American Elements Tantalum Oxide Nanopowder

Category Ceramic , Oxide
Manufacturer American Elements
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF American Elements Tantalum Oxide Nanopowder.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
General DescriptionTantalum Oxide ( TaO) Nanopowder or Nanoparticles, nanodots or nanocrystals are ferric and ferrous spherical or faceted high surface area oxide magnetic nanostructure particles. Nanoscale Tantalum Oxide Particles are typically 20-80 nanometers (nm) with specific surface area (SSA) in the 10 – 50 m 2 /g range and also available in with an average particle size of 100 nm range with a specific surface area of approximately 7- 10 m 2 /g. Nano Tantalum Oxide Particles are also available in ultra high purity and high purity, transparent, and coated and dispersed forms. Applications for Tungsten Oxide Nanocrystals include in dental imaging because they are sufficiently radiopaque (is impervious to radiation) for good X-ray resolution, and in coatings, plastics, nanowire, nanofiber and textiles and in certain alloy and catalyst applications. Further research is being done for their potential electrical, dielectric, magnetic, optical, imaging, biomedical and bioscience properties.
Physical Properties Metric English Comments
Particle Size 0.020 - 0.080 µm
0.020 - 0.080 µm
0.10 µm
0.10 µm
Specific Surface Area 7.0 - 10 m²/g
7.0 - 10 m²/g
10 - 50 m²/g
10 - 50 m²/g
Molecular Weight 441.89 g/mol
441.89 g/mol
Descriptive Properties Value Comments
Appearance White