Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | >= 2.0 µm | >= 2.0 µm | 10% smaller than |
Nyco NYAD® M400 Wollastonite Powdered grade.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance m.. |
|||
Particle Size | >= 2.0 µm | >= 2.0 µm | 10% smaller than |
Nyco NYAD® MD400 Wollastonite Powdered grade.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance m.. |
|||
Particle Size | 2.0 µm | 2.0 µm | |
Nabaltec NABALOX® NO 715-10 Reactive Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Particle Size | 2.0 µm | 2.0 µm | Median particle diameter |
Old Hickory M&M Clays, Inc. Wilco-LPC Kaolin Clay Wilco LPC is the same selection as the SLU grade except it is in natural shredded or Airfloat (powdered) form. It offers the same benefits in a ceramic casting formulation discussed above for the SL.. |
|||
Particle Size | <= 2.0 µm | <= 2.0 µm | |
Hong Kun Group DBDPE Flame Retardant Chemical Name:1,2-Bis(pentabromophenyl) ethaneDecabromodiphenylethaneDecabromodiphenyl EthylCAS No. 84852-53-9All information provided by Hongkun Group |
|||
Particle Size | 2.0 - 6.0 µm | 2.0 - 6.0 µm | Primary crystal size |
Magyar Aluminum ALO-Ex35 LS Alumina Calcined Alumina |
|||
Particle Size | >= 2.0 µm | >= 2.0 µm | 2% finer |
Malvern Minerals Novakup® L-207A Surface-Treated Lamellar Quartz Filler/Extender Novakup® is a surface modified or silane treated Novacite®. It has been used its barrier prosperities in chemical and corrosion resistant applications and as a filler/extender/reinforcing agen.. |
|||
Particle Size | 2.0 µm | 2.0 µm | 67% finer than |
Imerys Carverâ„¢ Kaolin Information provided by Imerys |
|||
Particle Size | 2.0 µm | 2.0 µm | 60% finer than |
Imerys DB-Floatâ„¢ Kaolin Information provided by Imerys |
|||
Particle Size | 2.0 µm | 2.0 µm | 68% finer than |
Imerys Diamondâ„¢ Kaolin Diamond is an intermediate-grained montmorillonitc kaolin used primarily in plastic formed bodies. This kaolin is known for its good strength and white-firing characteristics.Information provided by.. |
|||
Particle Size | 2.0 µm | 2.0 µm | 58% finer than |
Imerys Ewingâ„¢ Kaolin Ewing is an intermediate grained air-floated kaolin which is selected, processed and controlled to meet specific requirements of the fibreglass industry.Information provided by Imerys |
|||
Particle Size | 2.0 µm | 2.0 µm | 63% finer than |
Imerys Franklin™ R Kaolin Franklin R is an intermediate-grained Kaolin used as a filler is “soft†rubber products, plastic compounds, adhesives, protective coatings and similar applications.Information provided by .. |
|||
Particle Size | 2.0 µm | 2.0 µm | 62% finer than |
Imerys KT-Cast/Rogersâ„¢ Kaolin Information provided by Imerys |
|||
Particle Size | <= 2.0 µm | <= 2.0 µm | Main Break; Fineness of Grind |
Gwent Electronic Materials C2021031D3 Electrode Ink Electrode Ink C2021031D3 is a Silver Palladium (90/10) electrode ink, designed for use with PVB Tape. It has been specifically formulated for use with PZT ceramics.The ink is in a ready to use form.. |
|||
Particle Size | 2.0 - 4.5 µm | 2.0 - 4.5 µm | Average Particle Size/Laser Diffraction D50 |
H.C. Starck Grade B Aluminum Nitride AIN High thermally conductive ceramicsComposite ceramicsSiAlONsHeat sinksElectrically insulating packages for electronicsCrucibles for metals and salt meltsThermally conductive filler for polymersCompon.. |
|||
Particle Size | 2.0 - 3.0 µm | 2.0 - 3.0 µm | Average Particle Size/Laser Diffraction D50 |
H.C. Starck Grade C Molybdenum Disilicide MoSi2 Composite ceramicsHeating elementsConstituent of glow plugs for enginesRaw material for MoSi2 sputter target (PVD) |
|||
Particle Size | 2.0 - 6.0 µm | 2.0 - 6.0 µm | X50% |
Solvay Chemicals NOCOLOK® Flux P2 Potassium Fluoroaluminate Mixtures of NOCOLOK® Flux P2 with NOCOLOK® Flux allow for gradual viscosity adjustments in suspensions to suit specific process conditions.HS No.: 38109090 /CAS-No.: 60304-36-1Uses: Automoti.. |
|||
Particle Size | 2.0 µm | 2.0 µm | Medium Grain (d50) |
CeramTec Rubalit® HSS Alumina, 75% (High Strength Substrate) Rubalit® HSS (High Strength Substrate) displays the successful union of elasticity and strength. The ultrafine microstructure of Rubalit® HSS is the basis for its outstanding substrate surface qua.. |
|||
Particle Size | 2.0 µm | 2.0 µm | D10 (Malvern) Size D |
Vesta Ceramics SicoMill® Grade 2 Silicon Powder General Description:SicoMill® is a fine-grained silicon powder, specially developed for the ceramic industry. We have five standard grinding grades, but we can produce powders adapted to single cu.. |
|||
Particle Size | 2.0 µm | 2.0 µm | D10 (Malvern) Size D |
Vesta Ceramics SicoMill® Grade 4 Silicon Powder General Description:SicoMill® is a fine-grained silicon powder, specially developed for the ceramic industry. We have five standard grinding grades, but we can produce powders adapted to single cu.. |
|||
Particle Size | 2.0 - 7.0 µm | 2.0 - 7.0 µm | |
Dow Corning EP-9215 Cosmetic Powder A hard white elastomeric silicone powder that provides a silky and powdery skin feel, along with oil and sebum absorption. It also improves color intensity and coverage in pressed powder formulation.. |
|||
Particle Size | 2.0 µm | 2.0 µm | D50 |
Dandong Taico Minerals TAICOCITE® TC50 Magnesium Hydroxide Made from local natural brucite minerals, TAICOCITE® is the name of milled magnesium hydroxide products which is produced (micronized/surface treated) by Dandong Taico Minerals Co., Ltd. TAICOCITE®.. |
|||
Particle Size | 2.0 µm | 2.0 µm | |
China Tungsten YG6 Tungsten Carbide Powder Information provided by China Tungsten |
|||
Particle Size | 2.0 µm | 2.0 µm | Median |
CIMBAR CIMBAR™ UF Barite Powder (BaSO4) CIMBAR barite products are made using only the highest quality white, natural barium sulfate ore. CIMBAR barites unique properties of fine grind, high specific gravity, low solubility and chemical .. |
|||
Particle Size | <= 2.0 µm | <= 2.0 µm | 10% |
BYK Cloisite® 93A Nanoclay Cloisite® 93A is an additive for plastics to improve various plastic physical properties, such as reinforcement, HDT, CLTE and barrier.Information provided by Southern Clay ProductsSouthern Clay Pr.. |
|||
Particle Size | 2.0 µm | 2.0 µm | |
Astro Met AmAlOx 87 Alumina - Aluminum Oxide General Description:AmAlOx 87 alumina (Astro Met Aluminum Oxide) is a 99.95% alumina ceramic manufactured by Astro Met for specialty applications which require a higher purity of alumina than found .. |
|||
Particle Size | 2.0 µm | 2.0 µm | Hegman; Grinde Gauge |
3M Dyneon™ J14 PTFE Micropowder 3M™ Dyneon™ PTFE Micropowders can be used as additives in many applications and at concentrations typically from 5 to 20%. Homogeneous incorporation is the single most important process and applic.. |
|||
Particle Size | 2.0 - 3.0 µm | 2.0 - 3.0 µm | Median Grain (d50) |
CeramTec 977 Zirconia Toughened Alumina (ZTA), Al2O3•ZrO2 977 is a zirconia toughened alumina ceramic designed for use in ballistic protection and ceramic armor. |
|||
Particle Size | <= 2.0 µm | <= 2.0 µm | 10% |
BYK Cloisite® Na+ Nanoclay Cloisite® Na+ is an additive for plastics to improve various plastic physical properties, such as reinforcement, HDT, CLTE and barrier.Information provided by Southern Clay ProductsSouthern Clay Pr.. |