Material Notes:
Silvet® AD grades are non-leafing aluminum pigments designed for use in solvent borne flexographic and gravure inks to provide optimal adhesion to polymer films and other substrates. They are similar to Silberline's Silvet® "J" technology, but have been reformulated to improve adhesion properties. Silvet® AD grades are supplied in pellet form composed of 80% aluminum pigment and 20% carrier resin. The carrier resin contributes to the resin solids of the ink formulation. Cost savings can be realized by adjusting the resin solids of the ink to accommodate the resin contribution from the pigment pellet. Like Silvet® "J" products, Silvet® AD grades provide excellent compatibility, ease of handling and ease of dispersion.Applications: Printing Inks
Physical Properties Metric English Comments
Specific Gravity 2.07 g/cc
2.07 g/cc
Volatiles 1.0 %
1.0 %
Particle Size 7.0 µm
7.0 µm
Descriptive Properties Value Comments
% Carrier 20
Carrier Aldehyde
Category Non-leafing