Material Notes:
General Description:AmAlOx 87 alumina (Astro Met Aluminum Oxide) is a 99.95% alumina ceramic manufactured by Astro Met for specialty applications which require a higher purity of alumina than found in commercial grades of 99.5% and 99.8% alumina. AmAlOx 87 alumina is especially cost effective for applications, which need the unique combination of high purity, high strength, high density and small grain size in one material.AmAlOx 87 alumina, originally developed for critical load bearing medical implants, has an unusually small grain size for an alumina ceramic, this enables extremely tight tolerances and surface finishes of 2 microinches Ra to be achieved when proper finishing techniques are used.
Physical Properties Metric English Comments
Bulk Density 3.97 g/cc
0.143 lb/in³
Particle Size 2.0 µm
2.0 µm
Mechanical Properties Metric English Comments
Hardness, Vickers 2000
2000
Flexural Strength 482 MPa
69900 psi
Component Elements Properties Metric English Comments
Al2O3 99.95 %
99.95 %