Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | >= 1.0 µm | >= 1.0 µm | 10% smaller than |
Nyco 10 AS WOLLASTOCOAT® Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Particle Size | >= 1.0 µm | >= 1.0 µm | 10% smaller than |
Nyco M1250 WOLLASTOCOAT® Wollastonite Chemically treated grade.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal per.. |
|||
Particle Size | 1.0 µm | 1.0 µm | |
Poco Graphite ZXF-5Q Industrial Grade Graphite SSH hardness is 86.General Poco Specialty Graphite Information: Poco's high strength, fine-grained, isotropic graphites offer maximum design flexibility. Easily machined. High strength and small p.. |
|||
Particle Size | 1.0 µm | 1.0 µm | 52% of particles less than |
Old Hickory FC-340 Tennessee Ball Clay The FC-340 clay is designed for all types of casting formulas ranging from low fire earthenware to vitreous composition. It has excellent response to deflocculation and a very good casting rate whil.. |
|||
Particle Size | 1.0 µm | 1.0 µm | 61% of particles less than |
Old Hickory M-33 Kentucky Ball Clay The M-33 ball clay is a carbonaceous selection that bears similarity to some clays found in the Southwestern section of England. It has a uniquely waxy type of plasticity and provides high green and.. |
|||
Particle Size | 1.0 µm | 1.0 µm | 63% of particles less than |
Old Hickory No. 1 Glaze Kentucky Ball Clay No. 1 Glaze Clay is a very high kaolin bearing selection with extremely low levels of carbon content. it provides excellent suspension to all types of glazes especially glazes containing a high perc.. |
|||
Particle Size | 1.0 µm | 1.0 µm | 60% of particles less than |
Old Hickory No. 5 Kentucky Ball Clay No. 5 clay is a kaolinitic ball clay containing low levels of carbon. It provides high suspension and plasticity to a variety of ceramic formulations and is an excellent source of Al2O3 content. No... |
|||
Particle Size | 1.0 µm | 1.0 µm | at 80% distribution <1 to 5 microns. |
PolyChem Alloy 6004 Talc Nucleator Talc nucleator products are additive masterbatch concentrates designed for the nucleation of both commodity and engineering thermoplastic resins. Talc Nucleators typically contain 40 to 60 % by weig.. |
|||
Particle Size | <= 1.0 µm | <= 1.0 µm | |
Poco Graphite EDM-AF5 EDM Graphite POCO's EDM-AF5 is the only graphite electrode material available on the market today with an average particle size of less than one micron. This particle structure gives EDM-AF5 superior strength, p.. |
|||
Particle Size | >= 1.0 µm | >= 1.0 µm | 13% finer |
Malvern Minerals Novakup® L-337 Surface-Treated Lamellar Quartz Filler/Extender Novakup® is a surface modified or silane treated Novacite®. It has been used its barrier prosperities in chemical and corrosion resistant applications and as a filler/extender/reinforcing agen.. |
|||
Particle Size | 1.0 µm | 1.0 µm | 86% finer than |
Imerys Aftonâ„¢ Kaolin Afton is a fine-grained air floating kaolin which is widely used as an anit-caking agent in certain agricultural compounds.Information provided by Imerys |
|||
Particle Size | 1.0 µm | 1.0 µm | 47% finer than |
Imerys Allenâ„¢ Kaolin Allen is an intermediate-grained kaolin suitable for use as a filler and pigment in a wide variety of industrial applications such as soft rubber, plastics, ceiling tile, adhesives and paper product.. |
|||
Particle Size | 1.0 µm | 1.0 µm | 46.5% finer than |
Imerys DB-Floatâ„¢ Kaolin Information provided by Imerys |
|||
Particle Size | 1.0 µm | 1.0 µm | 49% finer than |
Imerys Kingsley - Rogersâ„¢ Kaolin Information provided by Imerys |
|||
Particle Size | 1.0 - 2.0 µm | 1.0 - 2.0 µm | FSSS |
H.C. Starck Ampersint® MAP FeNi 50/50 For Hardmetals High-temperature, oxidation-resistant, abrasion-resistant and biocompatible materials can be processed with all standard powder metallurgical technologies. The customized alloy can be supplied as a .. |
|||
Particle Size | 1.0 - 2.0 µm | 1.0 - 2.0 µm | Laser Diffraction D50 |
H.C. Starck Grade C Titanium Carbonitride Hard metals (tooling and machining)CermetsBlack ceramics |
|||
Particle Size | 1.0 - 1.5 µm | 1.0 - 1.5 µm | Average |
H.C. Starck Grade D Titanium Carbonitride Narrow grain distribution and low oxygen contentHard metals (tooling and machining)CermetsBlack ceramics |
|||
Particle Size | <= 1.0 µm | <= 1.0 µm | 2% |
SGL Carbon Group CF 1135 Carbon Filler Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Particle Size | 1.0 - 2.0 µm | 1.0 - 2.0 µm | D50 Sedigraph |
Solvay SUPER CEROXâ„¢ 1663 Surfactant Description: Super Ceroxâ„¢1663 is particularly suited for the polishing of ophthalmic lenses (mass production and prescription) and optical lenses. Benefits: High polishing efficiency, Very high.. |
|||
Particle Size | 1.0 µm | 1.0 µm | Rubber Particle Size |
UBE UBEPOL BR15H HIPS (n-DM = 0.03 wt % and PH-3H = 0.03 wt %) Description: UBEPOL-BR15H is a in-between polymer of UBEPOL-BR15HB and UBEPOL-BR15HL.Information provided by UBE. |
|||
Particle Size | 1.0 µm | 1.0 µm | Median |
CIMBAR BariScan Elite Chemically Purified White Barium Sulfate (BaSO4) BariScan barite products are produced using a proprietary chemical process to enhance the purity of the natural barium sulfate ore. BariScan and BariScan Ultra barite meet and exceed the requireme.. |
|||
Particle Size | 1.0 µm | 1.0 µm | @ 10% |
CIMBAR Gel Talc for Polyester Filler Gel Talc and Body Filler talc products are produced from high purity ore. Gel Talc and Body Filler products provide an excellent balance of color and mechanical properties for primary use in polyes.. |
|||
Particle Size | 1.0 µm | 1.0 µm | @ 10% |
CIMBAR RP 9410 Talc RP 9400 Series talcs are produced from ores, which provide an excellent balance of mechanical properties at an economical price, for primary use in commodity polypropylene. RP 9400 Series talcs are.. |
|||
Particle Size | 1.0 - 80 µm | 1.0 - 80 µm | 95% in range |
Arkema Group PLATAMID® H106 PA80 Powder Copolyamide Platamid® H106 PA powder is a special purpose, medium melting point, very low viscosity, thermoplastic copolyamide adhesive suitable for thermal bonding and laminating of textile and foam substrate.. |
|||
Particle Size | 1.0 - 2.5 µm | 1.0 - 2.5 µm | MA147LFE |
C.O.I.M. FILCO® 650 Film Former for Glass Fiber Sizes Description: Film Former for Glass Fiber SizesGeneral Information: COIM has developed a range of polyesters for the treatment of glass fiber. These polyesters come in powder and emulsion form and ar.. |
|||
Particle Size | 1.0 µm | 1.0 µm | 10" Percentile |
3M W-410 Ceramic Microspheres 3M™ White Ceramic Microspheres are unique, semi-transparent, white-colored, fine particle size, high-strength microspheres. These products are typically used to reduce VOC levels; increase filler l.. |
|||
Particle Size | >= 1.0 µm | >= 1.0 µm | 10% smaller than |
Nyco 10 ES WOLLASTOCOAT® Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |