Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Surface Area | 25 m²/g | 25 m²/g | |
NanoAmor 95%; OD: 200-500 nm Carbon Nanofibers ApplicationsCatalyst support materialsElectronic devicesFiber/polymer nanocomposites for enhanced electrical conductivityFiber/polymer nanocomposites for enhanced strengthFuel-cell electrodesGas sto.. |
|||
Specific Surface Area | 25 - 35 m²/g | 25 - 35 m²/g | BET |
NanoAmor 95%; OD: 80-200 nm Carbon Nanofibers ApplicationsCatalyst support materialsElectronic devicesFiber/polymer nanocomposites for enhanced electrical conductivityFiber/polymer nanocomposites for enhanced strengthFuel-cell electrodesGas sto.. |
|||
Specific Surface Area | 25 - 35 m²/g | 25 - 35 m²/g | BET |
NanoAmor 99.8%; OD: 80-200 nm Graphitized Carbon Nanofibers ApplicationsCatalyst support materialsElectronic devicesFiber/polymer nanocomposites for enhanced electrical conductivityFiber/polymer nanocomposites for enhanced strengthFuel-cell electrodesGas sto.. |
|||
Specific Surface Area | 25 - 35 m²/g | 25 - 35 m²/g | |
Zircar Zirconia ZYP-30 Zirconia Powder Zircar Zirconia Powder Type ZYP is an ultra fine, highly reactive powder composed of yttria- stabilized zirconia. It is offered with two different surface areas; Type ZYP-30 has a surface area of 25.. |
|||
Specific Surface Area | 25 m²/g | 25 m²/g | BET Analysis |
Gwent Electronic Materials P2121112P1 Acid Vapor Plasma Modified Graphene Nanoplatelets Production Method: Plasma Exfoliation of Natural GraphiteColor: Black/Grey Trial product which has not yet been extensively tested.Information provided by Gwent Electronic Materials Ltd. |
|||
Specific Surface Area | 25 m²/g | 25 m²/g | BET Analysis |
Gwent Electronic Materials P2121112P2 Argon Plasma Modified Graphene Nanoplatelets Production Method: Plasma Exfoliation of Natural GraphiteColor: Black/Grey Trial product which has not yet been extensively tested.Information provided by Gwent Electronic Materials Ltd. |
|||
Specific Surface Area | 25 m²/g | 25 m²/g | BET Analysis |
Gwent Electronic Materials P2121112P4 Nitrogen Plasma Modified Graphene Nanoplatelets Production Method: Plasma Exfoliation of Natural GraphiteColor: Black/Grey Trial product which has not yet been extensively tested.Information provided by Gwent Electronic Materials Ltd. |
|||
Specific Surface Area | 25 m²/g | 25 m²/g | BET Analysis |
Gwent Electronic Materials P2121112P5 Ammonia Plasma Modified Graphene Nanoplatelets Production Method: Plasma Exfoliation of Natural GraphiteColor: Black/Grey Trial product which has not yet been extensively tested.Information provided by Gwent Electronic Materials Ltd. |
|||
Specific Surface Area | 25 m²/g | 25 m²/g | BET Analysis |
Gwent Electronic Materials P2121112P6 Oxygen Plasma Modified Graphene Nanoplatelets Production Method: Plasma Exfoliation of Natural GraphiteColor: Black/Grey Trial product which has not yet been extensively tested.Information provided by Gwent Electronic Materials Ltd. |
|||
Specific Surface Area | 25 m²/g | 25 m²/g | BET Analysis |
Gwent Electronic Materials P2121112P3 Tetrafluoromethane Plasma Modified Graphene Nanoplatelets Production Method: Plasma Exfoliation of Natural GraphiteColor: Black/Grey Trial product which has not yet been extensively tested.Information provided by Gwent Electronic Materials Ltd. |
|||
Specific Surface Area | 25 - 35 m²/g | 25 - 35 m²/g | |
Zircar Zirconia ZYP-30 Zirconia Powder Zircar Zirconia Powder Type ZYP is an ultra fine, highly reactive powder composed of yttria- stabilized zirconia. It is offered with two different surface areas; Type ZYP-30 has a surface area of 25.. |
|||
Specific Surface Area | 25 - 50 m²/g | 25 - 50 m²/g | |
American Elements Hafnium Oxide Nanopowder General DescriptionHafnium Oxide or Hafnia Nanopowder or Nanoparticles (HfO), nanodots or nanocrystals are white high surface area particles. Nanoscale Hafnium Oxide Nanoparticles are typically 5 - .. |
|||
Specific Surface Area | 25 - 50 m²/g | 25 - 50 m²/g | |
American Elements Indium Oxide Nanopowder General DescriptionIndium Oxide Nanopowder or Nanoparticles (InO), nanodots or nanocrystals are white high surface area particles. Nanoscale Indium Oxide Nanoparticles are typically 5 - 100 nanomete.. |
|||
Specific Surface Area | 25 - 50 m²/g | 25 - 50 m²/g | |
American Elements Magnesium Oxide Nanopowder General DescriptionMagnesium Oxide Nanoparticles or Magnesia Nanoparticles (MgO) Nanoparticles, nanodots or nanopowder are spinel, high surface area particles. Nanoscale Magnesium Oxide Nanoparticle.. |
|||
Specific Surface Area | 25 - 50 m²/g | 25 - 50 m²/g | |
American Elements Manganese Oxide Nanopowder General DescriptionManganese Oxide Nanopowder (MnO), nanodots or nanoparticles are high surface area particles. Nanoscale Manganese Oxide Nanoparticles are typically 5 - 100 nanometers (nm) with spe.. |
|||
Specific Surface Area | 25 - 50 m²/g | 25 - 50 m²/g | |
American Elements Niobium Oxide Nanoparticles General DescriptionNiobium Oxide ( MoO) Nanopowder or Nanoparticles, nanodots or nanocrystals are ferric and ferrous spherical or faceted high surface area oxide magnetic nanostructure particles. Na.. |
|||
Specific Surface Area | 25 - 75 m²/g | 25 - 75 m²/g | |
American Elements Silicon Nitride Nanoparticles General DescriptionSilicon Nitride (SiN) Nanoparticles, nanodots or nanopowder are spherical high surface area particles. Nanoscale Silicon Nitride Particles are typically 10 - 100 nanometers (nm) w.. |
|||
Specific Surface Area | 25 - 50 m²/g | 25 - 50 m²/g | |
American Elements Silicon Oxide Nanopowder General DescriptionSilicon Oxide (SiO2) Nanopowder, Silica Nanoparticles or nanodots are high surface area particles. Nanoscale Silicon Oxide Nanoparticles or Silica Particles are typically 5 - 100 .. |
|||
Specific Surface Area | 25 - 50 m²/g | 25 - 50 m²/g | |
American Elements Yttria stabilized Zirconia General DescriptionYttria stabilized Zirconia or Zirconium Oxide Nanopowder or Nanoparticles (YSZ), nanodots or nanocrystals are white high surface area particles available fully stabilized (8 mol%).. |
|||
Specific Surface Area | 25 - 50 m²/g | 25 - 50 m²/g | |
American Elements Zirconium Oxide Nanopowder General DescriptionZirconium Oxide or Zirconia Nanopowder or Nanoparticles (ZrO2), nanodots or nanocrystals are white high surface area particles available in monoclinic or as stabilized or doped wi.. |
|||
Specific Surface Area | 25 m²/g | 25 m²/g | |
BASF Paliotol™ Yellow L 2140 Color Additive Description: Isoindoline yellow with high opacity and reddish shade for OEM and industrial coatings.Suitable for: Baking systems, Waterborn systems, Acrylic-isocyanate systems, Acid curing system, A.. |