Linear Mold Shrinkage 0.0012 cm/cm
0.0012 in/in
ASTM D955
RheTech Products FRG130-01 30% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Flame Retardant, Black
Applications: Electrical component housingsSunroof componentsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products.
Linear Mold Shrinkage 0.0012 cm/cm
0.0012 in/in
ASTM D955
RheTech Products GC43P250-00 43% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Natural
Applications: Consumer goodsFunctional supportsHead lamp bracketsInjection molding conditions reported in table.Information provided by RheTech Products.
Linear Mold Shrinkage 0.0012 cm/cm
0.0012 in/in
ASTM D955
RheTech Products GC43P250-777 43% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Ivory
Applications: BracketsStructural supportsDurable GoodsInjection molding conditions reported in table.Information provided by RheTech Products.
Linear Mold Shrinkage 0.0012 cm/cm
0.0012 in/in
ATM D955
Plenco 50030 PET, Pellet, Injection Molded, White  (discontinued **)
PLENCO 50030 is an engineering grade glass reinforced polyethylene terephthalate resin designed for good physical strength. It is UL listed and available in white, natural, and black.Information sup..
Linear Mold Shrinkage 0.0012 cm/cm
0.0012 in/in
ATM D955
Plenco 50240 PET, Pellet, Injection Molded, Natural Color  (discontinued **)
PLENCO 50240 is an engineering grade glass reinforced UL flame rated polyethylene terephthalate resin designed for excellent dimensional stability. It is UL listed and available in natural and black..
Linear Mold Shrinkage 0.0012 cm/cm
0.0012 in/in
ATM D955
Plenco 51045 PET, Pellet, Injection Molded, Black  (discontinued **)
PLENCO 51045 is an engineering grade glass reinforced polyethylene terephthalate resin designed for higher physical strength. It is It is UL listed and available in black only.Information supplied b..
Linear Mold Shrinkage 0.0012 cm/cm
0.0012 in/in
ATM D955
Plenco 51240 PET, Pellet, Injection Molded, Black  (discontinued **)
PLENCO 51240 is an engineering grade glass reinforced flame retarded recycled polyethylene terephthalate resin designed for excellent dimensional stability. It is UL listed.Information supplied by P..
Linear Mold Shrinkage 0.0012 cm/cm
0.0012 in/in
Haysite 270FRII Polyester BMC, Glass Reinforced
Haysite Grade 270FRII is a second generation glass reinforced thermoset polyester bulk molding compound. This material can be compression, transfer, or injection molded. Qualified under MIL-M-14, Ty..
Linear Mold Shrinkage 0.0012 cm/cm
0.0012 in/in
ISO 2577
Menzolit Menzolit® BMC 2900 Unsaturated Polyester UP
BMC 2900 is a specially designed BMC to meet the EC Safety Signs Directive (92/58/EEC) on the provision and use of safety signs at work. In areas where it is not possible to include the use of illu..
Linear Mold Shrinkage 0.0012 cm/cm
0.0012 in/in
ISO 2577
Polyram Polytron P40B07 Polypropylene, 40% Long Glass Fiber, UV Stabilized
A chemically coupled 40% long glass fiber reinforced black polypropylene, heat stabilized, UV stabilized for injection molding applications.Information provided by Polyram.
Linear Mold Shrinkage 0.0012 cm/cm
0.0012 in/in
Polyram Polytron P40B11 Homopolymer Polypropylene, Chemically Coupled 40% LGF
A chemically coupled 40% LGF reinforced black PP, heat stabilized for injection molding applications.Information provided by Polyram Ram On Ind.
Linear Mold Shrinkage 0.0012 cm/cm
0.0012 in/in
Polyram Polytron P40N01 Homopolymer Polypropylene, Chemically Coupled 40% Long Glass Fiber
A CHEMICALLY COUPLED 40% LONG GLASS FIBER REINFORCED NATURAL POLYPROPYLENE HEAT STABILIZED FOR INJECTION MOLDING APPLICATION.Information provided by Polyram Ram On Ind.
Linear Mold Shrinkage 0.0012 cm/cm
0.0012 in/in
Polyram Polytron P40B01 Homopolymer Polypropylene, Chemically Coupled 40% LGF
A chemically coupled 40% LGF reinforced black PP, heat stabilized for high temperature applications such as under the hood automotive parts.Information provided by Polyram Ram On Ind.
Linear Mold Shrinkage 0.0012 cm/cm
0.0012 in/in
ISO 2577
Polyram Polytron P40N11 Polypropylene, 40% Long Glass Fibers
A chemically coupled 40% long glass fiber reinforced natural polypropylene, heat stabilized, for injection molding applications.Information provided by Polyram.
Linear Mold Shrinkage 0.0012 cm/cm
0.0012 in/in
Cold Part VS Cold Tool; ASTM D955
Applied Composites 8022 Polyester SMC
Industry Application: ConstructionProduct Application: Water TreatmentDistinct Features: Ideal for Buried Applications, Construction, High Corrosion Resistance in Waste Water Treatment, Dimensional ..
Linear Mold Shrinkage 0.0012 cm/cm
0.0012 in/in
ASTM D2566-69
BCC Products BC 7062H Epoxy Casting
BC 7062 are aluminum filled, low viscosity epoxy mass casting resins. These room temperature cure systems allow the user choice thicknesses of 1/8 inch to a maximum of 6 inches without foaming or yi..
Linear Mold Shrinkage 0.0012 cm/cm
0.0012 in/in
ATM D955
Plenco 51015 PET, Pellet, Injection Molded, Natural Color  (discontinued **)
PLENCO 51015 is an engineering grade glass reinforced recycled polyethylene terephthalate resin designed for increased flexibility and good physical strength. It is UL listed.Information supplied by..
Linear Mold Shrinkage 0.0012 cm/cm
0.0012 in/in
E-Polymers SEPAZ® C130HS 30% Glass Fiber Reinforced High Temperature Stabilized LCP Resin
Liquid Crystal Polymer Resin: SEPAZ LCP resin has a unique structure and performance unthought of in a traditional plastics. Beside SEPAZ LCP takes the excels in all-around performance and molding ..
Linear Mold Shrinkage 0.0012 cm/cm
0.0012 in/in
ASTM D955
RheTech Products GC43P250-01 43% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Black
Applications: Consumer goodsFunctional supportsHead lamp bracketsDurable GoodsInjection molding conditions reported in table.Information provided by RheTech Products.
Copyright © lookpolymers.com All Rights Reserved