Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.00030 cm/cm | 0.00030 in/in | Polymerization Shrinkage |
Premix Premi-Glas® 3404 33% Glass Reinforced SMC Description: Premi-Glas® 3404 is a glass reinforced thermoset sheet molding compound designed for mass transit and high strength flame retardant applications where low smoke and flame are required... |
|||
Linear Mold Shrinkage | 0.00030 cm/cm | 0.00030 in/in | Polymerization Shrinkage |
Premix Premi-Glas® 8101 Glass Reinforced Polyester BMC Description: Premi-Glas® 8101 is a glass reinforced thermoset polyester Bulk Molding Compound designed for injection molding of automotive forward lighting reflectors. Key features and benefits: Ex.. |
|||
Linear Mold Shrinkage | 0.00030 cm/cm | 0.00030 in/in | ISO 2577 |
Menzolit Menzolit® BMC 1100 Unsaturated Polyester UP BMC 1100 is a special BMC for high strength application. The glass content is set to a level that provides sufficient mouldability with high strength and stiffness properties. The selection of the r.. |
|||
Linear Mold Shrinkage | 0.00030 cm/cm | 0.00030 in/in | ISO 2577 |
Menzolit Menzolit® BMC 1500 Unsaturated Polyester UP BMC 1500 is a special BMC for the use at elevated temperature. The glass content is set to a level that combines good flowability with good strength and stiffness properties. Even without a specific.. |
|||
Linear Mold Shrinkage | 0.00030 cm/cm | 0.00030 in/in | ISO 2577 |
Menzolit Menzolit® SMC 0520 Unsaturated Polyester UP SMC 0520 is a special SMC with significantly reduced density. The glass level has been selected to combine good moulding with sufficient strength and stiffness properties. Even without a specific fi.. |
|||
Linear Mold Shrinkage | 0.00030 cm/cm | 0.00030 in/in | ISO 2577 |
Menzolit Menzolit® SMC 1400 Unsaturated Polyester UP SMC 1400 is a special SMC being used in the environment of a combustion engine. The glass level has been selected to combine good mouldability with good stiffness and strength properties. The produc.. |
|||
Linear Mold Shrinkage | 0.00030 cm/cm | 0.00030 in/in | ISO 2577 |
Menzolit Menzolit® BMC 1400 Unsaturated Polyester UP BMC 1400 is a special BMC for the use on an engine. The glass content is set to a level that combines good mouldability with good strength and stiffness properties. The product has been developped f.. |
|||
Linear Mold Shrinkage | 0.00030 cm/cm | 0.00030 in/in | ASTM D955 |
A. Schulman COMTUF® 5011 10% Glass Fiber Reinforced Polycarbonate Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.00030 cm/cm @Thickness 1.59 mm |
0.00030 in/in @Thickness 0.0625 in |
ASTM D955 |
Plastics Group Polifil® GFRMPPCC-40 40% Glass Reinforced Polypropylene, High Impact Polifil® GFRMPPCC series compounds are high impact polypropylenes reinforced with chemically coupled glass fibers. This combination provides higher impact strength while retaining high stiffness.Ap.. |
|||
Linear Mold Shrinkage | 0.00030 cm/cm | 0.00030 in/in | ASTM D955 |
A. Schulman COMTUF® 5011 10% Glass Fiber Reinforced Polycarbonate Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.00030 cm/cm | 0.00030 in/in | ASTM D955 |
A. Schulman COMTUF® 5011 10% Glass Fiber Reinforced Polycarbonate Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.00030 cm/cm | 0.00030 in/in | ASTM D955 |
A. Schulman COMTUF® 5011 10% Glass Fiber Reinforced Polycarbonate Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.00030 cm/cm | 0.00030 in/in | ASTM D955 |
A. Schulman COMTUF® 5011 10% Glass Fiber Reinforced Polycarbonate Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.00030 cm/cm | 0.00030 in/in | ASTM D955 |
A. Schulman COMTUF® 5011 10% Glass Fiber Reinforced Polycarbonate Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.00030 cm/cm | 0.00030 in/in | Cured |
Atom Adhesives AA-DUCT 902 Epoxy Adhesive and Coating AA-DUCT 902 is an epoxy adhesive and coating formulation based on pure silver. This versatile silver formulation offers the maximum continuity of conductivity with an electrical resistivity value of.. |
|||
Linear Mold Shrinkage | 0.00030 cm/cm | 0.00030 in/in | ASTM D2566 |
BCC Products BC 8782 Urethane Casting BC 8782 produces a high impact rigid 82 Shore D material that is commonly used to make clear or tinted castings of all kinds. When used at room temperature castings 1/8" thick or larger can be readi.. |
|||
Linear Mold Shrinkage | 0.00030 cm/cm | 0.00030 in/in | |
Polyram Polytron P50B01 Homopolymer Polypropylene, Chemically Coupled 50% LGF A chemically coupled 50% LGF reinforced black PP, heat stabilized for high temperature applications such as under the hood automotive parts.Information provided by Polyram Ram On Ind. |
|||
Linear Mold Shrinkage | 0.00030 - 0.0010 cm/cm | 0.00030 - 0.0010 in/in | |
Bulk Molding Compounds BMC T70 Automotive Grade Molding compound BMC T70 is a low profile automotive grade molding compound specifically formulated for the vacuum metallization process. These compounds have excellent physical properties as well as superior adhes.. |