Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Surface Area | 10 m²/g | 10 m²/g | |
Old Hickory M&M Clays, Inc. Wilco-LPC Kaolin Clay Wilco LPC is the same selection as the SLU grade except it is in natural shredded or Airfloat (powdered) form. It offers the same benefits in a ceramic casting formulation discussed above for the SL.. |
|||
Specific Surface Area | 10 m²/g | 10 m²/g | |
Old Hickory M&M Clays, Inc. Wilco-SLU Kaolin Clay Wilco SLU is an aqueous suspension of kaolin produced at 70% solids content. The slurry is deflocculated and rheology stabilized with sodium silicate. The Wilco SLU grade is a highly permeable selec.. |
|||
Specific Surface Area | 10 m²/g | 10 m²/g | |
Omya COVERCARB® HP Calcium Carbonate An ultrafine ground calcium carbonate for paper and board coating. An opacifying product that is designed to reduce coating costs through the replacement of more expensive pigments. This product is .. |
|||
Specific Surface Area | 10 - 16 m²/g | 10 - 16 m²/g | |
NYC YT3W Y2O3 Powder |
|||
Specific Surface Area | 10 - 16 m²/g | 10 - 16 m²/g | |
NYC YT3WP Y2O3 Granules |
|||
Specific Surface Area | 10 m²/g | 10 m²/g | BET; DIN 66132 |
3M Dyneon™ TF 9201 PTFE
(discontinued **) Low molecular weight virgin PTFE (non-degraded)Agglomerate particlesEasily deagglomerated when incorporated into other matrixesSuitable for use in food contact applications. Complies with FDE specif.. |
|||
Specific Surface Area | 10 - 16 m²/g | 10 - 16 m²/g | BET |
H.C. Starck Grade C Yttrium Oxide Sintering additive for Si3N4 and ALNStabilizer for zirconias (PSZ) and insulating coatings (TBC`s)Catalyst carrierYttria stabilized zirconias electrolytes for solid oxide fuel cellsLuminescent mater.. |
|||
Specific Surface Area | >= 10 m²/g | >= 10 m²/g | BET |
H.C. Starck Grade I Amorphous Boron Automotive (igniter in airbags and belt tighteners)Additive in pyrotechnic mixtures (flares, igniters, and delay compositions)Additive in solid rocket propellant fuels and explosivesPreparation of r.. |
|||
Specific Surface Area | 10 - 20 m²/g | 10 - 20 m²/g | BET |
H.C. Starck Grade C Boron Nitride, BN White powder for hot pressing (min. lot size 100 kg)Solid lubricant for high-temperature applicationsMold release for die casting and injection moldingRaw material for cubic BNThermally conductive f.. |
|||
Specific Surface Area | 10 - 300 m²/g | 10 - 300 m²/g | |
Terio Corporation TZOH-40 Zirconium Hydroxide Information provided by TERIO Corporation. |
|||
Specific Surface Area | 10 - 300 m²/g | 10 - 300 m²/g | |
Terio Corporation TZOH-50 Zirconium Hydroxide Information provided by TERIO Corporation. |
|||
Specific Surface Area | 10 - 300 m²/g | 10 - 300 m²/g | |
Terio Corporation TZOH-60 Zirconium Hydroxide Information provided by TERIO Corporation. |
|||
Specific Surface Area | 10 - 12 m²/g | 10 - 12 m²/g | High Range |
Vesta Ceramics SicoNide® P Silicon Nitride Powder General Description:SicoNide® is a silicon nitride powder with a broad particle size distribution allowing better, tighter packing when pressed. Our computer-controlled production processes guaran.. |
|||
Specific Surface Area | 10 - 12 m²/g | 10 - 12 m²/g | High Range |
Vesta Ceramics SicoNide® S S Silicon Nitride Powder General Description:SicoNide® is a silicon nitride powder with a broad particle size distribution allowing better, tighter packing when pressed. Our computer-controlled production processes guaran.. |
|||
Specific Surface Area | 10 m²/g | 10 m²/g | BET |
TIMCAL TIMREX® MK15 Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |
|||
Specific Surface Area | 10 m²/g | 10 m²/g | BET |
TIMCAL TIMREX® PP 10 Natural Flake Graphite TIMREX Natural Flake Graphite is produced in a wide range of products distinguished by particle size distribution, chemistry and carbon content. Timcal mines the graphite from its own source in Lac-.. |
|||
Specific Surface Area | 10 m²/g | 10 m²/g | BET |
TIMCAL TIMREX® T44 Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |
|||
Specific Surface Area | 10 - 75 m²/g | 10 - 75 m²/g | |
American Elements Aluminum Nitride Nanoparticles General DescriptionAluminum Nitride (AlN) Nanoparticles, nanodots or nanopowder are spherical high surface area particles. Nanoscale Aluminum Nitride Particles are typically 10 - 100 nanometers (nm).. |
|||
Specific Surface Area | 10 - 50 m²/g | 10 - 50 m²/g | |
American Elements Antimony Oxide Nanopowder General DescriptionAntimony Oxide ( SbO) Nanopowder or Nanoparticles, nanodots or nanocrystals are ferric and ferrous spherical or faceted high surface area oxide magnetic nanostructure particles. N.. |
|||
Specific Surface Area | 10 - 50 m²/g | 10 - 50 m²/g | |
American Elements Bismuth Oxide Nanopowder General DescriptionBismuth Oxide ( BiO) Nanopowder or Nanoparticles, nanodots or nanocrystals are ferric and ferrous spherical or faceted high surface area oxide magnetic nanostructure particles. Na.. |
|||
Specific Surface Area | 10 - 75 m²/g | 10 - 75 m²/g | |
American Elements Boron Carbide Nanoparticles General DescriptionBoron Carbide (BC) Nanoparticles, nanodots or nanopowder are spherical high surface area particles. Nanoscale Boron Carbide Particles are typically 10 - 100 nanometers (nm) with s.. |
|||
Specific Surface Area | 10 - 75 m²/g | 10 - 75 m²/g | |
American Elements Boron Nitride Nanoparticles General DescriptionBoron Nitride (BN) Nanoparticles, nanodots or nanopowder are spherical high surface area particles. Nanoscale Boron Nitride Particles are typically 10 - 100 nanometers (nm) with s.. |
|||
Specific Surface Area | 10 - 50 m²/g | 10 - 50 m²/g | |
American Elements Molybdenum Oxide Nanopowder General DescriptionMolybdenum Oxide ( MoO) Nanopowder or Nanoparticles, nanodots or nanocrystals are ferric and ferrous spherical or faceted high surface area oxide magnetic nanostructure particles... |
|||
Specific Surface Area | 10 - 75 m²/g | 10 - 75 m²/g | |
American Elements Silicon Nanotubes General DescriptionSilicon (Si) Nanotubes, Single-Walled, Double Walled and Multi-Walled are tubular ultra high surface area nanotubes. Nanoscale Silicon Nanotubes are typically 10 - 100 nanometers .. |
|||
Specific Surface Area | 10 - 50 m²/g | 10 - 50 m²/g | |
American Elements Tantalum Oxide Nanopowder General DescriptionTantalum Oxide ( TaO) Nanopowder or Nanoparticles, nanodots or nanocrystals are ferric and ferrous spherical or faceted high surface area oxide magnetic nanostructure particles. N.. |
|||
Specific Surface Area | 10 - 80 m²/g | 10 - 80 m²/g | |
American Elements Tin Oxide Nanopowder General DescriptionTin Oxide ( SnO) Nanopowder or Nanoparticles, nanodots or nanocrystals are spherical or faceted high surface area oxide magnetic nanostructure particles. Nanoscale Tin Oxide Parti.. |
|||
Specific Surface Area | 10 - 75 m²/g | 10 - 75 m²/g | |
American Elements Titanium Nitride Nanoparticles General DescriptionTitanium Nitride (TiN) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Titanium Nitride Particles are typically 10 - 100 nanometer.. |
|||
Specific Surface Area | 10 - 80 m²/g | 10 - 80 m²/g | |
American Elements Tungsten Oxide Nanopowder General DescriptionTungsten Oxide ( WO) Nanopowder or Nanoparticles, nanodots or nanocrystals are spherical or faceted high surface area oxide magnetic nanostructure particles. Nanoscale Tin Oxide P.. |
|||
Specific Surface Area | 10 m²/g | 10 m²/g | |
BASF Sicopal® Yellow L 1100 Color Additive Description: Weather-resistant inorganic bismuth vanadate pigment with high hiding power Chemical Structure: Bismuth vanadatSuitable for: Baking System, Waterborn systems, Acrylic-isocyanate systems.. |
|||
Specific Surface Area | <= 10 m²/g | <= 10 m²/g | |
Momentive Performance Materials PolarTherm® PT620 Boron Nitride (BN) Powder High Density BN AgglomerateWhen used in a variety of polymeric materials, PolarTherm™'s heat dissipating capability helps extend the service life and enhance the reliability of electronic comp.. |