Zircar Zirconia ZYP-30 Zirconia Powder

Category Ceramic , Machinable Ceramic , Oxide , Zirconium Oxide
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Zircar Zirconia ZYP-30 Zirconia Powder.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Zircar Zirconia Powder Type ZYP is an ultra fine, highly reactive powder composed of yttria- stabilized zirconia. It is offered with two different surface areas; Type ZYP-30 has a surface area of 25-35 square meters per gram. Sintering of ZYP powder particles begins around 900°C and zirconia ceramic bodies approaching theoretical density can be achieved using ZYP as low as 1450°C.Features: Available in Two Surface AreasExtreme Environmental StabilityStabilized with ~10 wt% YttriaLow Sintering TemperaturePre-fired and Organic FreeAvailable ‘Off the Shelf’Application Information: ZYP is used for filtration mediaZYP can be used in the fabrication of Oxygen sensorsZYP can be used in thermal barrier coatings for gas turbines and diesel enginesZYP can be used as a grain growth inhibitor for non-oxide ceramicsInformation provided by Zircar Zirconia.
Physical Properties Metric English Comments
Loss On Ignition 1.8 %
1.8 %
Specific Surface Area 25 - 35 m²/g
25 - 35 m²/g
Component Elements Properties Metric English Comments
Chlorine, Cl 1.8 %
1.8 %
H2O 0.15 %
0.15 %
HfO2 1.0 - 2.0 %
1.0 - 2.0 %
Y2O3 10 %
10 %
ZrO2 88 - 89 %
88 - 89 %
Descriptive Properties Value Comments
Trace Impurities <1%