Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 800 - 1200 µm | 800 - 1200 µm | |
Potters Industries A-Series A-100 Soda-Lime Silica Technical Quality Solid Glass Spheres Technical Quality, A-Series glass spheres are used to reduce particle size in coatings and inks. Glass Spheres used in oil well drilling improve lubrication and overall efficiencies of down hole oil.. |
|||
Particle Size | 800 - 1700 µm | 800 - 1700 µm | 98% range |
NOVA Chemicals Arcel 730 70% PS/30% PE Interpolymer ARCEL is a high-performance, moldable foam resin consisting of 70% polystyrene (PS) and 30% polyethylene (PE). ARCEL provides toughness, flexibility and durability in a lightweight foam.The strength.. |
|||
Particle Size | 800 - 1700 µm | 800 - 1700 µm | 98% within range |
NOVA Chemicals Arcel 730 LV Resin 70% Polystyrene/30% Polyethylene ARCEL advanced foam resin consists of polystyrene and polyethylene. ARCEL resin providesl toughness, flexibility and durability in a lightweight foam.The strength and flexibility of ARCEL resin crea.. |
|||
Particle Size | 800 µm | 800 µm | ASTM D4894 |
3M Dyneon™ TF 4103 PTFE 15% Glass Fiber Filled
(discontinued **) Type II PTFE. Applications include valve seats, bearings, seals/gaskets, moldings, piston rings.Data provided by Dyneon. |
|||
Particle Size | 800 µm | 800 µm | average; ASTM D4894 |
3M Dyneon™ TR 1105 PTFE
(discontinued **) Ideal for thin wall ram extrusion productsReduces cold flow and melt viscosityLower permeabilityLower porosityWeldableExcellent product smoothnessIncreased machine outputInformation provided by Dyne.. |
|||
Particle Size | <= 800 µm | <= 800 µm | sieve < 5% |
ICO Polymers ICOFLOâ„¢ 510-5051 800 Micron LDPE Powder Description: ICOFLO 510-5051 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma.. |
|||
Particle Size | <= 800 µm | <= 800 µm | sieve < 5% |
ICO Polymers ICOFLOâ„¢ 510-5054 800 Micron LDPE Powder Description: ICOFLO 510-5054 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma.. |
|||
Particle Size | <= 800 µm | <= 800 µm | sieve < 5% |
ICO Polymers ICOFLOâ„¢ 510-5057 80 Micron LDPE Powder Description: ICOFLO 510-5057 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma.. |
|||
Particle Size | <= 800 µm | <= 800 µm | sieve < 5% |
ICO Polymers ICOFLOâ„¢ 510-5060 800 Micron LDPE Powder Description: ICOFLO 510-5060 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a barrier in ma.. |
|||
Particle Size | <= 800 µm | <= 800 µm | sieve < 5% |
ICO Polymers ICOFLOâ„¢ 510-5063 800 Micron LDPE Powder Description: ICOFLO 510-5063 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma.. |
|||
Particle Size | <= 800 µm | <= 800 µm | sieve < 5% |
ICO Polymers ICOFLOâ„¢ 510-5074 800 Micron LLDPE Powder Description: ICOFLO 510-5074 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma.. |
|||
Particle Size | <= 800 µm | <= 800 µm | sieve < 5% |
ICO Polymers ICOFLOâ„¢ 510-5071 800 Micron LLDPE Powder Description: ICOFLO 510-5071 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma.. |
|||
Particle Size | 800 µm | 800 µm | |
TIMCAL TIMREX® FC800 Coke TIMREX Petroleum Coke is calcined at appropriate temperature with low ash and sulfur content, well defined texture and consistent particle size distribution.Advantages and applications: Suitable fo.. |
|||
Particle Size | 800 µm | 800 µm | Median |
Eliokem Chemigum® P7D Nitrile Elastomer High viscosity grade for friction materials. High gel strength. 33% bound ACN. Branched polymer structure. CaCO3 partitioning agent.Can be used in phenolic blends.Used in friction materials such.. |
|||
Particle Size | 800 µm | 800 µm | Median |
Eliokem Chemigum® P615D Nitrile Elastomer Medium viscosity grade for friction materials. 33% bound ACN. Linear polymer structure. CaCO3 partitioning agent.Can be used in phenolic blends.Used in friction materials such as disc-pads, clutc.. |
|||
Particle Size | 800 µm | 800 µm | Average |
Azoty Tarnow™ TARFLEN ST PTFE Free-Flowing suspension powder for ram extrusion of rods, pipes and other profiles.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Particle Size | 800 µm | 800 µm | |
Asahi Glass Fluon® PA3540LT 10% Carbon Fiber, 30% Bronze, PTFE Filled Compound Fluon®PTFE FC has improved creep and wear resistance. A wide range of fillers such as glass fiber, graphite, bronze, carbon fiber are available. Information provided by Asahi Glass Company, Inc. |