Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.0025 - 0.0045 cm/cm | 0.0025 - 0.0045 in/in | Injection and Compression; ISO 2577 |
Raschig Group 2568 AMC Glass fiber-reinforced polyester molding compound. Very good mechanical strength, very good electrical properties and dimensional stability, heat resistant up to 500°C for short time - usable for s.. |
|||
Linear Mold Shrinkage | 0.0025 - 0.0040 cm/cm | 0.0025 - 0.0040 in/in | ASTM D955 |
PolyOne Stat-Tech™ PS-NX 102902 CM Black Polybutylene Terephthalate (PBT)
(discontinued **) Preliminary Data SheetPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Linear Mold Shrinkage | 0.0025 cm/cm | 0.0025 in/in | ASTM D955 |
RheTech Products G20P252-01 20% Glass Fiber Reinforced Polypropylene Copolymer, Black Applications: Interior trimArm rest insertConsolesDome light housingInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Linear Mold Shrinkage | 0.0025 - 0.0035 cm/cm | 0.0025 - 0.0035 in/in | With Flow; ISO 2577 |
Polykemi AB POLYfill PPH GF3030 PD2 PP, Glass Fiber-Reinforced, Chemically Coupled Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.0025 - 0.0035 cm/cm | 0.0025 - 0.0035 in/in | With Flow; ISO 2577 |
Polykemi AB POLYfill PPH GF4030 PD2 Polypropylene Homopolymer, Glass Fibre-Reinforced, Chemically Coupled Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.0025 - 0.0035 cm/cm | 0.0025 - 0.0035 in/in | With Flow; ISO 2577 |
Polykemi AB POLYfill PPH GF8030 PD1 VT2 PP, Glass Fiber-Reinforced, Chemically Coupled Heat Stabilized Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.0025 - 0.0040 cm/cm | 0.0025 - 0.0040 in/in | ASTM D955 |
PolyOne Edgetek® ATH-20CF/000 Acetal-Homopolymer, Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedElectrically ConductivePolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Linear Mold Shrinkage | 0.0025 cm/cm | 0.0025 in/in | |
Cookson Group Plaskon® ULS-12 Epoxy Encapsulant
(discontinued **) Test specimens were transfer molded and post cured 4 hours at 175°C.A state-of-the-art, ultra low stress epoxy encapsulant designed for packaging large, stress-sensitive DIPs, PLCCs and QFPs. It i.. |
|||
Linear Mold Shrinkage | 0.0025 cm/cm | 0.0025 in/in | |
Haysite 20000 Polyester BMC, 15% Glass Reinforced The 20000 series bulk molding compound is an electrical grade that can be compression, transfer, or injection molded. Offering good arc/track properties and mechanical strength, this grade is also r.. |
|||
Linear Mold Shrinkage | 0.0025 cm/cm | 0.0025 in/in | ASTM D955 |
SK Chemicals SKYTHANE® T865A Polyester Based, Low Hardness Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Linear Mold Shrinkage | 0.0025 cm/cm | 0.0025 in/in | |
Styron Pulse® 759 ABS + Polycarbonate, 15% Glass Reinforced PULSE® 759 Engineering resin is a 15% glass reinforced resin designed to provide excellent processability, high heat resistance, and practical toughness. PULSE 759 Engineering resin has been used.. |
|||
Linear Mold Shrinkage | 0.0025 cm/cm | 0.0025 in/in | ASTM D6289 |
Sumitomo Bakelite Durez® 32245 Phenolic, Compression Grade Durez 32245 Black Phenolic is a two-stage glass fiber and mineral filled special purpose molding compound. It is especially designed for applications requiring high strength and dimensional stabilit.. |
|||
Linear Mold Shrinkage | 0.0025 cm/cm | 0.0025 in/in | ISO 2577 |
Polyram RamSter PF300G9 PBT, 45% Glass Fiber 45% Glass fiber reinforced PBT for injection molding applications.Information provided by Polyram. |
|||
Linear Mold Shrinkage | 0.0025 cm/cm | 0.0025 in/in | ASTM D955 |
Adell AR-18 Nylon 66, 40% Glass Reinforced Data provided by Adell Plastics, Inc. |
|||
Linear Mold Shrinkage | 0.0025 cm/cm | 0.0025 in/in | ASTM D955 |
Adell AR-38 Nylon 66, 40% Glass Reinforced Data provided by Adell Plastics, Inc. |
|||
Linear Mold Shrinkage | 0.0025 cm/cm | 0.0025 in/in | ASTM D955 |
Ashley Polymers Ashlene® 528L-30LG Nylon 66, 30% Long Glass Fiber Reinforced Long glass fiber reinforced Nylon 66 designed for parts requiring excellent thermal and dimensional stability and higher strength than available with conventional glass reinforced resins.Data provid.. |
|||
Linear Mold Shrinkage | 0.0025 - 0.00345 cm/cm | 0.0025 - 0.00345 in/in | |
Bulk Molding Compounds BMC 620X Mineral Filled, Glass Fiber Reinforced Polyester Compound BMC 620X molding compound is a mineral filled, glass fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is a high impact material produced in ex.. |
|||
Linear Mold Shrinkage | 0.0025 - 0.0040 cm/cm | 0.0025 - 0.0040 in/in | |
Bulk Molding Compounds BMC 6241 Glass Fiber Reinforced Compound BMC 6241 is a glass fiber-reinforced material formulated specifically for molding of industrial lighting reflectors where adequate strength is required along with a high reflectivity. It is availabl.. |
|||
Linear Mold Shrinkage | 0.0025 cm/cm | 0.0025 in/in | |
BCC Products BC 8160 Urethane Casting BC8160 is a low viscosity two-component urethane casting compound that is specifically formulated for its flexural and impact strength. It is recommended for use for the production casting of highly.. |
|||
Linear Mold Shrinkage | 0.0025 - 0.0040 cm/cm | 0.0025 - 0.0040 in/in | |
Bulk Molding Compounds BMC 2274 Mineral Filled, Glass Reinforced Polyester BMC 2274 molding compound is a mineral filled, glass-fiber-reinforced polyester compound suitable for compression transfer and stuffer injection molding. It is a general-purpose material with medium.. |
|||
Linear Mold Shrinkage | 0.0025 - 0.0045 cm/cm | 0.0025 - 0.0045 in/in | |
Bulk Molding Compounds BMC 610 Mineral Filled, Glass Reinforced Polyester Compound BMC 610 molding compound is a mineral filled, glass fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is set a part form other medium impact el.. |
|||
Linear Mold Shrinkage | 0.0025 - 0.0035 cm/cm | 0.0025 - 0.0035 in/in | |
Bulk Molding Compounds BMC 620 Mineral Filled, Glass Fiber Reinforced Polyester Compound BMC 620 molding compound is a mineral filled, glass fiber-reinforced polyester compound suitable for compression, and stuffer injection molding It is characterized by good moldability high impact st.. |
|||
Linear Mold Shrinkage | 0.0025 cm/cm | 0.0025 in/in | |
E-Polymers SEPAZ® LA40 PA66 LFT Resin Long Fiber Thermoplastics: SEPAZ LFT products, injection moldable long fiber-reinforced thermoplastics (LFT), are made using a unique pultrusion that thoroughly wets out the glass fibers and deliver.. |
|||
Linear Mold Shrinkage | 0.0025 cm/cm | 0.0025 in/in | LATI |
LATI LASULF G/30 30% Glass Reinforced Polysulfone (PSU)
(Unverified Data**) Description: Lasulf products are composed of polysulfone (PSU). They feature good thermal and mechanical properties such as excellent toughness, even at low temperatures, excellent dimensional stabi.. |
|||
Linear Mold Shrinkage | 0.0025 cm/cm | 0.0025 in/in | LATI |
LATI LARIL 13 G/30 30% Glass Fiber Reinforced Polyphenylene Oxide (PPOm)
(Unverified Data**) Description: Laril thermoplastics are polyphenylene oxide (PPOm) products. They exhibit excellent toughness, even at low temperatures, good thermal resistance and dimensional stability are the most .. |
|||
Linear Mold Shrinkage | 0.0025 cm/cm | 0.0025 in/in | ASTM D955 |
Sumitomo Bakelite North America FM 4005 Fiberglass Reinforced Phenolic Novolac FM 4005 is a fiberglass reinforced phenolic novolac molding compound, with excellent dimensional stability and good strength at elevated temperatures. This material is compliant with the specificat.. |