H.C. Starck Grade I Amorphous Boron

Category Metal , Nonferrous Metal , Pure Element
Manufacturer H.C. Starck
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF H.C. Starck Grade I Amorphous Boron.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Automotive (igniter in airbags and belt tighteners)Additive in pyrotechnic mixtures (flares, igniters, and delay compositions)Additive in solid rocket propellant fuels and explosivesPreparation of refractory metal boridessintering additive for SiC advanced ceramicsReducing additive in fluxes for soldering stainless steelNeutron absorber in nuclear technology
Physical Properties Metric English Comments
Particle Size 1.0 - 2.0 µm
1.0 - 2.0 µm
Laser Diffraction D50
Specific Surface Area >= 10 m²/g
>= 10 m²/g
BET
Component Elements Properties Metric English Comments
Boron, B >= 95 %
>= 95 %
Magnesium, Mg <= 0.80 %
<= 0.80 %