Material Notes:
Description: ICOFLO 510-5054 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in masterbatch (instead of pellet), superior color development or additive dispersion can be achieved in the final concentrate. Key Characteristics: good stiffness, good impact strength and excellent appearance. Information provided by ICO Polymers.A Schulman acquired ICO, Inc. in 2010.
Physical Properties Metric English Comments
Density 0.924 g/cc
0.0334 lb/in³
ASTM D1505
Particle Size >= 150 µm
>= 150 µm
pan, 13%
<= 800 µm
<= 800 µm
sieve < 5%
Melt Index of Compound 6.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
6.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 50
50
ASTM D2240
Elongation at Break 100 %
100 %
50 mm/min; ASTM D638
Tensile Modulus 0.200 GPa
29.0 ksi
1 mm/min; ASTM D638
Thermal Properties Metric English Comments
Melting Point 111 °C
232 °F
DSC; ASTM D3418
Vicat Softening Point 82.0 °C
180 °F
ASTM D1525
Processing Properties Metric English Comments
Processing Temperature 200 °C
392 °F
recommended
Descriptive Properties Value Comments
Max Dry Flow max 31 sec/100g
ASTM