Shrinkage | 0.021 cm/cm | 0.021 in/in | ISO 294-4 |
Premix Thermoplastics PRE-ELEC® TPE 1502 Conductive Thermoplastic Compound PRE-ELEC® TPE 1502 is a conductive thermoplastic compound based on a thermoplastic elastomer (TPE). Conductivity is achieved by using a special conductive carbon black. In addition to a low electri.. |
|||
Linear Mold Shrinkage | 0.021 cm/cm | 0.021 in/in | ASTM D955 |
PolyOne Edgetek® AT-10GB/000 Black Acetal-Copolymer, Glass Bead Filled
(discontinued **) Description/Features:Glass Bead FilledInformation provided by PolyOne Corporation. |
|||
Linear Mold Shrinkage | 0.021 - 0.023 cm/cm | 0.021 - 0.023 in/in | ASTM D955 |
LNP Lubricomp® FL-4410 Polyetherimide, Silicone Lubricant Additive
(discontinued **) Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac.. |
|||
Linear Mold Shrinkage | 0.021 cm/cm | 0.021 in/in | |
Aardvark Polymers AARTEL® 820UV Acetal Copolymer Rotational Molding Resin Aartel 820UV is a natural acetal copolymer with added UV stabilizers.Aartel 820UV is a low viscosity resin with excellent flow characteristics.Aartel 820UV is available in natural white and may be p.. |
|||
Linear Mold Shrinkage | 0.021 cm/cm | 0.021 in/in | |
Shin-Etsu Silicones LIMSâ„¢ KE1950-20A/B Elastomer KE-1950-20 is a liquid injection molding silicone. It is supplied as two components which are mixed in a 1:1 ratio to ensure easy and accurate blending. It's viscosity is low enough to allow easy .. |
|||
Linear Mold Shrinkage | 0.021 cm/cm | 0.021 in/in | |
Shin-Etsu Silicones LIMSâ„¢ KE1950-70A/B Elastomer KE-1950-70 is a liquid injection molding silicone. It is supplied as two components which are mixed in a 1:1 ratio to ensure easy and accurate blending. It's viscosity is low enough to allow easy .. |
|||
Linear Mold Shrinkage | 0.021 cm/cm | 0.021 in/in | |
Shin-Etsu Silicones LIMSâ„¢ KE2001-50A/B Elastomer Information Provided by Shin-Etsu Silicones of America, Inc. |
|||
Linear Mold Shrinkage | 0.021 cm/cm | 0.021 in/in | |
Shin-Etsu Silicones LIMSâ„¢ KE2090-50AB Elastomer KE-2090-50 is a selective self-adhesive liquid injection molding silicone. It is supplied as two components which are mixed in a 1:1 ratio to ensure easy and accurate blending. Its viscosity is lo.. |
|||
Linear Mold Shrinkage | 0.021 cm/cm | 0.021 in/in | |
Polyram RamSter PF702 PBT, UV Stabilized UV stabilized, medium viscosity PBT for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Linear Mold Shrinkage | 0.021 cm/cm | 0.021 in/in | |
Polyram RamSter PF713 PBT, UV Stabilized UV stabilized, medium viscosity PBT for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Linear Mold Shrinkage | 0.021 - 0.023 cm/cm | 0.021 - 0.023 in/in | ISO 2577 |
Polyram RamSter PF810 PBT, Impact Modified Impact modified PBT for injection molding applications.Information provided by Polyram. |
|||
Linear Mold Shrinkage | 0.021 cm/cm | 0.021 in/in | |
Advanced Polymer Alloys DuraGrip™ DGR 6070 NC Thermoplastic Elastomer (TPE) DuraGrip® DGR 6070NC is designed to be a general purpose Thermoplastic Elastomer (TPE) that is easy to use in injection molding and extrusion processes. DGR 6070NC has an
excellent soft touch feel,.. |
|||
Linear Mold Shrinkage | 0.021 cm/cm @Thickness 2.00 mm |
0.021 in/in @Thickness 0.0787 in |
ISO 294-4 |
Ascend Performance Materials Vydyne® 66B Nylon 66, General Purpose, high viscosity, Conditioned Vydyne® 66B is a high-viscosity, heat-stabilized PA66 resin suitable for injection-molding and extrusion applications. It is available in natural color only. Vydyne 66B resin offers high strength, .. |
|||
Linear Mold Shrinkage | 0.021 cm/cm @Thickness 2.00 mm |
0.021 in/in @Thickness 0.0787 in |
ISO 294-4 |
Ascend Performance Materials Vydyne® 66J Nylon 66, General Purpose, high viscosity, DAM Vydyne® 66J is a high-viscosity, heat-stabilized PA66 resin suitable for injection-molding and extrusion applications. It is available in natural color only. Vydyne 66J resin offers high strength, .. |
|||
Linear Mold Shrinkage | 0.021 cm/cm @Thickness 2.00 mm |
0.021 in/in @Thickness 0.0787 in |
ISO 294-4 |
Ascend Performance Materials Vydyne® 66R Nylon 66, General Purpose, high viscosity, Conditioned Vydyne® 66R is a high-viscosity, heat-stabilized PA66 resin suitable for injection-molding and extrusion applications. It is available in natural color only. Vydyne 66R resin offers high strength, .. |
|||
Linear Mold Shrinkage | 0.021 cm/cm @Thickness 2.00 mm |
0.021 in/in @Thickness 0.0787 in |
ISO 294-4 |
Ascend Performance Materials Vydyne® 66R Nylon 66, General Purpose, high viscosity, DAM Vydyne® 66R is a high-viscosity, heat-stabilized PA66 resin suitable for injection-molding and extrusion applications. It is available in natural color only. Vydyne 66R resin offers high strength, .. |
|||
Linear Mold Shrinkage | 0.021 cm/cm | 0.021 in/in | Radial shrinkage of 10 cm o.d. sintered rod at 23°C |
Solvay Specialty Polymers Algoflon® 15GR PTFE; Graphite Filled
(discontinued **) Data provided by the manufacturer.15 wt.% Graphite. Suspension polymer powder grade recommended for compression molding. Pure PTFE possesses high inertness, excellent dielectric properties, almost n.. |
|||
Linear Mold Shrinkage | 0.021 cm/cm | 0.021 in/in | |
Plastcom SLOVALEN PC 91 T 30 PP, 30% mineral filling FeaturesModified copolymer PP for injection moulding with the content of 30% microground, floated, chemically modified talc. General application - packing material, garden flower-pots, toys, furnitu.. |
|||
Linear Mold Shrinkage | 0.021 cm/cm | 0.021 in/in | |
Polyram RamSter PF701 PBT, UV Stabilized UV stabilized high viscosity PBT for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Linear Mold Shrinkage | 0.021 cm/cm | 0.021 in/in | MPC method, MD |
Mitsui TPX® RT18 Methylpentene Copolymer, Transparent Grade TPX® is a 4-methylpentene-1 based polyolefin with a unique combination of transparency, heat and chemical resistant qualities. TPX is used in a wide variety of applications, including: medical equi.. |
|||
Linear Mold Shrinkage | 0.021 cm/cm | 0.021 in/in | MPC method, MD |
Mitsui TPX® RT18 XB Methylpentene Copolymer TPX® is a 4-methylpentene-1 based polyolefin with a unique combination of transparency, heat and chemical resistant qualities. TPX is used in a wide variety of applications, including: medical equi.. |
|||
Linear Mold Shrinkage | 0.021 cm/cm | 0.021 in/in | ASTM D955 |
PolyOne Edgetek® AT-10GB/000 Acetal-Copolymer, Glass Bead Filled
(discontinued **) Description/Features:Glass Bead FilledPolyOne First ChoiceInformation provided by PolyOne Corporation. |