Polymer Property : Linear Mold Shrinkage = 0.00020 cm/cm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage 0.00020 - 0.0020 cm/cm

@Thickness 4.00 mm
0.00020 - 0.0020 in/in

@Thickness 0.157 in
Teijin Panlite® BS-8120R Friction and Abrasion Resistant, Carbon Fiber Reinforced Polycarbonate Resin
CF 20% reinforced grade, meeting UL 94 V-2. it is compounded with fluorine powder to improve friction and abrasion resistance and also exhibits a mold release property, maintaining excellent charact..
Linear Mold Shrinkage <= 0.00020 cm/cm
<= 0.00020 in/in
Typical, molds cut to zero
Azdel SuperLite® SL550600-100 PP Resin Matrix / 55% Glass Fiber (1 mm Molded Thickness)
AZDEL SuperLite® SL550600-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic..
Linear Mold Shrinkage <= 0.00020 cm/cm
<= 0.00020 in/in
Typical, molds cut to zero
Azdel SuperLite® SL550600-100 PP Resin Matrix / 55% Glass Fiber (3.5 mm Molded Thickness)
AZDEL SuperLite® SL550600-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic..
Linear Mold Shrinkage <= 0.00020 cm/cm
<= 0.00020 in/in
Typical, molds cut to zero
Azdel SuperLite® SL550700-100 PP Resin Matrix / 55% Glass Fiber (1 mm Molded Thickness)
AZDEL SuperLite® SL550700-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic..
Linear Mold Shrinkage <= 0.00020 cm/cm
<= 0.00020 in/in
Typical, molds cut to zero
Azdel SuperLite® SL550800-100 PP Resin Matrix / 55% Glass Fiber (2.5 mm Molded Thickness)
AZDEL SuperLite® SL550800-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic..
Linear Mold Shrinkage <= 0.00020 cm/cm
<= 0.00020 in/in
Typical, molds cut to zero
Azdel SuperLite® SL550900-100 PP Resin Matrix / 55% Glass Fiber (2 mm Molded Thickness)
AZDEL SuperLite® SL550900-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic..
Linear Mold Shrinkage <= 0.00020 cm/cm
<= 0.00020 in/in
Typical, molds cut to zero
Azdel SuperLite® SL550900-100 PP Resin Matrix / 55% Glass Fiber (2.5 mm Molded Thickness)
AZDEL SuperLite® SL550900-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic..
Linear Mold Shrinkage <= 0.00020 cm/cm
<= 0.00020 in/in
Typical, molds cut to zero
Azdel SuperLite® SL550900-100 PP Resin Matrix / 55% Glass Fiber (3 mm Molded Thickness)
AZDEL SuperLite® SL550900-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic..
Linear Mold Shrinkage <= 0.00020 cm/cm
<= 0.00020 in/in
Typical, molds cut to zero
Azdel SuperLite® SL550900-100 PP Resin Matrix / 55% Glass Fiber (3.5 mm Molded Thickness)
AZDEL SuperLite® SL550900-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic..
Linear Mold Shrinkage <= 0.00020 cm/cm
<= 0.00020 in/in
Typical, molds cut to zero
Azdel SuperLite® SL551000-100 PP Resin Matrix / 55% Glass Fiber (2 mm Molded Thickness)
AZDEL SuperLite® SL551000-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic..
Linear Mold Shrinkage <= 0.00020 cm/cm
<= 0.00020 in/in
Typical, molds cut to zero
Azdel SuperLite® SL551400-100 PP Resin Matrix / 55% Glass Fiber (5 mm Molded Thickness)
AZDEL SuperLite® SL551400-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic..
Linear Mold Shrinkage <= 0.00020 cm/cm
<= 0.00020 in/in
Typical, molds cut to zero
Azdel SuperLite® SL551600-100 PP Resin Matrix / 55% Glass Fiber (7 mm Molded Thickness)
AZDEL SuperLite® SL551600-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic..
Linear Mold Shrinkage <= 0.00020 cm/cm
<= 0.00020 in/in
Typical, molds cut to zero
Azdel SuperLite® SL551800-100 PP Resin Matrix / 55% Glass Fiber (4 mm Molded Thickness)
AZDEL SuperLite® SL551800-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic..
Linear Mold Shrinkage <= 0.00020 cm/cm
<= 0.00020 in/in
Typical, molds cut to zero
Azdel SuperLite® SL551800-100 PP Resin Matrix / 55% Glass Fiber (8 mm Molded Thickness)
AZDEL SuperLite® SL551800-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic..
Linear Mold Shrinkage 0.00020 cm/cm
0.00020 in/in
ASTM D2566-69
BCC Products SLO-KAST BC 8009 Urethane Casting
Slo-Kast is a low viscosity, medium setting, easy to use casting material. This polyurethane system features extremely low shrinkage when properly cured. Unlike Kwik-Kast, BC 8009 offers the user lo..
Linear Mold Shrinkage <= 0.00020 cm/cm
<= 0.00020 in/in
Typical, molds cut to zero
Azdel SuperLite® SL551000-100 PP Resin Matrix / 55% Glass Fiber (4 mm Molded Thickness)
AZDEL SuperLite® SL551000-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic..
Linear Mold Shrinkage <= 0.00020 cm/cm
<= 0.00020 in/in
Typical, molds cut to zero
Azdel SuperLite® SL551200-100 PP Resin Matrix / 55% Glass Fiber (4 mm Molded Thickness)
AZDEL SuperLite® SL551200-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic..
Linear Mold Shrinkage 0.00020 cm/cm
0.00020 in/in
ASTM D2566-69
BCC Products HPX-850 Epoxy Backfill System
HPX-850 is a light weight, heat resistant, two component epoxy backfill system. HPX-850 features advantages such as low cost, long pot life, machineability, and low shrinkage. HPX-850 is ideally su..
Linear Mold Shrinkage 0.00020 - 0.0020 cm/cm

@Thickness 4.00 mm
0.00020 - 0.0020 in/in

@Thickness 0.157 in
Teijin Panlite® BN-8120R Improved Mold Release, Carbon Fiber Reinforced, Flame Resistant Polycarbonate Resin
CF 20% reinforced grade, meeting UL 94 V-2. It has excellent strength, stiffness, heat resistance and electric conductivity. Other features are flame retardance, low molding shrinkage and dimensiona..
Linear Mold Shrinkage <= 0.00020 cm/cm
<= 0.00020 in/in
Typical, molds cut to zero
Azdel SuperLite® SL551400-100 PP Resin Matrix / 55% Glass Fiber (2 mm Molded Thickness)
AZDEL SuperLite® SL551400-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic..
Linear Mold Shrinkage <= 0.00020 cm/cm
<= 0.00020 in/in
Typical, molds cut to zero
Azdel SuperLite® SL551600-100 PP Resin Matrix / 55% Glass Fiber (2 mm Molded Thickness)
AZDEL SuperLite® SL551600-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic..