Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay Specialty Polymers Polymist® F-5A EX PTFE Powder Lubricant  (Unverified Data**)

Category Polymer , Thermoplastic , Fluoropolymer , PTFE , PTFE Powder
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Polymist® F-5A EX PTFE Powder Lubricant  (Unverified Data**).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Polymist® powders are a family of white free-flowing polytetrafluoroethylene powders for use as additives in other materials to enhance processing or end-use performance characteristics. Polymist powders have been specially produced to provide a finely divided product which will not agglomerate and can easily be dispersed in dry or liquid media. Polymist powders are used as additives in elastomers and plastics where improved lubricity and/or wear resistance is required. In paints and coatings Polymist powders are designed for use as additives where narrow particle size distribution is required and improvements in release, mar resistance, slip, chemical resistance, weatherability, and moisture repelling characteristics are desired. Printing inks use Polymist powders as scuff resistant additives. Polymist powders are used as dry lubricants in machinery where liquid lubricants and/or potential staining cannot be tolerated.Uses: Thermoplastics, thermoset resins, paints, coatings, printing inks, oils, and greases.Benefits of Polymist powders are it can be used alone as dry-film lubricants, or as additives in plastics, elastomers and other media; does not agglomerate or lump during handling or processing; inert to practically all chemical solvents; reduces the friction coefficient; improves wear characteristics; UV and weather resistant; improved nonstick and release properties; increased rub resistance; improved corrosion resistance, improved thermal stability; improved thermal stability; improved corrosion resistance; improved thermal stability; excellent electrical insulator; and does not absorb moisture.Information provided by Solvay Solexis, Inc.
Physical Properties Metric English Comments
Bulk Density 0.400 g/cc
0.0145 lb/in³
Density 2.28 g/cc
0.0824 lb/in³
Particle Size <= 7.0 µm
<= 7.0 µm
<4% of particles are less than 20 microns
Specific Surface Area 2.58 m²/g
2.58 m²/g
Mechanical Properties Metric English Comments
Coefficient of Friction <= 0.10
<= 0.10
Thermal Properties Metric English Comments
Melting Point 325 - 330 °C
617 - 626 °F
Crystallization Temperature 312 - 318 °C
594 - 604 °F
Descriptive Properties Value Comments
Color White