Information provided by China Tungsten
Physical Properties Metric English Comments
Bulk Density 3.40 g/cc
0.123 lb/in³
Scott
Density 14.9 g/cc
0.538 lb/in³
Binder 2.0
2.0
wax
Particle Size 2.0 µm
2.0 µm
Mechanical Properties Metric English Comments
Hardness, Rockwell A 91.5
91.5
Tensile Strength, Ultimate 2200 MPa
319000 psi
Component Elements Properties Metric English Comments
Cobalt, Co 6.0 %
6.0 %
WC 94 %
94 %
Descriptive Properties Value Comments
Flow Rate; sec/50g 28