American Elements Hafnium Oxide Nanopowder

Category Ceramic , Oxide
Manufacturer American Elements
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF American Elements Hafnium Oxide Nanopowder.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
General DescriptionHafnium Oxide or Hafnia Nanopowder or Nanoparticles (HfO), nanodots or nanocrystals are white high surface area particles. Nanoscale Hafnium Oxide Nanoparticles are typically 5 - 100 nanometers (nm) with specific surface area (SSA) in the 25 – 50 m 2 /g range. Nano Hafnium Oxide Particles are also available in Ultra high purity and high purity and coated and dispersed forms. Applications for Hafnium oxide or hafnia nanocrystals include in fuel cells, in dielectric coatings and other electronic applications.
Physical Properties Metric English Comments
Particle Size 0.0050 - 0.10 µm
0.0050 - 0.10 µm
Specific Surface Area 25 - 50 m²/g
25 - 50 m²/g
Molecular Weight 210.49 g/mol
210.49 g/mol
Descriptive Properties Value Comments
Appearance White