Category Carbon
Manufacturer Nanostructured & Amorphous Materials Inc
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF NanoAmor 95%; OD: 80-200 nm Carbon Nanofibers.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
ApplicationsCatalyst support materialsElectronic devicesFiber/polymer nanocomposites for enhanced electrical conductivityFiber/polymer nanocomposites for enhanced strengthFuel-cell electrodesGas storage (nanoscale gas cylinders)High-power electrochemical capacitorsHigh surface-area electrodesLithium-ion batteriesShielding of electromagnetic radiationInformation provided by NanoAmor Inc.
Physical Properties Metric English Comments
Density 1.90 g/cc
0.0686 lb/in³
True Density
Apparent Bulk Density 0.0600 - 0.0800 g/cc
0.00217 - 0.00289 lb/in³
Particle Size 0.0010 - 0.010 µm
0.0010 - 0.010 µm
core diameter
0.080 - 0.20 µm
0.080 - 0.20 µm
outside diameter
Specific Surface Area 25 - 35 m²/g
25 - 35 m²/g
BET
Mechanical Properties Metric English Comments
Modulus of Elasticity 0.0200 - 0.180 GPa
2.90 - 26.1 ksi
Electrical Properties Metric English Comments
Electrical Resistivity 7.50e-7 - 1.00e-6 ohm-cm
7.50e-7 - 1.00e-6 ohm-cm
Descriptive Properties Value Comments
Color black
Length (um) 0.5-20
Purity (vol% carbon nanotubes), min 95