Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.0125 cm/cm | 0.0125 in/in | |
Plastcom SLOVALEN PC 12 T 30 TS PP reinforced with 30% mineral filler Features: Modified copolymer PP for injection moulding or extrusion parts with the content of 30 % mineral filler. Increased rigidity, strength and impact strenght.Delivered in natural mode and in t.. |
|||
Linear Mold Shrinkage | 0.0125 cm/cm | 0.0125 in/in | |
Plastcom SLOVALEN PC 13 T 30 PP, 30% mineral filling FeaturesModified copolymer PP for injection moulding or extrusion parts with the content of 30 % mineral filler. Increased rigidity, strength and impact strenght.Delivered in natural mode and in the.. |
|||
Linear Mold Shrinkage | 0.0125 cm/cm | 0.0125 in/in | ASTM D955 |
RheTech Products FT1055-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black Applications: Bumper coversInterior trimSplash shieldsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Linear Mold Shrinkage | 0.0125 cm/cm | 0.0125 in/in | ASTM D955 |
RheTech Products FT1055-50 Thermoplastic Polyolefin, UV Stabilized, Black Applications: Bumper coversInterior trimSplash shieldsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Linear Mold Shrinkage | 0.0125 cm/cm | 0.0125 in/in | ASTM D955 |
RheTech Products FT1055-624 Thermoplastic Polyolefin, Non-UV Stabilized, General Purpose Light Grey Applications: Bumper coversInterior trimSplash shieldsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Linear Mold Shrinkage | 0.0125 cm/cm | 0.0125 in/in | ASTM D955 |
RheTech Products FT1055-685UV Thermoplastic Polyolefin, UV Stabilized, Graphite Applications: Bumper coversInterior trimSplash shieldsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Linear Mold Shrinkage | 0.0125 cm/cm | 0.0125 in/in | ASTM D955 |
RheTech Products FT2500-01A Thermoplastic Polyolefin, Non-UV Stabilized, Black Applications: Air DamsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Linear Mold Shrinkage | 0.0125 cm/cm | 0.0125 in/in | ASTM D955 |
RheTech Products HP531-680UV 22% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, Medium Scratch Resistant, BJAA Light Parchment Applications: I/P componentsInterior trimA/B/C/ PillarsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Linear Mold Shrinkage | 0.0125 cm/cm | 0.0125 in/in | ASTM D955 |
RheTech Products RCC220-01 20% Calcium Carbonate Reinforced Polypropylene Copolymer, Black, Recycled Content Applications: I/P hush panelsSplash shieldsUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Linear Mold Shrinkage | 0.0125 cm/cm | 0.0125 in/in | |
Plastcom SLOVALEN PH 59 T 40 LW 031 PP, 40% mineral filling, laser label FeaturesModified homopolymer PP for injection moulding with the content of 40% microground, floated, chemically modified talc.Contains modificator for laser labeling of finisched parts. /LASER NdIAG.. |
|||
Linear Mold Shrinkage | 0.0125 cm/cm | 0.0125 in/in | ASTM D955 |
RheTech Products HP531-678UV 22% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, Medium Scratch Resistant, IT3A Medium Light Stone Applications: I/P componentsInterior trimA/B/C/ PillarsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Linear Mold Shrinkage | 0.0125 cm/cm | 0.0125 in/in | ASTM D955 |
RheTech Products HP531-679UV 22% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, Medium Scratch Resistant, 2B5A Black Ink Applications: I/P componentsInterior trimA/B/C/ PillarsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Linear Mold Shrinkage | 0.0125 - 0.0155 cm/cm | 0.0125 - 0.0155 in/in | ASTM D955 |
Metabolix Mirel™ F1005 Injection Molding Grade PHA Bioplastic Mirel F1005 is FDA cleared for use in non-alcoholic food contact applications, from frozen food storage and microwave reheating to boiling water up to 212°F. FDA clearance includes products such.. |
|||
Linear Mold Shrinkage | 0.0125 - 0.0155 cm/cm | 0.0125 - 0.0155 in/in | ASTM D955 |
Metabolix Mirel™ F1006 Injection Molding Grade PHA Bioplastic Mirel F1006 is FDA cleared for use in non-alcoholic food contact applications, from frozen food storage and microwave reheating to boiling water up to 212°F. FDA clearance includes products such.. |
|||
Linear Mold Shrinkage | 0.0125 - 0.0155 cm/cm | 0.0125 - 0.0155 in/in | ASTM D955 |
Metabolix Mirelâ„¢ P1003 Injection Molding Grade PHA Bioplastic Mirelâ„¢ P1003 is a general purpose injection molding material with high modulus.Mirel is suitable for a wide range of injection molded food service and packaging applications including caps and .. |
|||
Linear Mold Shrinkage | 0.0125 - 0.0155 cm/cm | 0.0125 - 0.0155 in/in | ASTM D955 |
Metabolix Mirelâ„¢ P1004 Injection Molding Grade PHA Bioplastic Mirel P1004 is a general purpose injection molding grade with high toughness.About Mirel BioplasticsMirel is a family of bioplastic materials that have physical properties comparable to petroleum-ba.. |
|||
Linear Mold Shrinkage | 0.0125 cm/cm | 0.0125 in/in | ASTM D955 |
Tipco Tipcolene® FPT 30 PPC - 30% Talc Reinforced Polypropylene Copolymer Compound 30% Talc Reinforced PP CopolymerApplications: General PurposeProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India. |
|||
Linear Mold Shrinkage | 0.0125 cm/cm | 0.0125 in/in | ASTM D955 |
Tipco Tipcolene® FX 4000 - UL94-V0 Flame Retardant Polypropylene Copolymer, High Impact Strength V-0 Flame Retardant PP Copolymer with High Impact StrengthApplications: Battery HousingsProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India. |
|||
Linear Mold Shrinkage | 0.0125 cm/cm | 0.0125 in/in | ASTM D955 |
Tipco Tipcolene® NPI 200 IN - 25% Talc/Mineral Reinforced Polypropylene Copolymer with Very High Flow, Stiffness & Impact Strength 20% Mineral Reinforced, Very High Stiffness & Very High Impact PP CopolymerApplications: Automotive DashboardsProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries .. |
|||
Linear Mold Shrinkage | 0.0125 cm/cm | 0.0125 in/in | |
Cytec EN-12 (Conap) Casting, Potting, and Molding Compound High Technology Potting, Casting and Molding CompoundsTwo-component, polybutadiene-based liquid urethane casting and potting systems. When reacted these high technology systems produce tough, stable.. |
|||
Linear Mold Shrinkage | 0.0125 cm/cm | 0.0125 in/in | Bayer Test |
Covestro Bayflex® MP-5000 Polyurethane Elastomeric RIM, MDI-based 2-Component Liquid System 0.118 in. thickness. RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and of.. |
|||
Linear Mold Shrinkage | 0.0125 cm/cm | 0.0125 in/in | ASTM D955 |
Adell AI-10 Nylon 66, Impact Modified Data provided by Adell Plastics, Inc. |
|||
Linear Mold Shrinkage | 0.0125 cm/cm | 0.0125 in/in | ASTM D955 |
Adell BI-10 Nylon 6, Impact Modified Data provided by Adell Plastics, Inc. |
|||
Linear Mold Shrinkage | 0.0125 cm/cm | 0.0125 in/in | ASTM D955 |
Adell BI-30 Nylon 6, Impact Modified Data provided by Adell Plastics, Inc. |
|||
Linear Mold Shrinkage | 0.0125 cm/cm | 0.0125 in/in | ASTM D955 |
Adell BS-10 Nylon 6, General Purpose Data provided by Adell Plastics, Inc. |
|||
Linear Mold Shrinkage | 0.0125 cm/cm | 0.0125 in/in | ASTM D955 |
Adell BS-30 Nylon 6, General Purpose Data provided by Adell Plastics, Inc. |
|||
Linear Mold Shrinkage | 0.0125 cm/cm | 0.0125 in/in | ASTM D955 |
Ashley Polymers Ashlene® 538 Nylon 66 A general purpose high viscosity extrusion grade Nylon 66.Data provided by the manufacturer |
|||
Linear Mold Shrinkage | 0.0125 cm/cm | 0.0125 in/in | ASTM D955 |
PolyOne Synprene® RT-3860MS Thermoplastic Elastomer - SBC
(discontinued **) Description/Features:High Performance Thermoplastic ElastomerUV StabilizedTranslucentApplications:Multi-PurposeMarket:Consumer GoodsProcessing Method:Injection MoldingPolyOne First ChoiceInformation.. |
|||
Linear Mold Shrinkage | 0.0125 cm/cm | 0.0125 in/in | ASTM D955 |
PolyOne Synprene® IT 37-031 Thermoplastic Elastomer - SBC
(discontinued **) Description/Features:Specialty Thermoplastic ElastomerMarket:IndustrialConsumer GoodsProcessing Method:Injection MoldingPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Linear Mold Shrinkage | 0.0125 cm/cm | 0.0125 in/in | ASTM D955 |
Adell AI-30 Nylon 66, Impact Modified Data provided by Adell Plastics, Inc. |