Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 7.0 µm | 7.0 µm | median; Microtrac |
Nyco ASPECT® 3000 Wollastonite High aspect ratio grade. It is available untreated or with a surface modification treatment.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. .. |
|||
Particle Size | <= 7.0 µm | <= 7.0 µm | 90% smaller than |
Nyco NYAD® 5000 Wollastonite Fine particle size grade. This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distincti.. |
|||
Particle Size | >= 7.0 µm | >= 7.0 µm | 10% smaller than |
Nyco NYAD® MG Wollastonite High aspect ratio grade. This grade is recommended for elastomer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinct.. |
|||
Particle Size | 7.0 µm | 7.0 µm | median; Microtrac |
Nyco NYGLOS® 4W Wollastonite High aspect ratio grade. This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctiv.. |
|||
Particle Size | 7.0 µm | 7.0 µm | median; Microtrac |
Nyco RRIMGLOS® 4W Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Particle Size | <= 7.0 µm | <= 7.0 µm | <4% of particles are less than 20 microns |
Solvay Specialty Polymers Polymist® F-5A EX PTFE Powder Lubricant
(Unverified Data**) Polymist® powders are a family of white free-flowing polytetrafluoroethylene powders for use as additives in other materials to enhance processing or end-use performance characteristics. Polymist .. |
|||
Particle Size | 7.0 µm | 7.0 µm | 50% of particles, (REG Powder) |
Ferro IP 760 Passivation Glasses (Pb-B-Si-Al; Pb-Si-Al; Si-Pb-Al Silicates) Glass Type: Pb-B-Si-Al Typical Powder Form: TF, REG, RWG, SRRG Ferro's passivation glasses are designed for use on transistors, thyristors, and diodes. These products are formulated and produced to.. |
|||
Particle Size | 7.0 µm | 7.0 µm | 50% of particles, (REG Powder) |
Ferro IP 830 Passivation Glasses (Pb-B-Si-Al; Pb-Si-Al; Si-Pb-Al Silicates) Glass Type: Pb-B-Si-Al Typical Powder Form: TF, REG, RWG, SRRG Ferro's passivation glasses are designed for use on transistors, thyristors, and diodes. These products are formulated and produced to.. |
|||
Particle Size | 7.0 - 14 µm | 7.0 - 14 µm | average |
Malvern Minerals Novacite® 1250 Untreated Lamellar Quartz Filler/Extender Novacite® quartz silica has closely controlled sizing that is used extensively in the coatings field. Novacite® has broad acceptance as silica in special purpose, product finishes OEM, automo.. |
|||
Particle Size | 7.0 - 15 µm | 7.0 - 15 µm | average |
Malvern Minerals Novacite® 325 Untreated Lamellar Quartz Filler/Extender Novacite® quartz silica has closely controlled sizing that is used extensively in the coatings field. Novacite® has broad acceptance as silica in special purpose, product finishes OEM, automo.. |
|||
Particle Size | 7.0 - 14 µm | 7.0 - 14 µm | average |
Malvern Minerals Novakup® 1250 Surface-Treated Lamellar Quartz Filler/Extender Novakup® is a surface modified or silane treated Novacite®. It has been used its barrier prosperities in chemical and corrosion resistant applications and as a filler/extender/reinforcing agen.. |
|||
Particle Size | 7.0 - 15 µm | 7.0 - 15 µm | average |
Malvern Minerals Novakup® 325 Surface-Treated Lamellar Quartz Filler/Extender Novakup® is a surface modified or silane treated Novacite®. It has been used its barrier prosperities in chemical and corrosion resistant applications and as a filler/extender/reinforcing agen.. |
|||
Particle Size | 7.0 - 11 µm | 7.0 - 11 µm | Mean (agglomerates) |
Momentive Performance Materials AC6003 Boron Nitride (BN) Powder GE Advanced Ceramics boron nitride (BN) powders of grades HCV, AC6003, and AC6097 are agglomerates composed of submicron hexagonal turbostratic crystals. The mean particle size for these fine powder.. |
|||
Particle Size | 7.0 - 12 µm | 7.0 - 12 µm | 10% |
H.C. Starck Amperit® 250.071 Water Atomized (NiCr 80-20) |
|||
Particle Size | 7.0 - 11 µm | 7.0 - 11 µm | Average Particle Size/Laser Diffraction D50 |
H.C. Starck Grade A Aluminum Nitride AIN High thermally conductive ceramicsComposite ceramicsSiAlONsHeat sinksElectrically insulating packages for electronicsCrucibles for metals and salt meltsThermally conductive filler for polymersCompon.. |
|||
Particle Size | 7.0 - 13 µm | 7.0 - 13 µm | Laser Diffraction D50 |
H.C. Starck Grade A Titanium Carbonitride Hard metals (tooling and machining)CermetsBlack ceramics |
|||
Particle Size | 7.0 - 10 µm | 7.0 - 10 µm | Laser Diffraction D50 |
H.C. Starck Grade A Titanium Nitride Additive for ceramic parts to increase electrical conductivityConstituent for cermets and black ceramicsRaw material for TiN sputter targets |
|||
Particle Size | 7.0 - 11 µm | 7.0 - 11 µm | Average Particle Size/Laser Diffraction D50 |
H.C. Starck Grade AT Aluminum Nitride AIN High thermally conductive ceramicsComposite ceramicsSiAlONsHeat sinksElectrically insulating packages for electronicsCrucibles for metals and salt meltsThermally conductive filler for polymersCompon.. |
|||
Particle Size | 7.0 µm | 7.0 µm | 50% of particles, (REG Powder) |
Ferro IP 730 Passivation Glasses (Pb-B-Si-Al; Pb-Si-Al; Si-Pb-Al Silicates) Glass Type: Pb-B-Si-Al Typical Powder Form: TF, REG, RWG, SRRG Ferro's passivation glasses are designed for use on transistors, thyristors, and diodes. These products are formulated and produced to.. |
|||
Particle Size | 7.0 µm | 7.0 µm | Before Conversion |
Silberline Aquavet® 651-136M Aquavet® grades are aluminum pigment pellets designed for use in aqueous inks for flexographic and gravure printing. The pellets are composed of 80% aluminum pigment and 20% of a proprietary poly.. |
|||
Particle Size | 7.0 µm | 7.0 µm | |
Silberline EternaBrite® 651-1 EternaBrite® pigments are leafing aluminum pigment pastes carried in isopropyl alcohol. These grades are based on cornflake geometry and offer enhanced leafing properties in solvent and waterborn.. |
|||
Particle Size | 7.0 µm | 7.0 µm | |
Silberline EternaBrite® 651-DL EternaBrite® "DL" pigments are leafing aluminum pigment pastes carried in a glycol. These grades are based on cornflake geometry and offer enhanced leafing properties flexographic and gravure ink.. |
|||
Particle Size | 7.0 µm | 7.0 µm | |
Silberline EternaBrite® 651-PA EternaBrite® pigments are leafing aluminum pigment pastes carried in isopropyl alcohol. These grades are based on cornflake geometry and offer enhanced leafing properties in solvent and waterborn.. |
|||
Particle Size | 7.0 µm | 7.0 µm | |
Silberline Extra Fine "N" Standard Series Extra Fine "N" - is an ultra fine, high opacity, non-leafing aluminum pigment for solvent based industrial coatings. Due to the small particle size, this grade is well suited for imparting high opac.. |
|||
Particle Size | 7.0 µm | 7.0 µm | |
Silberline Silvet® AD 2000 LT20353 Silvet® AD grades are non-leafing aluminum pigments designed for use in solvent borne flexographic and gravure inks to provide optimal adhesion to polymer films and other substrates. They are sim.. |
|||
Particle Size | 7.0 µm | 7.0 µm | |
Silberline Sparkle Silver® 7000-AR Sparkle Silver® 7000-AR is an super fine, bright non-leafing aluminum pigment with good opacity for solvent-based general industrial coatings. It provides excellent coverage and color.Application.. |
|||
Particle Size | >= 7.0 µm | >= 7.0 µm | |
Chesterton 787 Sliding Paste Description: Chesterton® 787 Sliding Paste is a premium quality pure synthetic lubricant that will function affectivity even at ultra high temperatures and pressures. Designed for the most severe o.. |
|||
Particle Size | 7.0 - 13 µm | 7.0 - 13 µm | Average; ATO 40-41-0 (Coulter Counter) |
Arkema Group ORGASOL® 3501 EXD Nat 1 Copolyamide 6/12 Information provided by Arkema Group |
|||
Particle Size | 7.0 - 11 µm | 7.0 - 11 µm | Mean particle size is 7 to 11 µm. Crystal size is 0.1 µm. %-325 mesh is 95%. |
Momentive Performance Materials HCV Boron Nitride (BN) Powder Grade HCV is a 95%, -325 mesh hexagonal Boron Nitride (BN) powder exhibiting the unique properties of BN in a form readily used in the production of many advanced materials. Grade HCV is an initial .. |
|||
Particle Size | 7.0 µm | 7.0 µm | median; Microtrac |
Nyco ULTRAFIBRE® 4W Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |